Mechanical degradation behavior and γ′ coarsening mechanism of a Ni-based superalloy during long-term high-temperature thermal exposure
Source abstract
Abstract
Aero engine design necessitates crucial components, such as turbine discs, to be highly stable in high-temperature environments. Therefore, the accurately determining of the mechanical properties and microstructure evolution of these components under long-term high-temperature exposure is of significant engineering and scientific value. Herein, we systematically analyzed the microstructure and performance evolution of a Ni-based superalloy during long-term high-temperature exposure, explored the relationship between service conditions and yield strength, and introduced novel strength decay factors, namely temperature (|α|) and time (|β|) decay factors. |α| was strongly positively correlated with the exposure temperature, whereas |β| exhibited a more complex behavior and was more affected by the microstructure before thermal exposure, especially at low temperatures (650–700 °C). Microstructural analysis revealed minimal changes in average grain size and Σ3 twin boundaries following long-term thermal exposure. However, γ′ particles coarsened after thermal exposure, particularly at higher temperatures and longer exposure times. The coarsening process under different conditions was examined using Lifshitz–Slyozov–Wagner and trans-interface diffusion-controlled models. The coarsening of γ′ particles led to mechanical degradation, as the critical failure stress decreased with increasing γ′-particle size.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Minimizing intermetallic Laves phase evolution and enhancing precipitation strengthening of Superalloy-718 joints using InterPulse magnetic arc constriction and high frequency pulsation10.1016/j.msea.2023.145323 ↗
2. Discontinuous dynamic recrystallization and nucleation mechanisms associated with 2-, 3- and 4-grain junctions of polycrystalline nickel-based superalloys10.1016/j.matdes.2023.112041 ↗
3. Microstructural origin and control mechanism of the mixed grain structure in Ni-based superalloys10.1016/j.jallcom.2021.163515 ↗
4. Date-drive design of Ni-based turbine disc superalloys to improve yield strength10.1016/j.jmst.2023.01.032 ↗
5. Understanding the fracture mechanisms of Ni-Co-Cr-type superalloys: Role of precipitate evolution and strength degradation10.1016/j.msea.2024.146623 ↗
6. Formation and evolution of M6C carbide in a Ni-W-Cr superalloy10.1016/j.matchar.2023.113211 ↗
7. Interface microstructural evolution, microhardness variation mechanism and 750 °C tensile behavior of the HIPed/FGed PM superalloy plastic bonded joints10.1016/j.jmrt.2024.05.259 ↗
8. Effect of μ precipitation and γ′ evolution on intra-/intergranular strength of Ni-Co-Cr-based superalloys after 800 ℃ thermal exposure10.1016/j.jallcom.2024.175073 ↗
9. Hot deformation characteristics and dynamic recrystallization mechanism of GH4730 Ni-based superalloy10.1016/j.jallcom.2019.01.237 ↗
10. Microstructure-performance relationships in Ni-based superalloy with coprecipitation of γ′ and γ′′ phases10.1016/j.msea.2022.143954 ↗
11. Nitride precipitation and formation in IN617 superalloy during creep10.1016/j.jallcom.2023.169709 ↗
12. Effect of P and B compound strengthening on the evolution of phases and stress rupture properties of the IN718 superalloy during long-term exposure at 650 °C10.1016/j.msea.2023.145386 ↗
13. The evolution of γ′ precipitates and hardness response of a novel PM Ni-based superalloy during thermal exposure10.1016/j.jallcom.2023.168757 ↗
14. Influence of thermal exposure on microstructural stability and tensile properties of a new Ni-base superalloy10.1016/j.jmrt.2022.11.050 ↗
15. Temporal evolution of γ′ precipitate in HAYNES 282 during ageing: growth and coarsening kinetics, solute partitioning and lattice misfit10.1016/j.mtla.2022.101633 ↗
16. Study on the mechanism of γ′ phase rafting in a 4th generation nickel-based single crystal superalloy during thermal exposure at high temperature10.1016/j.jallcom.2024.173594 ↗
17. Microstructural evolution and stress rupture behavior of a Ni-Based wrought superalloy during thermal exposure10.1016/j.msea.2021.141659 ↗
18. Coarsening kinetics of γ′ precipitates in a Re-containing Ni-based single crystal superalloy during long-term aging10.1016/j.jmst.2020.05.034 ↗
19. Investigation of microstructural stability and tensile deformation behavior of a novel PM Ni-based superalloy during long-term thermal exposure10.1016/j.msea.2024.146457 ↗
20. Microstructure, thermal stability and tensile properties of a Ni-Fe-Cr based superalloy with different Fe contents10.1016/j.intermet.2022.107785 ↗
21. Low-temperature tensile properties, deformation and fracture behaviors in the ferrite and austenite duplex stainless steel with various grain sizes10.1016/j.msea.2023.145354 ↗
22. Delineating hardening contributions of secondary and tertiary γ′ particles in an aged Alloy 69310.1016/j.msea.2020.139384 ↗
23. Effect of squareness of initial γ′ precipitates on creep-rupture life of a Ni-based single crystal superalloy at 760/982 °C10.1007/s11661-018-4635-y ↗
24. Effect of heat treatment on microstructure and stress rupture life of DD32 single crystal Ni-base superalloy10.1016/j.msea.2007.01.117 ↗
25. Effect of primary and secondary precipitates on creep strength of Ni-base superalloy single crystals10.1016/S0921-5093(99)00579-1 ↗
26. Aging process design based on the morphological evolution of γ′ precipitates in a 4th generation nickel-based single crystal superalloy10.1016/j.jmst.2022.10.072 ↗
27. Mechanical properties of an Al10Nb20Ta15Ti30V5Zr20A2/B2 refractory superalloy and its constituent phases10.1016/j.actamat.2023.119017 ↗
28. Ricks R.A., Porter A.J., Ecob R.C. The growth of γ′ precipitates in nickel-base superalloys. Acta Metall 1983;31 (1):43–53. doi:10.1016/0001-6160(83)90062-7.10.1016/0001-6160(83)90062-7 ↗
29. Impurity diffusion of Al in Ni single crystals studied by secondary ion mass spectrometry (SIMS)10.1002/pssa.2210640120 ↗
30. Unveiling the Re effect on long-term coarsening behaviors of γ′ precipitates in Ni-based single crystal superalloys10.1016/j.actamat.2022.117979 ↗
31. Interfacial dislocation motion and interactions in single-crystal superalloys10.1016/j.actamat.2014.06.048 ↗
32. Application of a modified Ostwald riening theory in coarsening of γ′ phases in Ni based single crystal superalloys10.1016/j.jallcom.2015.01.215 ↗
33. Coarsening behaviour of a Ni-base superalloy under different heat treatment conditions10.1016/j.msea.2006.12.107 ↗
34. Phase transformations and γ′ phase stability in model CoAlW superalloys10.1016/j.jallcom.2019.05.180 ↗
35. On the proof and uniqueness of Wulff's construction of the shape of minimum surface free energy10.1063/1.1704791 ↗
36. Interdiffusion and its size effect in nickel solid solutions of Ni-Co, Ni-Cr and Ni-Ti systems10.1007/BF00729354 ↗
37. A model for the creep deformation behaviour of nickel-based single crystal superalloys10.1016/j.actamat.2012.05.023 ↗
38. Thermodynamic principle to enhance enzymatic activity using the substrate affinity10.1038/s41467-023-40471-y ↗
39. Multi-component solid solution hardening10.1007/BF00540987 ↗
40. Yield strength prediction in Ni-base alloy 718Plus based on thermo-kinetic precipitation simulation10.1016/j.msea.2014.04.054 ↗
41. A numerical model to predict mechanical properties of Ni-base disk superalloys10.1016/j.ijplas.2018.06.011 ↗
42. Composition and temperature dependence of kinetic behavior of γ′ precipitation in Ni–Al–Cr–Mo quaternary model superalloys: a phase field study10.1016/j.jallcom.2023.172982 ↗
43. Effect of Ti/Nb/Ta addition on γ/γ′ coherent microstructure in low-density and high-strength Co-Al-W-Wo-based superalloys10.1016/j.jmst.2023.11.021 ↗
44. Hall-Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
45. Strengthening mechanisms in polycrystalline multimodal nickel-base superalloys10.1007/s11661-009-9858-5 ↗
46. Microstructural stability and tensile properties of a new γ′ -hardened Ni-Fe-base superalloy10.1016/j.mtla.2021.101061 ↗
47. Effect of long-term exposure on microstructural stability and tensile deformation of a Fe-Ni-based superalloy10.1016/j.msea.2022.143298 ↗
48. Correlation between secondary γ′ and high-temperature tensile behavior of a powder metallurgy nickel-based superalloy EP962NP10.1016/j.msea.2023.144687 ↗
49. Physics and phenomenology of strain hardening: the FCC case10.1016/S0079-6425(02)00003-8 ↗