journal article·2024-05Open access

Hybrid interlayer hot rolling and wire arc additive manufacturing of Al-Mg alloy: Microstructure, mechanical properties and strengthening mechanism

Jianwu Huang, Youheng Fu, Wenzheng Zhai, Runsheng Li, Xushan Zhao, Hang Lin, Haiou Zhang, Guilan Wang

Abstract

Considering the deformation-strengthening benefits of Al-Mg alloy and the high forming efficiency offered by wire and arc additive manufacturing (WAAM), the microstructure evolution and strengthening mechanism of hybrid interlayer hot rolling and wire arc additive manufacturing (HR-WAAM) samples have been systematically investigated in this study. The results indicate that interlayer hot rolling can effectively reduce the size and number of pores, which diminishes the stress concentration areas. Additionally, rolling deformation significantly enhances the effect of dislocation strengthening. Furthermore, a high density of dislocations can promote recrystallization to refine grain size, while also improving grain orientation, all of which contribute to better stress distribution. Due to these reasons, the strength and toughness of the alloy are notably improved. The average ultimate tensile strength (UTS), yield strength (YS), and elongation (EL) values achieved by HR-WAAM samples were 338 MPa, 276 MPa, and 20.9%, respectively. These values represent increases of 28.5%, 41.5%, and 38.4% compared to conventional WAAM samples. These findings are expected to provide an efficient and cost-effective method for additive manufacturing (AM) of deformation-strengthened aluminum alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
2. High deposition rate powder- and wire-based laser directed energy deposition of metallic materials: a review10.1016/j.ijmachtools.2022.103942 ↗
3. A critical review on wire-arc directed energy deposition of high-performance steels10.1016/j.jmrt.2023.05.163 ↗
4. Achieving material diversity in wire arc additive manufacturing: leaping from alloys to composites via wire innovation10.1016/j.ijmachtools.2023.104103 ↗
5. A review of the wire arc additive manufacturing of metals: properties, defects and quality improvement10.1016/j.jmapro.2018.08.001 ↗
6. Research challenges, quality control and monitoring strategy for Wire Arc Additive Manufacturing10.1016/j.jmrt.2023.03.200 ↗
7. Research progress in arc based additive manufacturing of aluminium alloys – a review10.1016/j.measurement.2022.111672 ↗
8. Microstructure and mechanical properties of Al-Zn-Mg-Cu alloy fabricated by wire + arc additive manufacturing10.1016/j.jmapro.2020.12.045 ↗
9. Microstructure and mechanical properties of wire arc additive manufactured ZL205A alloy10.1016/j.jmrt.2023.08.107 ↗
10. Pore formation and evolution in wire + arc additively manufactured 2319 Al alloy
11. A high-performance WAAM process for Al–Mg–Mn using controlled short-circuiting metal transfer at increased wire feed rate and increased travel speed10.1016/j.matdes.2020.109040 ↗
12. Influence of travel speed on microstructure and mechanical properties of wire + arc additively manufactured 2219 aluminum alloy10.1016/j.jmst.2019.06.016 ↗
13. Porosity in wire arc additive manufacturing of aluminium alloys
14. Wire arc additive manufacturing of Al-Mg-Sc alloy: an analysis of the effect of Sc on microstructure and mechanical properties10.1016/j.matchar.2023.113116 ↗
15. A comparative study on Al-Mg-Sc-Zr alloy fabricated by wire arc additive manufacturing with controlling interlayer temperature and continuous printing: porosity, microstructure, and mechanical properties10.1016/j.jmst.2023.12.062 ↗
16. Deformation microstructures and strengthening mechanisms for the wire+arc additively manufactured Al-Mg4.5Mn alloy with inter-layer rolling10.1016/j.msea.2017.11.113 ↗
17. Micropore evolution in additively manufactured aluminum alloys under heat treatment and inter-layer rolling10.1016/j.matdes.2019.108288 ↗
18. Periodic microstructure of Al–Mg alloy fabricated by inter-layer hammering hybrid wire arc additive manufacturing: formation mechanism, microstructural and mechanical characterization10.1016/j.msea.2022.144314 ↗
19. Microstructure evolution of wire-arc additively manufactured 2319 aluminum alloy with interlayer hammering10.1016/j.msea.2020.140168 ↗
20. Enhanced strength-plasticity of 2319 Al-Cu alloy formed by hybrid interlayer friction stir processing and wire-arc additive manufacturing10.1016/j.jmatprotec.2023.118146 ↗
21. Tailoring the microstructure and mechanical properties of wire and arc additive manufactured Al–Mg alloy via interlayer friction stir processing10.1016/j.jmrt.2023.06.053 ↗
22. Precipitation phenomena and strengthening mechanism of Al–Cu alloys deposited by in-situ rolled wire-arc additive manufacturing10.1016/j.msea.2022.143770 ↗
23. Evaluation of in situ hot-rolling forming effect on plastic zone of wire + arc additively manufactured 5087 alloys using digital image correlation technique10.1016/j.ijfatigue.2022.107189 ↗
24. Defect-correlated fatigue resistance of additively manufactured Al-Mg4.5Mn alloy with in situ micro-rolling10.1016/j.jmatprotec.2020.117039 ↗
25. Effect of arc oscillation on porosity and mechanical properties of 2319 aluminum alloy fabricated by CMT-wire arc additive manufacturing10.1016/j.jmrt.2023.03.203 ↗
26. Optimization of the geometry for the end lateral extension path strategy to fabricate intersections using laser and cold metal transfer hybrid additive manufacturing
27. Effect of pulsed metal inert gas (pulsed-MIG) and cold metal transfer (CMT) techniques on hydrogen dissolution in wire arc additive manufacturing (WAAM) of aluminium10.1007/s00170-020-04946-2 ↗
28. A review on Cold Metal Transfer (CMT) technology of welding10.1016/j.matpr.2022.04.016 ↗
29. Hardness reversal in severely deformed automotive Al-Mg-Si alloys10.1016/j.jallcom.2024.173515 ↗
30. Portevin-Le Chatelier characterization of annealed Al-Mg alloy sheets with different Mg contents10.1016/j.msea.2024.146118 ↗
31. Validating continuum theory for Cottrell atmosphere solute drag by molecular dynamics simulations10.1016/j.jmps.2023.105514 ↗
32. Impact of dispersoids' distribution on portevin-le-chatelier effect and surface quality in Al–Mg-Sc-Zr alloys10.1016/j.msea.2023.145108 ↗
33. The dependency of work hardening on dislocation statistics in cold rolled 1050 aluminum alloy10.1016/j.matchar.2022.112166 ↗
34. Microstructure evolution of 5052 aluminum alloy after electromagnetic-driven stamping following different heat treatment conditions10.1016/j.jmrt.2024.03.049 ↗
35. Understanding the effect of deformation combined with heat treatment on age hardening of Al–Zn–Mg–Cu alloy AA707510.1016/j.msea.2023.145212 ↗
36. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
37. Mechanism for enhanced precipitation strengthening due to the addition of copper to Al-Zn-Mg alloys with high Zn/Mg ratio10.1016/j.matdes.2023.112295 ↗
38. Dynamic impact constitutive relation of 6008-T6 aluminum alloy based on dislocation density and second-phase particle strengthening effects10.1016/j.jallcom.2022.167718 ↗
39. Strengthening mechanisms and work hardening in a heterostructured cast aluminum alloy under compressive loading: correlation with nanomechanical properties10.1016/j.jallcom.2023.171844 ↗
40. Precipitation, mechanical properties and early slant ductile fracture in cyclic and naturally aged Al-Zn-Mg(-Cu) alloys10.1016/j.matdes.2022.111026 ↗
41. Precipitation strengthening in naturally aged Al–Zn–Mg–Cu alloy10.1016/j.msea.2020.140719 ↗
42. Significantly improved particle strengthening of Al–Sc alloy by high Sc composition design and rapid solidification10.1016/j.msea.2020.140304 ↗
43. Macro/micro-structure and mechanical properties of Al-6Mg-0.3Sc alloy fabricated by oscillating laser-arc hybrid additive manufacturing10.1016/j.jallcom.2022.167325 ↗