Microstructure and dynamic mechanical behavior of wire-arc additive manufactured high-strength steel
Source abstract
Abstract
The working environment of high-strength steel components produced by wire-arc additive manufacturing (WAAM) often faced challenges of explosion and impact, but the microstructure evolution and dynamic mechanical behavior of WAAM produced high-strength steel were still unclear. In this study, low alloy high-strength steel (HSS) components were produced by WAAM. Split Hopkinson Pressure Bar (SHPB) tests at different strain rates were carried out on WAAM-HSS, and the specimens before and after dynamic compression were characterized by techniques such as SEM, EDS, XRD, EBSD, etc. The results showed that: The as-built WAAM-HSS plate mainly consists of five typical structures: lath martensite (ML), acicular ferrite (AF), polygonal ferrite (PF), martensite-austenite (M-A), and precipitated phase δ. The central area of the precipitated phase is Si and Mn, and the C element is mainly distributed in the surrounding area of the precipitated phase. Under dynamic compression, the as-built WAAM-HSS exhibited obvious yield phenomenon, and the yield stress increased with the increase of strain rate. The yield-strengthening mechanism is mainly contributed by grain refinement strengthening mechanism and dislocation density strengthening mechanism. Under dynamic compression, the martensite transformation occurred in the WAAM-HSS. The deformation mechanism is dislocation slip and twinning, which compete with each other. Dislocation slip deformation is dominant at low strain rate and twinning deformation is more dominant at high strain rate.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Velocity Impact and Material Behavior · Additive Manufacturing Materials and Processes · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Characterization and mechanical properties of cladded stainless steel 316L with nuclear applications fabricated using electron beam melting10.1016/j.jnucmat.2018.04.026 ↗
2. Functionally graded Ti6Al4V-Mo alloy manufactured with DED-CLAD® process
3. Invited review article: strategies and processes for high quality wire arc additive manufacturing
4. Corrosion behavior of wire-arc additive manufactured and as-cast Ni-Al bronze in 3.5 wt% NaCl solution10.1016/j.corsci.2023.111048 ↗
5. Element partitioning and electron backscatter diffraction analysis from feeding wire to as-deposited microstructure of wire and arc additive manufacturing with super duplex stainless steel10.1016/j.msea.2019.138856 ↗
6. Direct metal additive manufacturing processes and their sustainable applications for green technology: a review10.1007/s40684-016-0048-9 ↗
7. Cold metal transfer (CMT) technology - an overview10.1016/j.dt.2017.08.002 ↗
8. Formation mechanism and control methods of acicular ferrite in HSLA steels: a review10.1016/j.jmst.2017.11.020 ↗
9. Dynamic mechanical behavior of ultra-high strength steel 30CrMnSiNi2A at high strain rates and elevated temperatures10.1016/S1006-706X(17)30109-7 ↗
10. Dynamic mechanical behaviors and failure thresholds of ultra-high strength low-alloy steel under strain rate 0.001/s to 106/s10.1016/j.msea.2018.02.019 ↗
11. Study on dynamic mechanical behavior of Q460JSC and HQ600 high strength steel10.1016/j.jcsr.2020.106232 ↗
12. Prediction of ductile fracture for advanced high strength steel with a new criterion: experiments and simulation10.1016/j.jmatprotec.2013.03.001 ↗
13. The investigation on Johnson-Cook model and dynamic mechanical behaviors of ultra-high strength steel M5410.1016/j.msea.2022.142693 ↗
14. Strain rate behaviour in tension of S355 steel: base for progressive collapse analysis10.1016/j.engstruct.2016.04.013 ↗
15. Analysis of fracture toughness properties of wire + arc additive manufactured high strength low alloy structural steel components10.1016/j.msea.2019.138285 ↗
16. Anisotropic mechanical properties and deformation behavior of low-carbon high-strength steel component fabricated by wire and arc additive manufacturing10.1016/j.msea.2020.139514 ↗
17. Dynamic mechanical properties of 316L stainless steel fabricated by an additive manufacturing process10.1016/j.jmrt.2020.12.097 ↗
18. Mechanical properties and dynamic constitutive model of 42CrMo steel10.1016/j.matdes.2017.01.066 ↗
19. Effect of martensite-austenite (MA) distribution on mechanical properties of inter-critical Reheated Coarse Grain heat affected zone in X80 linepipe steel10.1016/j.msea.2019.138301 ↗
20. Analysis of martensite–austenite constituent and its effect on toughness in submerged arc welded joint of low carbon bainitic steel10.1007/s10853-012-6346-x ↗
21. Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone: Part I. Fractographic evidence10.1007/BF02651598 ↗
22. Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by austenitic filler metal10.1016/j.matchar.2015.05.017 ↗
23. Flow behavior and microstructure evolution during dynamic deformation of 316 L stainless steel fabricated by wire and arc additive manufacturing10.1016/j.matdes.2020.109325 ↗
24. Kinetics of Martensitic transformation in partially bainitic 300M steel10.1016/0921-5093(90)90273-6 ↗
25. Martensitic transformation in SUS 316LN austenitic stainless steel at RT10.1007/s10853-008-2494-4 ↗
26. Quantitative interpretation of X-ray diffraction patterns of mixtures. I. Matrix-flushing method for quantitative multicomponent analysis10.1107/S0021889874010375 ↗
27. XRD-based quantitative analysis of clay minerals using reference intensity ratios, mineral intensity factors, Rietveld, and full pattern summation methods: a critical review10.1016/j.sesci.2017.12.002 ↗
28. Martensitic transformation dominated tensile plastic deformation of nanograins in a gradient nanostructured 316L stainless steel10.1016/j.actamat.2023.118780 ↗
29. Improved wear and corrosion resistance of microarc oxidation coatings on Ti–6Al–4V alloy with ultrasonic assistance for potential biomedical applications10.1002/adem.202001433 ↗
30. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
31. Mechanical properties and microstructure evolution of additive manufactured 316L stainless steel under dynamic loading10.1016/j.msea.2022.143896 ↗
32. Deformation twinning10.1016/B978-008044019-4/50025-8 ↗
33. A multiscale investigation into the effect of grain size on void evolution and ductile fracture: experiments and crystal plasticity modeling10.1016/j.ijplas.2019.09.009 ↗
34. Microstructure evolution and fracture behaviour of TWIP steel under dynamic loading10.1016/j.msea.2022.143657 ↗
35. Quasi-static and dynamic deformation mechanismsi nterpreted by microstructural evolution in TWinning Induced Plasticity (TWIP) steel10.1016/j.msea.2016.12.037 ↗
36. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗