Effect of heat treatment on microstructures and properties of vacuum laser welding Ti–6Al–4V titanium alloy

Cong Wang, Nuo Xu, Guoyu Zhang, Guojian Xu, Fei Xing

Abstract

Vacuum laser welding of titanium alloys is currently being explored for use in UAVs and military-related fields, but the impact of post-weld heat treatment has been seldom studied. In this paper, the Ti-6Al-4V titanium alloy was welded by vacuum laser welding(VLW)with IPG 50kW fiber laser, and analyze the microstructure and properties of the welds in as-welded state and post-welding heat treatment (850°C/2h/FC(FC:furnace cooling)and 980°C/10min/FC+720°C/2h/FC).The results show that the microstructure of the as-welded weld is composed of primary columnar crystal (primary β phase) and grain boundary martensite (α'), and the microstructure of primary columnar crystal is composed of α'+ (α'+β). The proportion of high-angle grain boundary(HAGB) is 92.3%. The tensile strength is 1009MPa, and the elongation is 9.3%. The average impact toughness at room temperature is 13J. The weld microstructure at 850°C/2h/FC is composed of the acicular α phase and the α+β between the acicular α phases, the primary columnar crystals basically disappear, and the acicular α phases criss-cross weave into the net basket structure.The proportion of HAGB is 97.4%.The tensile strength is 988.3MPa,and the elongation is 14.8%. The average impact toughness is 17J. The microstructure of the weld at 980°C/10min/FC+720°C/2h/FC is composed of the coarser acicular α phase and the (α+β) between the coarser acicular α phases. The proportion of HAGB is about 83.2%. The tensile strength is 586MPa, and the elongation is 1.6%. The average impact toughness is 1.4J.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Wear mechanisms analysis for turning Ti-6Al-4V towards the development of suitable tool coatings10.1007/s00170-011-3427-y ↗
2. Evolution of microstructure and mechanical properties of cold spray additive manufactured aluminum deposit on copper substrate10.1016/j.msea.2023.146024 ↗
3. Multi-scale analyses of phase transformation mechanisms and hardness in linear friction welded Ti17(α+β)/Ti17(β) dissimilar titanium alloy joint10.1016/j.cja.2023.08.018 ↗
4. A review on linear friction welding of Ni-based superalloys
5. Titanium and its alloys [J]
6. High-temperature deformation behavior and recrystallization mechanism of a near beta titanium alloy Ti-55511 in β phase region10.1016/j.msea.2022.143335 ↗
7. LASER SURFACE REINFORCEMENT OF THE Ti/Al TIG WELDED JOINT10.1142/S0218625X2050016X ↗
8. A comparative study of pulsed laser and pulsed TIG welding of Ti5Al2.5Sn titanium alloy sheet10.1016/j.jmatprotec.2016.11.018 ↗
9. Analysis of heterogeneity of fatigue properties of double-sided electron beam welded 140-mm thick TC4 titanium alloy joints
10. Comparative study of fatigue and fracture in friction stir and electron beam welds of 24 mm thick titanium alloy Ti-6Al-4V. Fatigue Fract10.1111/ffe.12434 ↗
11. Microstructure and tensile property of the joint of laser-MIG hybrid welded thick-section TC4 alloy
12. Laser-arc hybrid welding of Ti6Al4V titanium alloy:mechanical characterization of joints and gap tolerance10.1080/09507116.2011.600045 ↗
13. Microstructure characteristics and mechanical properties of laser–TIG hybrid welding joint of TA15 titanium alloy10.1179/143307508X333703 ↗
14. Microstructure characteristics and mechanical properties of laser-TIG hybrid welded dissimilar joints of Ti-22Al-27Nb and TA1510.1016/j.optlastec.2015.04.028 ↗
15. Lütjering · 2007
16. Influence of alloy element partitioning on strength of primary α phase in Ti6Al4V alloy10.1016/j.jmst.2017.07.016 ↗
17. Influence of thermal treatment on element partitioning in α+β titanium alloy
18. Research on microstructure and properties of TC4 titanium alloy MIG welded joints after heat treatment
19. An assessment into mechanical properties and microstructural behavior of TIG welded Ti6Al4V titanium alloy10.1108/GS-11-2019-0052 ↗
20. Enhancing the mechanical properties of electron beam welded TC17 titanium alloy joint by post-weld heat treatment
21. Improving impact toughness of heavy section reduced activation ferritic martensitic CLF-1 steel joints with electron beam welding10.1016/j.jnucmat.2020.152031 ↗
22. Jian. 30 kW-level laser welding characteristics of 5A06 aluminum alloy thick plate under subatmospheric pressure10.1016/j.optlastec.2019.105668 ↗
23. Effects of heat treatment and hot deformation on the secondary α phase evolution of TC8 titanium alloy10.1016/j.msea.2014.06.056 ↗
24. Modeling the hot working behavior of near-α titanium alloy IMI 83410.1016/j.pnsc.2013.11.004 ↗
25. G · Performance and microstructure of TC4 titanium alloy subjected to deep cryogenic treatment and magnetic field[J] · 2023
26. Relationship between lamellar α evolution and flow behavior during isothermal deformation of Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.msea.2012.08.074 ↗
27. Microstructural refinement of boron-containing β-solidifyingγ-titanium aluminide alloys through heat treatments in the β phase field10.1016/j.intermet.2012.08.010 ↗
28. The significant impact of introducing nanosize precipitates and decreased effective grain size on retention of high toughness of simulated heat affected zone (HAZ)10.1016/j.msea.2020.140484 ↗
29. Effect of pre and post weld heat treatments on the microstructure and mechanical properties of fiber optic beam delivery system assisted robotic Nd: yag Laser Welded Ti-6Al-4V Alloy10.24425/123795 ↗
30. Robotic Nd: YAG fiber laser welding of Ti-6Al-4V alloy10.3390/met7060221 ↗