Optimizing corrosion resistance of the Mg–4Zn-0.5Y-0.5Nd alloy by regulation of secondary phase and grain structure
Source abstract
Abstract
The Mg-4Zn-0.5Y-0.5Nd alloy was designed and fabricated using conventional casting and subsequently heat treatment to optimize its microstructure and corrosion properties. The effects of secondary phase morphology and grain structure on the in vitro corrosion behavior of the alloy were systematically investigated to elucidate the corresponding mechanisms. The results show that the T4 treatment coarsens the equiaxed grains and transforms the secondary phase into thin cell skeleton structure with a slight decrease in area fraction. While the T6 treatment reconstructs the secondary phase into bulk ones along the grain boundary and fine ones inside the grain. The T4 treatment changes the corrosion potential and current density of the alloy obviously, but these values are changed by the T6 treatment a little. The As-C alloy has the highest corrosion rate of 0.91 mg·cm -2 ·d -1 , while the T4 alloy with solid solution treatment decreases to 0.65 mg·cm -2 ·d -1 , and the T6 alloy has a middle value between them. Such a corrosion behavior should be mainly ascribed to the evolution of secondary phase morphology and distribution caused by heat treatment. The Mg-Zn-Y-Nd alloys with different states all experience passivation, pitting corrosion, galvanic corrosion, localized corrosion, and extensive corrosion stages, but the duration time of different stages of different alloys differs obviously, which is mainly determined by the secondary phase morphology. Comparatively, the secondary phase with thin cell skeleton structure contributes to corrosion resistance, while the isolated bulk secondary phase accelerates the corrosion. Moreover, the appropriate coarsened grain structure is also beneficial to corrosion resistance. • The solid solution treatment transforms the secondary phase into thin cell skeleton structure, while the solid solution and aging treatment reconstructs the secondary phase into bulk ones along grain boundary and fine ones inside grain. • The solid solution treated alloy exhibits optimum corrosion potential and current density of -1.492 VSCE and 1.21 × 10-5 A·cm-2, respectively. • The solid solution treated alloy exhibits low corrosion rate of 0.65 mg·cm-2·d-1. • The secondary phase with thin cell skeleton structure contributes to corrosion resistance, while the isolated bulk secondary phase accelerates the corrosion. • The appropriate coarsened grain structure is beneficial to corrosion resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (85)
Show source-provided references
1. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
2. In-vitro corrosion behavior of the cast and extruded biodegradable Mg-Zn-Cu alloys in simulated body fluid (SBF)10.1016/j.jma.2021.01.002 ↗
3. Optimizing mechanical property and cytocompatibility of the biodegradable Mg-Zn-Y-Nd alloy by hot extrusion and heat treatment10.1016/j.jmst.2018.09.020 ↗
4. Effect of extrusion process on the mechanical and in vitro degradation performance of a biomedical Mg-Zn-Y-Nd alloy
5. Effects of annealing treatment on microstructure and tensile behavior of the Mg-Zn-Y-Nd alloy10.1016/j.jma.2019.07.011 ↗
6. Overview of magnesium-ceramic composites: mechanical, corrosion and biological properties
7. Advances in degradation behavior of biomedical magnesium alloys: a review10.1016/j.jallcom.2022.164600 ↗
8. Design and nanoengineering of photoactive antimicrobials for bioapplications: from fundamentals to advanced strategies10.1002/adfm.202402607 ↗
9. Degradation mechanism of magnesium alloy stent under simulated human micro-stress environment10.1016/j.msec.2017.12.001 ↗
10. Susceptibility of rare-earth-magnesium alloys to micro-galvanic corrosion10.1016/j.corsci.2010.08.006 ↗
11. Unveiling the effect of Al–Mn intermetallic on the micro-galvanic corrosion of AM50 Mg alloy in NaCl solution
12. Corrosion and biocompatibility improvement of magnesium-based alloys as bone implant materials: a review10.1093/rb/rbx004 ↗
13. Recent advances on the development of magnesium alloys for biodegradable implants10.1016/j.actbio.2014.07.005 ↗
14. Challenges and opportunities for biodegradable magnesium alloy implants10.1080/10667857.2017.1377973 ↗
15. A comprehensive review on biocompatible Mg-based alloys as temporary orthopaedic implants: current status, challenges, and future prospects10.1016/j.jma.2021.09.005 ↗
16. Microstructure design for biodegradable magnesium alloys based on biocorrosion behavior by macroscopic and quasi-in-situ EBSD observations10.1016/j.corsci.2023.111366 ↗
17. Developments in metallic biodegradable stents10.1016/j.actbio.2009.10.006 ↗
18. Critical review on biodegradable and biocompatibility magnesium alloys: progress and prospects in bio-implant applications10.1016/j.inoche.2024.113111 ↗
19. Review of Mg alloy corrosion rates10.1016/j.jma.2020.08.002 ↗
20. Recent advances in biodegradation controls over Mg alloys for bone fracture management: a review10.1016/j.jmst.2018.10.008 ↗
21. NaF assisted preparation and the improved corrosion resistance of high content ZnO doped plasma electrolytic oxidation coating on AZ31B alloy10.1016/j.jma.2023.02.008 ↗
22. Regulating the ablation of nanoparticle-doped MAO coating on Mg alloy by MgF2 passivation layer construction10.1016/j.matlet.2023.135559 ↗
23. Corrosion of magnesium alloys: the role of alloying10.1179/1743280414Y.0000000046 ↗
24. Microstructural evolution, mechanical properties, and corrosion resistance of a heat-treated Mg alloy for the bio-medical application10.1016/j.jma.2018.11.002 ↗
25. A high-specific-strength and corrosion-resistant magnesium alloy10.1038/nmat4435 ↗
26. Towards development of a high-strength stainless Mg alloy with Al-assisted growth of passive film10.1038/s41467-022-33480-w ↗
27. Corrosion and passivation of magnesium alloys10.1016/j.corsci.2016.05.041 ↗
28. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
29. Influence of Zn content on microstructure and tensile properties of Mg–Zn–Y–Nd alloy10.1007/s40195-018-0713-9 ↗
30. The effect of Zn concentration on the corrosion behavior of Mg–xZn alloys10.1016/j.corsci.2012.08.037 ↗
31. Regulating microstructure and mechanical properties of the as-cast Mg-4Zn-0.5 Y-0.5 Nd alloy by heat treatment
32. Micro-alloying of Zn and Ca in vacuum induction casted bioresorbable Mg system: perspectives on corrosion resistance, cytocompatibility, and inflammatory response10.1016/j.jma.2024.07.001 ↗
33. Corrosion and in vitro cytocompatibility investigation on the designed Mg-Zn-Ag metallic glasses for biomedical application10.1016/j.jma.2022.09.025 ↗
34. Effect of the second phases on corrosion behavior of the Mg-Al-Zn alloys10.1016/j.jallcom.2016.11.100 ↗
35. Microstructure, precipitates and compressive properties of various holmium doped NiAl/Cr (Mo, Hf) eutectic alloys10.1016/j.matdes.2011.06.026 ↗
36. Microstructures, mechanical properties, corrosion, and biocompatibility of extruded Mg-Zr-Sr-Ho alloys for biodegradable implant applications10.1016/j.jma.2022.10.002 ↗
37. Effect of rare earth element Ce and La on corrosion behavior of AM60 magnesium alloy10.1016/j.corsci.2009.03.018 ↗
38. Improvement of corrosion resistance of magnesium metal by rare earth elements10.1016/j.electacta.2007.03.027 ↗
39. Revealing the intergranular corrosion mechanism of AA5083 alloys through experiments and atomic-scale computation10.1016/j.jmst.2024.06.055 ↗
40. The role of second phases in the corrosion behavior of Mg–5Zn alloy10.1016/j.corsci.2012.03.030 ↗
41. Development of highly corrosion-resistant Mg-Al-Y extruded alloy via regulating the Mg17Al12 phase10.1016/j.corsci.2024.112124 ↗
42. Investigation of the corrosion for Mg–xGd–3Y–0.4 Zr (x= 6, 8, 10, 12 wt%) alloys in a peak-aged condition10.1016/j.corsci.2007.06.003 ↗
43. Superhydrophobic surface on MAO-processed AZ31B alloy with zinc phosphate nanoflower arrays for excellent corrosion resistance in salt and acidic environments10.1016/j.matdes.2024.112769 ↗
44. Towards developing Mg alloys with simultaneously improved strength and corrosion resistance via RE alloying10.1016/j.jma.2020.08.016 ↗
45. Improved barrier effect of hierarchical micro-nano precipitate framework in magnesium-aluminum alloy for corrosion mitigation10.1016/j.corsci.2023.111220 ↗
46. Investigation of Mg-Zn-Y-Nd alloy for potential application of biodegradable esophageal stent material, bioact10.3390/ma10010001 ↗
47. Microstructural characteristics and mechanical properties of the hot extruded Mg-Zn-Y-Nd alloys10.1016/j.jmst.2020.05.021 ↗
48. Optimization of microstructure and mechanical property of a Mg-Zn-Y-Nd alloy by extrusion process10.1016/j.jallcom.2018.10.167 ↗
49. Anisotropic corrosion behavior of hot-rolled Mg-8 wt.% Li alloy10.1016/j.jmst.2020.04.029 ↗
50. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ9110.1016/j.corsci.2008.04.010 ↗
51. An innovative specimen configuration for the study of Mg corrosion10.1016/j.corsci.2010.09.016 ↗
52. Effects of solute redistribution during heat treatment on micro-galvanic corrosion behavior of dilute Mg-Al-Ca-Mn alloy10.1016/j.corsci.2023.110971 ↗
53. Microstructure and mechanical properties of Mg–Zn–Y–Mn magnesium alloys with different Zn/Y atomic ratio
54. Hot extrusion effect on the microstructure and mechanical properties of a Mg–Y–Nd–Zr alloy10.1007/s11223-018-9958-9 ↗
55. Development of a new magnesium alloy ZW2110.1016/j.matdes.2012.08.040 ↗
56. Designing the heat treatment process for Mg-10Gd-4Y-xZn-0.6 Zr (wt.%) alloy: a study on the transformation of microstructure and properties10.1016/j.jmrt.2024.05.073 ↗
57. Deformation and fracture mechanisms of an annealing-tailored “bimodal” grain-structured Mg alloy10.1016/j.jmst.2019.06.008 ↗
58. Effect of heat treatment on the microstructure and mechanical properties of a multidirectionally forged Mg-Gd-Y-Zn-Zr-Ag alloy10.1016/j.jma.2021.08.037 ↗
59. New insights on corrosion behavior of aging precipitates in dilute Mg-Al-Ca alloy by experiments and first-principles calculations10.1016/j.corsci.2023.111254 ↗
60. Sodium dodecyl sulfate (SDS) intercalated MgAl layered double hydroxides film to enhance the corrosion resistance of AZ31 magnesium alloy10.1016/j.surfcoat.2021.127524 ↗
61. The characteristics of the pitting corrosion of stainless steel above breakdown potential10.1016/0010-938X(83)90080-X ↗
62. Corrosion behavior of Al-6.8 Zn-2.2 Mg-Sc-Zr alloy with high resistance to intergranular corrosion10.1016/j.jmrt.2023.05.017 ↗
63. Effect of microalloyed Ca on the microstructure and corrosion behavior of extruded Mg alloy AZ3110.1016/j.jallcom.2020.153844 ↗
64. Effect of Al/Mn ratio on corrosion behavior of lean Mg-Zn-Ca-Al-Mn alloy processed by twin-roll casting10.1016/j.corsci.2022.110938 ↗
65. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗
66. Formation of abnormal coarse grains and its effects on corrosion behaviors of solution treated ZK60 Mg alloy10.1016/j.corsci.2020.109201 ↗
67. Accurate electrochemical measurement of magnesium corrosion rates; a combined impedance, mass-loss and hydrogen collection study10.1016/j.electacta.2013.12.124 ↗
68. First-principles modeling of corrosion current for passive magnesium alloys and its application in Mg-RE alloy
69. Influence of Ca and Zn on the microstructure and corrosion of biodegradable Mg–Ca–Zn alloys10.1016/j.corsci.2015.01.027 ↗
70. Influence of specific second phases on corrosion behaviors of Mg-Zn-Gd-Zr alloys10.1016/j.corsci.2019.108419 ↗
71. Effect of second phases on the corrosion behaviour of wrought Mg–Zn–Y–Zr alloy10.1016/j.corsci.2010.02.017 ↗
72. Mechanism of adhesion promotion between aluminium sheet and polypropylene with maleic anhydride‐grafted polypropylene by γ‐aminopropyltriethoxy silane10.1002/sia.2871 ↗
73. Study of the corrosion product films formed on the surface of Mg–xZn alloys in NaCl solution10.1016/j.corsci.2014.07.034 ↗
74. Corrosion and wear resistance of micro‐arc oxidation composite coatings on magnesium alloy AZ31—the influence of inclusions of carbon spheres10.1002/adem.201900446 ↗
75. Phase-species-dependent electrochemical and corrosion behaviors of wrought Mg-Y-Zn-based alloys10.1007/s11665-020-05034-y ↗
76. XPS and optical studies of different morphologies of ZnO nanostructures prepared by microwave methods10.1016/j.ceramint.2012.08.075 ↗
77. Magnesium salts and oxide: an XPS overview10.1016/S0169-4332(97)00180-3 ↗
78. Micro-galvanic corrosion behavior and mechanical properties of extruded Mg–2Y–1Zn-0.4 Zr-0.3 Sr alloys with different extrusion temperament immersed in simulated body fluids10.1016/j.matchemphys.2021.124928 ↗
79. Optimized mechanical properties of the hot forged Ti–6Al–4V alloy by regulating multiscale microstructure via laser shock peening10.1016/j.ijmachtools.2024.104192 ↗
80. Microstructure evolution and elevated temperature compressive properties of a rapidly solidified NiAl–Cr (Nb)/Dy alloy10.1016/j.matdes.2008.10.022 ↗
81. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
82. Effect of grain size and crystal orientation on the corrosion behavior of as-extruded Mg-6Gd-2Y-0.2 Zr alloy10.1016/j.corsci.2019.108338 ↗
83. Effect of grain size uniformity and crystallographic orientation on the corrosion behavior of Mg-2Zn-1Al bar10.1016/j.matchar.2021.111374 ↗
84. Role of microstructure and secondary phase on corrosion behavior of heat treated AZ series magnesium alloys10.1016/j.matpr.2019.06.291 ↗
85. Degradation behavior of Mg-based biomaterials containing different long-period stacking ordered phases10.1038/srep03620 ↗