Interfacial evolution and coordinated deformation mechanism of Ti/Al laminated metal composites prepared by diffusion bonding
Source abstract
Abstract
Laminated metal composites (LMCs) of titanium and aluminum (Ti/Al), combining the high strength and thermal stability of titanium with the low density and corrosion resistance of aluminum, hold substantial promise for industrial applications. Utilizing diffusion bonding under optimal processing conditions—specifically a bonding temperature of 550 °C and a holding time of 120 min—an average interfacial shear strength of 68.7 MPa was achieved. Transmission electron microscopy (TEM) revealed a metallurgically bonded interface facilitated by the mutual atomic diffusion of titanium and aluminum; this diffusion layer predominantly comprises the TiAl3 phase. Detailed insights into the microstructural evolution at the interface, including dislocation configurations, were also obtained in this study. The Burgers vectors of these dislocations were determined using the two-beam electron diffraction contrast imaging method. Based on these results, it can be elucidated that the deformation mechanism of Ti layer was dominated by the dislocation slip (mainly prismatic and the basal slip), while the coordinated deformation of TiAl3/Al interface benefitted by the dislocations gliding across the interface.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Achieve High interfacial bonding strength of Ti/Al laminated composite at room temperature via electropulsing-assisted ultrasonic additive manufacturing[J]10.1007/s11661-022-06923-8 ↗
2. Wu H., et al. Fabrication and microstructure evolution of novel laminated TiAl composite10.1016/j.matchar.2022.112446 ↗
3. Miao Y., et al. Microstructure, deformation behaviors and GND density evolution of Ti-Al laminated composites under the incremental compression test10.1016/j.mtcomm.2022.104605 ↗
4. Dash Biswaranjan., Karthikeyan S.Dynamic compression behavior of Ti/TiAl3/Al metal intermetallic laminates
5. Formability improvement of hot-pressed Ti/Al laminated sheet by TiAl3 layer growth and crack healing during deformation10.1016/j.jallcom.2022.168604 ↗
6. Li J., et al. Characterization of the Widmanstätten structure in γ-TiAl alloy using an EBSD-FIB-TEM combined process10.1016/j.scriptamat.2022.115001 ↗
7. Jiang B.,et al. Effect of layer thickness on the enhanced strength and ductility of laminated Ti/Al composite10.1016/j.msea.2022.144230 ↗
8. Li H.Formation mechanism and growth kinetics of TiAl3 phase in cold-rolled Ti/Al laminated composites during annealing10.1016/S1003-6326(22)65813-8 ↗
9. Xing B.,et al. Influence of the anisotropy on the microstructure and mechanical properties of Ti/Al laminated composites10.3390/ma13163556 ↗
10. Microstructure and mechanical properties of Al/Ti/Al laminated composites prepared by roll bonding10.1016/j.msea.2015.03.086 ↗
11. Liu X.,et al. Enhanced materials performance of Al/Ti/Al laminate sheets subjected to cryogenic roll bonding10.1557/jmr.2017.355 ↗
12. Preparation, microstructure and mechanical properties of CP-Ti/AA6060-Al laminated composite by differential temperature rolling with induction heating10.1016/j.jmapro.2019.05.053 ↗
13. Preparation and properties for Ti/Al clad plates generated by differential temperature rolling10.1016/j.jmatprotec.2017.06.013 ↗
14. Simultaneously achieving high tensile strength and fracture toughness of Ti/Ti-Al multilayered composites10.1016/j.intermet.2017.06.007 ↗
15. Laminated Ti-Al composites: processing, structure and strength10.1016/j.msea.2016.07.108 ↗
16. Effect of interface on mechanical properties and formability of Ti/Al/Ti laminated composites10.1016/j.jmrt.2021.07.021 ↗
17. He W., et al. Effect of intermetallic compounds (IMCs) on the interfacial bonding strength and mechanical properties of pre-rolling diffusion ARBed Al/Ti laminated composites10.1016/j.matchar.2020.110731 ↗
18. Synthesis and microstructural characterization of Ti–Al3Ti metal–intermetallic laminate (MIL) composites10.1016/j.scriptamat.2004.09.010 ↗
19. First-principles study of the Ti/Al3Ti interfacial properties10.1016/j.apsusc.2021.148960 ↗
20. Structural properties of Ti/Al clads manufactured by explosive welding and annealing10.1016/j.matdes.2015.11.087 ↗
21. Mechanical properties of Ti–(SiCp/Al) laminated composite with nano-sized TiAl3 interfacial layer synthesized by roll bonding10.1016/j.msea.2013.06.026 ↗
22. Diffusion in the Ti–Al system10.1016/S1359-6454(99)00400-0 ↗
23. On equilibrium and non-equilibrium peritectic transformations10.1016/0001-6160(74)90077-7 ↗
24. Thermodynamic assessment and calculation of the Ti-Al system10.1007/BF02646001 ↗
25. On the kinetics of TiAl3 intermetallic layer formation in the titanium and aluminum diffusion couple10.1016/j.intermet.2012.08.017 ↗
26. Growth kinetics of TiAl3 layer in multi-laminated Ti–(TiB2/Al) composite sheets during annealing treatment10.1016/j.msea.2012.01.107 ↗
27. Variant selection during secondary and tertiary twinning in pure titanium10.1016/j.actamat.2014.04.065 ↗
28. Initiation and accommodation of primary twins in high-purity titanium10.1016/j.actamat.2014.03.025 ↗
29. Wang · 2007 · 103
30. Theory of dislocations10.1115/1.3167075 ↗
31. Mittemeijer · 2021
32. Elastic constants of TiAl3 and ZrAl3 single crystals10.1007/BF00549190 ↗
33. Electronic, elastic, and fracture properties of trialuminide alloys: Al3Sc and Al3Ti10.1557/JMR.1990.0971 ↗
34. Atomic-scale simulations of the interaction between a moving dislocation and a bcc/fcc phase boundary10.1016/j.commatsci.2004.09.024 ↗
35. Slip transmission across fcc/bcc interfaces with varying interface shear strengths10.1016/j.actamat.2011.11.047 ↗
36. Chen N.,et al. Dislocations across interphase enable plain steel with high strength-ductility10.1016/j.scib.2021.02.032 ↗