Growth kinetics and IMCs layer analysis of SAC305 solder with the reinforcement of SiC during the isothermal aging condition

Manoj Kumar Pal, Gréta Gergely, Zoltán Gácsi

Abstract

The Sn–3.0wt.%Ag–0.5wt.%Cu(SAC305) - xSiC composite solder was prepared by powder metallurgy method with the addition of SiC ceramic reinforcement with various compositions (0, 0.5, 1, and 1.5wt.%). The IMC layer thickness of Cu3Sn and Cu6Sn5 was suppressed during 100 h aging and the minimum thickness was found for 1.0wt.% SiC addition. The SAC305-1.0wt.%SiC/Cu was then subjected to different aging conditions (413, 423, 433, and 443 K). The IMCs thickness at the Cu-solder interface was investigated by using FIB-SEM and image analysis software (ImageJ). The SiC and Ag3Sn particles were identified in the matrix's bulk area, and the growth kinetics were examined in a detailed manner in aging conditions. Diffusion coefficients and activation energies for the two mentioned IMCs were plotted as a temperature function, and the values were calculated by the Arrhenius equation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Investigation of microstructure and wetting behavior of Sn–3.0Ag–0.5Cu(SAC305) lead-free solder with additions of 1.0 wt % SiC on copper substrate10.1016/j.intermet.2020.106991 ↗
2. Cu/Sn interfacial reactions: thin-film case versus bulk case10.1016/S0254-0584(97)80016-8 ↗
3. Microstructure and intermetallic growth effects on shear and fatigue strength of solder joints subjected to thermal cycling aging10.1016/S0921-5093(00)01958-4 ↗
4. Influence of TiO2 nanoparticles on IMC growth in Sn–3.0Ag–0.5Cu–xTiO2 solder joints in reflow process10.1016/j.jallcom.2012.12.019 ↗
5. Effects of nano-Al2O3 particles on microstructure and mechanical properties of Sn–3.5Ag–0.5Cu composite solder ball grid array joints on Sn/Cu pads10.1016/j.matdes.2013.03.045 ↗
6. Effect of nano–Fe2O3 additions on wettability and interfacial intermetallic growth of low–Ag content Sn-Ag-Cu solders on Cu substrates10.1016/j.jallcom.2014.12.024 ↗
7. Effect of ZnO micron-particles on properties and intermetallic compound layers of a Sn–3.0Ag–0.5Cu solder
8. Growth mechanism of intermetallic compounds and damping properties of Sn–Ag–Cu-1wt% nano-ZrO2 composite solders10.1016/j.microrel.2014.01.026 ↗
9. Quasi-in-situ observation on diffusion anisotropy dominated asymmetrical growth of Cu-Sn IMCs under temperature gradient10.1016/j.actamat.2021.117168 ↗
10. Interfacial reaction and IMC growth of an ultrasonically soldered Cu/SAC305/Cu structure during isothermal aging10.3390/ma11010084 ↗
11. Thermal analysis and mechanical properties of Sn–1.0Ag–0.5Cu solder alloy after modification with SiC nano-sized particles10.1007/s10854-013-1200-8 ↗
12. Microstructure, mechanical properties, and deformation behavior of Sn–1.0Ag–0.5Cu solder after Ni and Sb additions10.1016/j.matdes.2012.06.058 ↗
13. Improvement on the microstructure stability, mechanical and wetting properties of Sn–Ag–Cu lead-free solder with the addition of rare earth elements10.1016/j.jallcom.2004.01.012 ↗
14. Solid-state intermetallic compound layer growth between copper and 95.5Sn–3.9Ag–0.6Cu solder10.1007/s11664-004-0026-9 ↗
15. Morphology, kinetics, and thermodynamics of solid-state aging of eutectic SnPb and Pb-free solders (Sn–3.5Ag, Sn–3.8Ag–0.7Cu and Sn–0.7Cu) on Cu10.1557/JMR.2002.0042 ↗
16. Solid-state reactions between Cu (Ni) alloys and Sn10.1007/s11664-007-0251-0 ↗
17. Effect of electromigration on intermetallic compound formation in line-type Cu/Sn/Cu interconnect10.1016/j.jallcom.2010.05.158 ↗
18. Influence of nanoparticle addition on the formation and growth of intermetallic compounds (IMCs) in Cu/Sn–Ag-Cu/Cu solder joint during different thermal conditions10.1088/1468-6996/16/3/033505 ↗
19. Distribution and microstructure analysis of ceramic particles in the lead-free solder matrix10.1002/crat.202000123 ↗
20. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
21. A review of intermetallic compound growth and void formation in electrodeposited Cu–Sn Layers for microsystems packaging10.1007/s10854-021-05412-9 ↗
22. Review Progress in Ostwald ripening theories and their applications to nickel-base superalloys Part I: Ostwald ripening theories10.1023/A:1015388912729 ↗
23. Effect of nano-TiO2 addition on the microstructure and bonding strengths of Sn–3.5Ag–0.5Cu composite solder BGA packages with immersion Sn surface finish10.1007/s10854-011-0327-8 ↗
24. Effect of SiC nanoparticle additions on microstructure and microhardness of Sn-Ag-Cu solder alloy10.1007/s11664-007-0366-3 ↗
25. Effect of Y2O3 particles on microstructure formation and shear properties of Sn-58Bi solder10.1007/s10854-009-0025-y ↗
26. A diffusion model and growth kinetics of interfacial intermetallic joints10.1016/j.jallcom.2019.152893 ↗
27. Ostwald–Freundlich diffusion-limited dissolution kinetics of nano particles10.1016/j.powtec.2014.01.095 ↗
28. Gibbs–Thomson effects in phase transformations10.1016/j.scriptamat.2004.12.026 ↗
29. Growth of η phase scallops and whiskers in liquid tin-solid copper reaction couples10.1007/s11837-001-0100-1 ↗
30. Kinetic theory of flux-driven ripening10.1103/PhysRevB.66.115403 ↗
31. Direct evidence for a Cu–enriched region at the boundary between Cu6Sn5 and Cu3Sn during Cu/Sn reaction10.1016/j.scriptamat.2010.04.011 ↗
32. Bismuth redistribution induced by intermetallic compound growth in SnBi/Cu microelectronic interconnect10.1007/s10853-008-3118-8 ↗
33. Evolution of nano–Ag3Sn particle formation on Cu–Sn intermetallic compounds of Sn–3.5Ag–0.5Cu composite solder/Cu during soldering10.1016/j.jallcom.2010.11.010 ↗
34. Interfacial reactions between lead-free solders and common base materials10.1016/j.mser.2005.03.001 ↗
35. Evolution of intermetallic compounds between Sn–0.3Ag–0.7Cu low–silver lead–free solder and Cu substrate during thermal aging10.1016/S1005-0302(12)60023-1 ↗
36. Analysis of low-temperature intermetallic growth in copper-tin diffusion couples10.1007/BF02675563 ↗
37. The growth of Cu–Sn intermetallics at a pretinned copper-solder interface10.1007/BF02665064 ↗
38. Okamoto · 1990
39. Evolutions of the interface and shear strength between SnAgCu–xNi solder and Cu substrate during isothermal aging at 150 °C10.1016/j.jallcom.2009.06.171 ↗
40. Intermetallics Interfacial reactions of eutectic Sn3.5Ag and pure tin solders with Cu substrates during liquid-state soldering10.1016/j.intermet.2012.02.023 ↗
41. Effect of Sn/Cu thickness ratio on the transformation law of Cu6Sn5 to Cu3Sn in Sn/Cu interface during aging10.1088/2053-1591/aad126 ↗
42. Dependence of intermetallic compound formation on the sublayer stacking sequence in Ag–Sn bilayer thin films10.1016/j.actamat.2015.09.042 ↗
43. Suppression of interdiffusion-induced voiding in oxidation of copper nanowires with twin-modified surface10.1038/s41467-017-02154-3 ↗
44. The growth behavior of interfacial intermetallic compound between Sn–3.5Ag–0.5Cu solder and Cu substrate under different thermal-aged conditions10.1007/s10854-017-7799-0 ↗
45. Influence of third elements on growth of Nb3Sn compounds and on global pinning force10.1007/BF01114703 ↗
46. Interdependent intermetallic compound growth in an electroless Ni-P/Sn-3.5Ag reaction couple10.1007/s11664-010-1447-2 ↗
47. Interfacial microstructure and the kinetics of interfacial reaction in diffusion couples between Sn–Pb solder and Cu/Ni/Pd metallization10.1016/S1359-6454(00)00165-8 ↗
48. Growth mechanism of Ni3Sn4 in a Sn/Ni liquid/solid interfacial reaction10.1016/j.actamat.2009.07.021 ↗
49. Activation energies of intermetallic growth of Sn-Ag eutectic solder on copper substrates10.1007/s11664-997-0268-4 ↗
50. Intermetallic compound layer growth between SnAgCu solder and Cu substrate in electronic packaging10.1007/s10854-013-1236-9 ↗