journal article·2024-01Open access

Formation mechanisms and control strategies of metallurgical defects and microstructures during laser powder bed fusion of AlSi10Mg lattice structures

Xiangyuan Chen, Wenhe Liao, Huiliang Wei, Zhiguang Zhu, Tao Yang, Changdong Zhang, Tingting Liu

Abstract

Lattice structures fabricated using laser powder bed fusion (LPBF) are pivotal for lightweight design. However, their small dimensions and intricate geometry intensify the likelihood of defect formation, such as lack of fusion (LOF), near-spherical pores, and microstructural coarsening. In this study, it was observed that the central region of lattice struts was especially susceptible to large-sized LOF in conjunction with the concave top surfaces due to frequent laser jumps. Furthermore, overheating during turnaround was identified as a contributor to excessive pores and surface bulging. Intriguingly, a unique layered melt mode emerged, characterized by coarse columnar grains exceeding 30 μm in size. A novel approach is proposed to reduce defects, refine grains, and enhance hardness during LPBF process, utilizing low laser power and a continuous scanning strategy. Using this manipulation strategy on typical lattice structures, porosity levels decreased by over 40 %. Ultimately, this research offers invaluable insights into refining printing conditions for lattice structures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. On the current research progress of metallic materials fabricated by laser powder bed fusion process: a review10.1016/j.jmrt.2022.07.085 ↗
2. Revealing the precipitation behavior of crack-free TiB2/Al-Zn-Mg-Cu composites manufactured by Laser Powder Bed Fusion
3. Melt pool controlled laser powder bed fusion for customised low-density lattice structures10.1016/j.matdes.2019.108054 ↗
4. A mechanical property evaluation of graded density AlSi10Mg lattice structures manufactured by selective laser melting10.1016/j.msea.2016.06.013 ↗
5. Review of defects in lattice structures manufactured by powder bed fusion10.1007/s00170-019-04753-4 ↗
6. SLM lattice structures: properties, performance, applications and challenges10.1016/j.matdes.2019.108137 ↗
7. Factors that affect the properties of additively-manufactured AlSi10Mg: porosity versus microstructure
8. Quality control: internal defects formation mechanism of selective laser melting based on laser-powder-melt pool interaction: a review
9. In-situ X-ray computed tomography tensile tests and analysis of damage mechanism and mechanical properties in laser powder bed fused Invar 36 alloy10.1016/j.jmst.2023.08.014 ↗
10. Defects in additive manufactured metals and their effect on fatigue performance: a state-of-the-art review10.1016/j.pmatsci.2020.100724 ↗
11. Spattering and denudation in laser powder bed fusion process: Multiphase flow modelling10.1016/j.actamat.2020.06.033 ↗
12. Correlation between forming quality and spatter dynamics in laser powder bed fusion
13. Lightweight lattice structures in selective laser melting: design, fabrication and mechanical properties
14. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
15. Understanding keyhole induced-porosities in laser powder bed fusion of aluminum and elimination strategy10.1016/j.ijmachtools.2022.103977 ↗
16. Part-scale thermal simulation of laser powder bed fusion using graph theory: effect of thermal history on porosity, microstructure evolution, and recoater crash10.1016/j.matdes.2021.109685 ↗
17. On the thermal conductivity of AlSi10Mg and lattice structures made by laser powder bed fusion
18. Investigation for macro mechanical behavior explicitly for thin-walled parts of AlSi10Mg alloy using selective laser melting technique10.1016/j.jmapro.2021.04.022 ↗
19. Dynamics of pore formation during laser powder bed fusion additive manufacturing10.1038/s41467-019-10009-2 ↗
20. Controlling interdependent meso-nanosecond dynamics and defect generation in metal 3D printing10.1126/science.aay7830 ↗
21. Microstructure and geometry effects on the compressive behavior of LPBF-manufactured inconel 718 honeycomb structures10.1016/j.jmrt.2023.03.093 ↗
22. Recent progress on microstructure manipulation of aluminium alloys manufactured via laser powder bed fusion10.1080/17452759.2022.2125880 ↗
23. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting10.1016/j.jmst.2019.08.049 ↗
24. A review on Friction stir welding/processing: numerical modeling10.3390/ma16175890 ↗
25. Crack-free high-strength AA-7075 fabricated by laser powder bed fusion with inoculations of metallic glass powders10.1016/j.msea.2023.145916 ↗
26. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
27. Additively manufactured AlSi10Mg ultrathin walls: microstructure and nano-mechanical properties under different energy densities and interlayer cooling times
28. Laser powder bed fusion of AlSi10Mg: influence of energy intensities on spatter and porosity evolution, microstructure and mechanical properties10.1016/j.jallcom.2020.156300 ↗
29. Fluctuations of tracks and layers during aluminium laser powder-bed fusion10.3390/app11073132 ↗
30. Additive manufacturing of metallic components - process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
31. Defect elimination and microstructure improvement of laser powder bed fusion β-solidifying γ-TiAl alloys via circular beam oscillation technology
32. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
33. Microstructure of selective laser melted AlSi10Mg alloy10.1016/j.matdes.2019.107677 ↗
34. Selective laser melted AlSi10Mg alloy under melting mode transition: microstructure evolution, nanomechanical behaviors and tensile properties10.1016/j.jallcom.2021.159823 ↗
35. Processing defect, microstructure evolution and mechanical properties of laser powder bed fusion Al-12Si alloys10.1016/j.jmrt.2023.07.231 ↗
36. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
37. Denudation of metal powder layers in laser powder bed fusion processes10.1016/j.actamat.2016.05.017 ↗
38. Revealing melt flow instabilities in laser powder bed fusion additive manufacturing of aluminum alloy via in-situ high-speed X-ray imaging10.1016/j.ijmachtools.2022.103861 ↗
39. Heat and fluid flow in additive manufacturing Part I: modeling of powder bed fusion10.1016/j.commatsci.2018.04.022 ↗
40. Mechanisms of processing map difference between laser powder bed fusion of Mg solid cubes and lattice structures
41. Understanding grain evolution in additive manufacturing through modeling
42. Origin of grain orientation during solidification of an aluminum alloy10.1016/j.actamat.2016.05.057 ↗
43. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
44. Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.matchar.2017.11.052 ↗
45. Defects, microstructures and mechanical properties of a box-shaped Ti–6Al–4V alloy part fabricated by laser powder bed fusion
46. Strength-hardness relationship for AlSi10Mg alloy produced by laser powder bed fusion: an experimental study
47. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
48. Influence of Si precipitates on fracture mechanisms of AlSi10Mg parts processed by Selective Laser Melting10.1016/j.actamat.2019.06.013 ↗
49. 3-D finite element analysis of stress concentration factor in spot-welded joints of steel: the effect of process-induced porosity10.1016/j.commatsci.2010.11.033 ↗
50. Defects-dictated tensile properties of selective laser melted Ti-6Al-4V10.1016/j.matdes.2018.08.004 ↗