journal article·2023-03Open access

Evolution of iron-rich intermetallics and its effect on the mechanical properties of Al–Cu–Mn–Fe–Si alloys after thermal exposure and high-temperature tensile testing

Lin Bo, He Xiangxiang, Xu Rui, Zhao Yuliang, Lu Yemao, Xiao Huaqiang

Abstract

Si addition is commonly used to modify the iron-rich intermetallics in Al–Cu–Mn–Fe alloys, which is beneficial to increasing the use of recycled aluminum. Most of the available research has focused on the effect of Si content on the room-temperature mechanical properties of Al–Cu–Mn–Fe alloys. To expand the application of Al–Cu–Mn–Fe–Si alloys as light heat-resistant structural components in the automotive and aerospace industries, it is of great importance to investigate the evolution of iron-rich intermetallics and its effect on the fracture behavior of Al–Cu–Mn–Fe–Si alloys after thermal exposure and high-temperature tensile testing. In this work, the evolution of iron-rich intermetallics and the high-temperature mechanical properties of heat-treated Al-6.5Cu-0.6Mn-0.5Fe alloys with different Si contents after thermal exposure and high-temperature tensile testing were assessed by tensile tests, image analysis, scanning electron microscopy, X-Ray diffraction, transmission electron microscopy, and atomic probe tomography. The results indicate that the Al-6.5Cu-0.6Mn-0.5Fe alloys with 0.1Si and 0.5Si additions have excellent and stable high-temperature mechanical properties after long thermal exposure, which are better than those of most heat-resistant Al alloys. The high performance of the high-temperature mechanical properties is attributed to the high heat resistance of secondary intermetallics and precipitated particles. The addition of Si is detrimental to the strength of Al-6.5Cu-0.6Mn-0.5Fe alloys after long thermal exposure. This can be attributed to the solid-state phase transformation of iron-rich intermetallics from α-Fe to β-Fe, which results in the increase of needle-like Fe-rich phases and Si particles, the agglomeration of secondary intermetallics, and the consumption of Al2Cu phases.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Cavitation-resistant intergranular precipitates enhance creep performance of θ′-strengthened Al-Cu based alloys10.1016/j.actamat.2022.117788 ↗
2. Enhancing the tensile strength and heat resistance induced by high-density Ω phases in an Al-Cu-Mg-Ag alloy10.1016/j.jmrt.2022.04.015 ↗
3. Revealing the nucleation and growth mechanisms of Fe-rich phases in Al-Cu-Fe (-Si) alloys under the influence of Al-Ti-B10.1016/j.intermet.2022.107584 ↗
4. 2006
5. Microstructure evolution and properties of 7075 aluminum alloy recycled from scrap aircraft aluminum alloys10.1016/j.jmrt.2022.05.011 ↗
6. Green · 2007
7. Processing map of 2219 Al alloy prepared by internal electromagnetic stirring direct chill casting10.1016/j.jmrt.2022.03.177 ↗
8. Processability, microstructure and precipitation of a Zr-modified 2618 aluminium alloy fabricated by Laser Powder Bed Fusion10.1016/j.jallcom.2022.165346 ↗
9. Mechanical properties of aluminium–copper B206 alloys with iron and silicon additions10.1179/1743133610Y.0000000012 ↗
10. Tensile properties of Al-Cu 206 cast alloys with various iron contents10.1007/s11661-014-2207-3 ↗
11. Effect of Si on Fe-rich intermetallic formation and mechanical properties of heat-treated Al-Cu-Mn-Fe alloys10.1557/jmr.2017.441 ↗
12. Microstructure evolution and mechanical properties of Al-6.5 Cu-0.6 Mn-0.5 Fe alloys with different Si additions10.1016/S1003-6326(19)65065-X ↗
13. Solid-state transformation of Fe-rich intermetallic phases in Al-5.0 Cu-0.6 Mn squeeze cast alloy with variable Fe contents during solution heat treatment10.1016/j.matchar.2015.03.035 ↗
14. Solid-state transformation of iron-rich intermetallic phases in Al-Cu 206 cast alloys during solution heat treatment10.1007/s11661-013-1726-7 ↗
15. Comparative study on microstructures and mechanical properties of the heat-treated Al-5.0 Cu-0.6 Mn-xFe alloys prepared by gravity die casting and squeeze casting10.1016/j.matdes.2014.02.012 ↗
16. Study on thermal expansion of intermetallics in multicomponent Al-Si alloys by high temperature X-ray diffraction10.1016/j.intermet.2010.05.015 ↗
17. Micro-mechanism of simultaneous improvement of strength and ductility of squeeze-cast Al-Cu alloy10.1016/j.msea.2021.142538 ↗
18. Quasicrystalline phases in conventionally cast Fe-containing Al-Cu-Mn alloys and its evolution during the annealing at 530°C
19. Microstructure and phase evolution in A201 alloys with additions of silicon
20. Catalyzed precipitation in Al-Cu-Si10.1007/BF02830329 ↗
21. Kaufman · 1999
22. Microstructure and high temperature tensile properties of Al-Si-Cu-Mn-Fe alloys prepared by semi-solid thixoforming10.1016/S1003-6326(21)65651-0 ↗
23. Thermal exposure of Al-Si-Cu-Mn-Fe alloys and its contribution to high temperature mechanical properties10.1016/j.jmrt.2019.12.018 ↗
24. Eutectic Al-Si-Cu-Fe-Mn alloys with enhanced mechanical properties at room and elevated temperature10.1016/j.matdes.2011.04.005 ↗
25. Effects of Nd on microstructure and mechanical properties of cast Al-Si-Cu-Ni-Mg piston alloys10.1016/j.jallcom.2016.10.300 ↗
26. Characterization of the aging precipitates of Al-12Si-4Cu-2Ni-0.8 Mg-0.2 Gd piston alloy
27. Aluminum alloy for internal-combustion piston, and aluminum alloy piston
28. Heat resistant Al die cast material
29. Contributions to high temperature strengthening from three types of heat-resistant phases formed during solidification, solution treatment and ageing treatment of Al-Cu-Mn-Ni alloys respectively10.1016/j.msea.2019.138819 ↗
30. Solid-state intermetallic phase tranformations in 3XXX aluminium alloys10.1016/S1359-6454(02)00085-X ↗
31. Solid-state phase transformations and reactions
32. Dispersoid particles precipitated during the solutionizing course of Al-12 wt% Si-4 wt% Cu-1.2 wt% Mn alloy and their influence on high temperature strength10.1016/j.msea.2017.04.091 ↗
33. Improvement in elevated-temperature properties of Al-13% Si piston alloys by dispersoid strengthening via Mn addition10.1557/jmr.2018.117 ↗
34. Solute repositioning to tune the multiple microalloying effects in an Al-Cu alloy with minor Sc, Fe and Si addition10.1016/j.msea.2020.140509 ↗
35. Enhanced thermal stability and mechanical properties of high-temperature resistant Al-Cu alloy with Zr and Mn micro-alloying10.1016/S1003-6326(21)65778-3 ↗
36. The role of Si in determining the stability of the θ′ precipitate in Al-Cu-Mn-Zr alloys10.1016/j.jallcom.2020.158152 ↗