journal article·2023-05Open access

Additive manufacturing of titanium alloys with enhanced strength and uniform ductility via multi-element alloying

Yingchun Fang, Cheng Liu, Kaihang Jin, Xiao Wei, Xinbao Zhao, Hongbin Bei, Ze Zhang

Abstract

The application of commercially pure titanium (CP–Ti) has long been limited by its insufficient strength and plastic instability. However, strength enhancement typically comes at the expense of ductility since the two important mechanical properties are often mutually exclusive. In the present work, multi-element Fe–Cr–Ni–Mo in the form of 316L steel was added into CP-Ti by additive manufacturing (AM), so as to realize the simultaneous enhancement of strength and uniform ductility. The localized homogenization of CP-Ti and 316L alloy melts during laser melting deposition produced the microstructure comprised of basket-weave ɑ laths, discontinuous ɑGB, and retained β phases, which endowed Ti-1.35Fe-0.36Cr-0.24Ni-0.05Mo alloy with related higher ultimate tensile strength (635 MPa) and larger uniform ductility (12%). This approach could provide guidance for designing high-performance metal materials starting with elements powder through additive manufacturing.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Influence of Fe addition in CP titanium on phase transformation, microstructure and mechanical properties during high pressure torsion10.1016/j.jallcom.2019.153604 ↗
2. Additive manufacturing of a novel alpha titanium alloy from commercially pure titanium with minor addition of Mo2C10.1016/j.mtla.2018.09.033 ↗
3. Preparation, structural and microstructural characterization of Ti-25Ta-10Zr alloy for biomedical applications10.1016/j.jmrt.2019.07.020 ↗
4. Enhancement in mechanical properties of a beta-titanium alloy by high-pressure torsion10.1016/j.jmrt.2014.10.010 ↗
5. Enhancing strength and ductility of pure titanium by interstitial oxygen atoms10.1016/j.msea.2022.143806 ↗
6. A novel cryogenic rolling method for commercially pure titanium sheets featuring high strength and ductility10.1016/j.jallcom.2022.167191 ↗
7. Emerging metallic systems for additive manufacturing: in-situ alloying and multi-metal processing in laser powder bed fusion10.1016/j.pmatsci.2021.100795 ↗
8. Selective laser melting for joining dissimilar materials: investigations of interfacial characteristics and in situ alloying10.1007/s11661-021-06178-9 ↗
9. Evaluation of the mechanical compatibility of additively manufactured porous Ti-25Ta alloy for load-bearing implant applications10.1016/j.jmbbm.2019.05.019 ↗
10. Cost-affordable, biomedical Ti-5Fe alloy developed using elemental powders and laser in-situ alloying additive manufacturing10.1016/j.matchar.2021.111526 ↗
11. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
12. Additive manufacturing of titanium-base alloys with equiaxed microstructures using powder blends
13. Additive manufacturing of fine-grained high-strength titanium alloy via multi-eutectoid elements alloying10.1016/j.compositesb.2022.110399 ↗
14. Interfacial reaction and microstructure investigation of TC4/Co/4J29 diffusion-bonded joints10.1016/j.matlet.2019.06.032 ↗
15. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium10.1016/S0031-8914(34)80244-3 ↗
16. Precipitation of grain boundary α in a laser deposited compositionally graded Ti–8Al–xV alloy – an orientation microscopy study10.1016/j.actamat.2003.09.038 ↗
17. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
18. In-situ alloying of a fine grained fully equiaxed Ti-based alloy via electron beam powder bed fusion additive manufacturing process
19. Development of a pre-heat treatment for obtaining discontinuous grain boundary α in laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe alloy10.1016/j.msea.2014.03.028 ↗
20. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
21. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
22. Achieving grain refinement and ultrahigh yield strength in laser aided additive manufacturing of Ti-6Al-4V alloy by trace Ni addition10.1080/17452759.2021.1949091 ↗
23. Effects of trace Sn and Cr addition on microstructure and mechanical properties of TC17 titanium alloy repaired by wire arc additive manufacturing10.1016/j.jallcom.2021.161473 ↗
24. Laser additive manufacturing of low-cost Ti-Mo alloys: microstructural evolution, phase analysis, and mechanical properties
25. Heterogeneous materials: a new class of materials with unprecedented mechanical properties10.1080/21663831.2017.1343208 ↗
26. Slip transmission behavior across α/β interface and strength prediction with a modified rule of mixtures in TC21 titanium alloy10.1016/j.jallcom.2017.07.002 ↗
27. Tensile deformation behaviors of Ti-6.5Al-3.5Mo-1.5Zr-0.25Si alloy with different percentages of primary α phase10.1016/j.msea.2022.143097 ↗
28. Oxygen-gradient titanium with high strength, strain hardening and toughness10.1016/j.actamat.2023.118674 ↗
29. Role of slip and twinning on strain hardening, and correlation with geometric hardening, latent hardening, and grain boundary strengthening in Titanium10.1016/j.ijplas.2023.103516 ↗
30. On the strain-hardening behavior and twin-induced grain refinement of CP-Ti under ambient temperature compression10.1007/s11661-019-05181-5 ↗
31. Microstructure and tensile properties of laser melting deposited Ti-5Al-5Mo-5V-1Cr-1Fe near beta titanium alloy10.1016/j.msea.2013.08.032 ↗
32. Influence of continuous grain boundary α on ductility of laser melting deposited titanium alloys10.1016/j.msea.2016.03.034 ↗
33. The influence of soft, precipitate-free zones at grain boundaries in Ti and Al alloys on their fatigue and fracture behavior10.1016/j.msea.2006.07.168 ↗
34. Microstructures and mechanical properties of laser-sintered commercially pure Ti and Ti-6Al-4V alloy for dental applications10.3390/ma13030609 ↗
35. Comparison study on microstructure and mechanical properties of Ti-6Al-4V alloys fabricated by powder-based selective-laser-melting and sintering methods10.1016/j.matchar.2020.110358 ↗