journal article·2023-05Open access

Effects of different cooling conditions on microstructure and precipitation behavior of fine-grained Al–Zn–Mg–Cu alloy friction stir welding joint

Lei Luo, Bo-Hai Yang, Xi-Rong Yang, Wen-Wen Yan, Chen Gan, Xiao-Yan Liu, Jing-Zhong Wang

Abstract

The microstructure evolution and precipitation phase distribution of 7075 aluminum alloy friction stir welding (FSW) joint were investigated under liquid CO2 cooling conditions. The fine grained 7075 aluminum alloy was developed by four-pass equal channel angular pressing (ECAP) and FSW joints with CO2 cooling at room temperature. It was found that CO2 cooling could effectively reduce the peak temperature of the weld, leading to a refinement of the welded grain and an improvement of the welded joint. Various recrystallization mechanisms were found in different areas of the weld. The grain boundary and dislocation density of large angles gradually decreased from the weld stir-zone (SZ) to the heat-affected-zone (HAZ) regions, and the anisotropy increased. The type of precipitated phase and the relationship with the matrix interface were determined by detecting the spacing between the precipitated phase and the crystal plane of the matrix. CO2 forced cooling not only enhanced the matrix dislocation strengthening and grain boundary strengthening, but also effectively improved the size and type of precipitated phases and the colattice strengthening effect. In addition, liquid CO2 cooling can greatly reduce the PFZ width and enhance the Zener pinning effect.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
2. Intergranular corrosion of spark plasma sintered 2024 aluminum alloy at different heat treatment states[J]10.1007/s12598-022-01990-7 ↗
3. Analytical model of residual stress in ultrasonic rolling of 7075 aluminum alloy10.1016/j.jmapro.2022.05.049 ↗
4. Tailoring the microstructure of a Cu-0.7Cr-0.07Zr alloy submitted to ECAP at cryogenic temperature for improved thermal stability10.1016/j.matchar.2022.112045 ↗
5. Effects of Mn addition on the microstructure and mechanical properties of Mg–Zn–Sn alloys
6. A constitutive model incorporating grain refinement strengthening on metallic alloys10.1016/j.jmst.2021.02.004 ↗
7. Strengthening-toughening methods and mechanisms of Mg–Li alloy: a review10.1007/s12598-021-01874-2 ↗
8. Tailoring the microstructure and texture to achieve high strength in a high-Al content Mg alloy by stepless-temperature-reduction ECAP10.1016/j.msea.2022.143023 ↗
9. Bacterial anti-adhesion surface design: surface patterning, roughness and wettability: a review10.1016/j.jmst.2021.05.028 ↗
10. Microstructural changes and formability of Al–Mg ultrafine-grained aluminum plates processed by multi-turn ECAP and upsetting
11. Grain refinement in hot working of 2219 aluminium alloy: on the effect of deformation mode and loading path
12. Analysis on exceptional cryogenic mechanical properties of AA2219 alloy FSW joints in multi-scale10.1016/j.msea.2022.143489 ↗
13. Rapidly improved tensile strength of 6N01 Al alloy FSW joints by electropulsing and artificial aging treatment10.1016/j.msea.2022.143056 ↗
14. Probing the anti-corrosion behavior of X65 steel underwater FSW joint in simulated seawater10.3389/fmats.2021.723986 ↗
15. Deformation behavior of friction-stir welded Al-Mg-Mn alloy with ultrafine-grained structure
16. Optimization of friction stir welding process to join dissimilar AA2014 and AA7075 aluminum alloys10.1016/j.matpr.2021.09.499 ↗
17. Mechanism of grain structure development for pure Cu and Cu-30Zn with low stacking fault energy during FSW[J]10.1080/13621718.2020.1818032 ↗
18. Crystallography of the nugget zone of bainitic steel by friction stir welding in various cooling mediums10.1016/j.matchar.2021.111523 ↗
19. Effect of rapid cooling on the microstructure and properties of fine-grained 7075 aluminium alloy under friction stir welding10.1088/2053-1591/ac6da5 ↗
20. Microstructure and corrosion behavior of friction stir welded Al alloy coated by in situ shot-peening-assisted cold spray10.1007/s40195-019-00966-4 ↗
21. Effect of retrogression re-aging treatment on the stress corrosion behavior of the 7075 Al–Zn–Mg–Cu alloy10.1002/maco.202112730 ↗
22. Microstructure of 7075 aluminum alloy by homogenization10.4028/www.scientific.net/MSF.993.138 ↗
23. Influence of contact solid-solution treatment on microstructures and mechanical properties of 7075 aluminum alloy
24. The strengthening mechanism of FSWed spray formed 7055 aluminum alloy under water mist cooling condition
25. Microstructural evolution of aluminum alloy during friction stir welding under different tool rotation rates and cooling conditions10.1016/j.jmst.2018.12.024 ↗
26. Conventional and underwater friction stir welded AA2024-T351 aluminium alloy – a comparative analysis10.1108/WJE-09-2019-0270 ↗
27. The tribocorrosion mechanism of aluminum alloy 7075-T6 in the deep ocean10.1016/j.corsci.2021.109306 ↗
28. Dynamic recrystallization and dynamic precipitation in AA6061 aluminum alloy during friction stir welding
29. Microstructure and tensile properties of rapid-cooling friction-stir-welded AZ31B Mg alloy along thickness direction10.1016/S1003-6326(20)65458-9 ↗
30. The impacts of grain boundary on the scattering of intermetallics in friction-stir-welded AA6061-T610.1016/j.matlet.2021.130206 ↗
31. Development of a fuzzy logic based model to elucidate the effect of FSW parameters on the ultimate tensile strength and elongation of pure copper joints
32. The failure mechanism at adiabatic shear bands of titanium alloy: high-precision survey using precession electron diffraction and geometrically necessary dislocation density calculation10.1016/j.msea.2019.01.016 ↗
33. Effects of ageing treatment on corrosion behavior of 7075 aluminum alloy coated by micro arc oxidation (MAO)10.1016/j.corsci.2022.110164 ↗
34. Strength mismatch mechanism on friction stir welding joint of 7075 aluminum alloy
35. Preparation of Ti-22Al-25Nb solid solution powders using mechanical alloying and solid solution mechanism analysis10.1016/j.apt.2020.02.029 ↗
36. Precipitate microstructures of high strength Mg-Gd-Y-Zn-Zr alloys10.4028/www.scientific.net/AMR.11-12.417 ↗
37. Effect of Nb micro-alloying on austenite nucleation and growth in a medium manganese steel during intercritical annealing10.1016/j.actamat.2022.117786 ↗