journal article·2024-03Open access

Distinctive localized corrosion behavior of β-Mg2Si and α-Al(Fe,Mn)Si phases in a 6082 alloy

Y.H. Gao, X.X. Zhang, Y. Lv, P. Xu, Y.F. Zhao, Y.P. Zhang, C.X. Li, G. Liu

Abstract

6xxx series (Al–Mg–Si) alloys are generally known to be greatly susceptible to localized corrosion, which is closely related to the presence of coarse intermetallic compounds (IMCs). In this work, the localized corrosion behaviour of two representative IMCs, namely β-Mg2Si and α-Al(Fe,Mn)Si, were investigated in a 6082 alloy (Al–Mg–Si–Mn-based). For the β-Mg2Si phase, a rapid de-alloying process is primarily observed. Subsequently, their surface will transform to the electric insulating SiO2 layer, which tends to suppress the further corrosion in its periphery. However, it is found that the α-Al(Fe,Mn)Si phase surprisingly tends to be a potentially effective cathode to promote the initiation of stable localized corrosion, which is contrast with its outstanding corrosion-resistance. Careful examinations reveal that such abnormal corrosion behaviour of α-Al(Fe,Mn)Si is most likely to be relevant to the surface aggregation of Cu impurities, which is clarified by a large number of Cu-rich nanoparticles on its surfaces.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Simultaneous enhancement in mechanical and corrosion properties of Al-Mg-Si alloys using machine learning10.1016/j.jmst.2023.04.072 ↗
2. Intergranular corrosion of AA6082 Al–Mg–Si alloy extrusion: the influence of trace Cu and grain boundary misorientation10.1016/j.jallcom.2020.157228 ↗
3. Effect of artificial aging on intergranular corrosion of extruded AlMgSi alloy with small Cu content10.1016/j.corsci.2005.05.045 ↗
4. Heat treatment-modulated coupling effect of multi-scale second-phase particles on the ductile fracture of aged aluminum alloys10.1016/j.actamat.2006.08.026 ↗
5. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
6. Investigation of the de-alloying behaviour of θ-phase (Al2Cu) in AA2024-T351 aluminium alloy10.1016/j.corsci.2016.03.003 ↗
7. Corrosion behavior of Mg-5.7Gd-1.9Ag Mg alloy sheet10.1016/j.jallcom.2022.165241 ↗
8. Effect of hierarchical precipitates on corrosion behavior of fine-grain magnesium-gadolinium-silver alloy10.1016/j.corsci.2021.109924 ↗
9. Investigation of dealloying of S phase (Al2CuMg) in AA 2024-T3 aluminium alloy using high resolution 2D and 3D electron imaging10.1016/j.corsci.2015.11.013 ↗
10. Observations of intergranular corrosion in AA2024-T351: the influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
11. Pitting corrosion of aluminium10.1016/S0010-938X(99)00012-8 ↗
12. Microstructure and corrosion behaviour of wire arc additive manufactured AA2024 alloy thin wall structure10.1016/j.corsci.2021.109453 ↗
13. When all intermetallics dealloy in AA2024-T3: quantifying early stage intermetallic corrosion kinetics under immersion10.1016/j.corsci.2021.109836 ↗
14. New insights on the initial local corrosion of composite Al7Cu2Fe/Al20Cu2Mn3 intermetallic particles in 2024-T351 aluminum alloy10.1016/j.corsci.2022.110657 ↗
15. Fe-bearing intermetallics transformation and its influence on the corrosion resistance of Al–Mg–Si alloy weld joints10.1016/j.jmrt.2020.11.077 ↗
16. The influence of room temperature storage on intergranular corrosion susceptibility of AA6082 Al-Mg-Si alloy10.1016/j.corcom.2021.09.004 ↗
17. Corrosion of AA2024-T3 Part I. Localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
18. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
19. Dislocation-assisted localised pitting corrosion behaviour of AlSiMgCuMn alloy10.1016/j.corsci.2023.111372 ↗
20. Dealloying of Al2CuMg in alkaline media10.1149/1.1393896 ↗
21. Dealloying below the critical potential10.1149/1.1838046 ↗
22. Enhancing mechanical properties of twin-roll cast Al–Mg–Si–Fe alloys by regulating Fe-bearing phases and macro-segregation10.1016/j.msea.2021.142256 ↗
23. Effect of micro-alloying element La on corrosion behavior of Al-Mg-Si alloys10.1016/j.corsci.2020.109113 ↗
24. Enhanced long-term thermal stability and mechanical properties of twin-roll cast Al–Mg–Si alloys with Mn and Cu additions
25. Effects of Al(MnFe)Si dispersoids with different sizes and number densities on microstructure and ambient/elevated-temperature mechanical properties of extruded Al–Mg–Si AA6082 alloys with varying Mn content10.1016/j.jallcom.2020.157937 ↗
26. The influence of MgSi particle reactivity and dissolution processes on corrosion in Al–Mg–Si alloys10.1016/j.electacta.2008.05.078 ↗
27. A SECM study of redox activity on Al-Mg-Si alloy in organic/aqueous solution10.1016/j.jallcom.2021.161596 ↗
28. The reliability of electrochemical noise and current transients characterizing metastable pitting of Al–Mg–Si microelectrodes10.1016/j.corsci.2013.11.008 ↗
29. Mechanical properties and corrosion behavior of artificially aged Al-Mg-Si alloy10.1016/j.jmrt.2019.11.040 ↗
30. The corrosion behavior of the 6061 Al alloy in simulated Nansha marine atmosphere10.1016/j.jmrt.2022.05.066 ↗
31. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of Al-Cu-Mg-Si alloy10.1016/j.jallcom.2019.152960 ↗
32. The effect of trace level copper content on intergranular corrosion of extruded AA6082-T6 alloys10.1016/j.matchemphys.2023.128303 ↗
33. Localized corrosion of 6056 T6 aluminium alloy in chloride media10.1016/S0010-938X(99)00053-0 ↗
34. Grain boundary structures and their correlation with intergranular corrosion in an extruded Al-Mg-Si-Cu alloy10.1016/j.matchar.2020.110695 ↗
35. Evidence for Cu ion formation by dissolution and dealloying the Al2CuMg intermetallic compound in rotating ring‐disk collection experiments10.1149/1.1393164 ↗
36. Dealloying of Al2CuMg in alkaline media10.1149/1.1393896 ↗
37. Yang M, Li K, Chen H, Wang J, Zhang Z, Yan N, Lu Q, Lan X, Yang T, Zhang Y, Li G, Zhang S, Du Y, Formation of amorphous precipitates in a corroded over-aged Al-Mg-Si alloy, Appl Surf Sci2021;549:149329..10.1016/j.apsusc.2021.149329 ↗
38. The influence of MgSi particle reactivity and dissolution processes on corrosion in Al-Mg-Si alloys10.1016/j.electacta.2008.05.078 ↗
39. Effect of excess silicon and small copper content on intergranular corrosion of 6000-series aluminum alloys10.1149/1.3261804 ↗
40. Corrosion mechanism associated with Mg2Si and Si particles in Al-Mg-Si alloys10.1016/S1003-6326(11)61092-3 ↗
41. Dealloying-driven local corrosion by intermetallic constituent particles and dispersoids in aerospace aluminium alloys10.1016/j.corsci.2020.108947 ↗
42. Pourbaix · 1974 · vol. 307
43. Role of intermetallic phases in localized corrosion of AA5083, Electrochim
44. Corrosion of AA2024-T3 Part III: propagation10.1016/j.corsci.2010.09.035 ↗
45. Evidence for Cu ion formation by dissolution and dealloying the Al2CuMg intermetallic compound in rotating ring-disk collection experiments10.1149/1.1393164 ↗
46. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
47. Localized corrosion evolution associated with intermetallic particles in Al-Cu-Li alloys10.1016/j.matchar.2023.113144 ↗
48. A compilation of corrosion potentials reported for intermetallic phases in aluminum-alloys10.1149/1.2048447 ↗
49. Intergranular corrosion of an Al-Cu-Li alloy: the influence from grain structure10.1016/j.corsci.2022.110845 ↗
50. Effect of copper enrichment on the electrochemical potential of binary Al-Cu alloys10.1149/1.1627343 ↗
51. Laser welding introduced segregation and its influence on the corrosion behaviour of Al-Cu-Li alloy10.1016/j.corsci.2018.02.044 ↗
52. Making sustainable aluminum by recycling scrap: the science of “dirty” alloys10.1016/j.pmatsci.2022.100947 ↗