Selective laser melting of Ti6Al4V-B4C-BN in situ reactive composites
Source abstract
Abstract
Desire for higher application temperatures and complex geometries for metallic materials has spurred significant development in additive manufacturing (AM) of metal-ceramic composites; however, limited process-microstructure-properties relationships exist for these materials and processing strategies. Herein we investigate the processing window and high-temperature oxidation performance of an in situ reactive, oxidation-resistant titanium metal-matrix composite reinforced with boron nitride (BN) and boron carbide (B4C) via selective laser melting (SLM) to understand the effects of processing parameters on the in situ reactive characteristics and their effects on build reliability and high-temperature oxidation performance. SLM processing required a 50% decrease in overall energy density relative to titanium's optimal parameters to avoid processing failure due to the high in situ reactivity and exothermic reaction between feedstock materials. A precise balance was necessary to combine decreasing the input energy to avoid cracking (due to in situ reactivity) while simultaneously providing enough input energy to keep the bulk density as high as possible to limit porosity that contributed to processing inconsistency at low input energy. Process optimization resulted in composites with as high as 98.3% relative density, comparable to some of the highest metal-ceramic composite densities reported in the AM literature. High-temperature oxidation testing revealed a 39% decrease in oxidation mass gain compared to AM-Ti6Al4V at 850°C, owing directly to ceramic reinforcement. Our results indicate that control of SLM processing parameters can yield advanced composites with enhanced properties and characteristics compared to the base material, revealing an array of design possibilities for researchers and engineers in many fields.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Nature-inspired materials and structures using 3D-Printing10.1016/j.mser.2021.100609 ↗
2. Design and tailoring of alloys for additive manufacturing10.1007/s11661-020-06009-3 ↗
3. Selective laser melting of titanium alloys and titanium matrix composites for biomedical applications: a review10.1002/adem.201500419 ↗
4. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
5. Reactive-deposition-based additive manufacturing of Ti-Zr-BN composites
6. Selective laser melting of in situ titanium-titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
7. Selective Laser Melting process optimization of Ti–Mo–TiC metal matrix composites10.1016/j.cirp.2019.04.120 ↗
8. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB+TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
9. In-situ TiB/near α Ti matrix composites manufactured by selective laser melting
10. Influence of in situ ceramic reinforcement towards tailoring titanium matrix composites using laser-based additive manufacturing
11. Additive manufacturing of reactive in situ Zr based ultra-high temperature ceramic composites
12. Influence of boron nitride on reinforcement to improve high temperature oxidation resistance of titanium
13. Invited review article: metal-additive manufacturing—modeling strategies for application-optimized designs, Addit
14. Effects of laser sintering processing parameters on the microstructure and densification of iron powder10.1016/S0921-5093(03)00341-1 ↗
15. 2016
16. 2015
17. Comparative investigation on microstructures and mechanical properties of (TiB + TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems10.1016/j.matchar.2018.04.010 ↗
18. Characterization of (TiB + TiC)/TC4 in situ titanium matrix composites prepared by laser direct deposition10.1016/j.jmatprotec.2010.11.009 ↗
19. In situ synthesized TiB-TiN reinforced Ti6Al4V alloy composite coatings: microstructure, tribological and in-vitro biocompatibility10.1016/j.jmbbm.2013.09.006 ↗
20. Effect of TiC particle size on the microstructure and tensile properties of TiCp/Ti6Al4V composites fabricated by laser melting deposition10.1016/j.optlastec.2018.03.009 ↗
21. Dry sliding wear characteristics of in-situ TiBw/Ti6Al4V composites with different network parameters10.1016/j.triboint.2018.01.053 ↗
22. In situ multicomponent MMC coating developed on Ti–6Al–4V substrate10.1179/1743294414Y.0000000252 ↗
23. Recent developments and opportunities in additive manufacturing of titanium-based matrix composites: a review10.1016/j.ijmachtools.2018.06.003 ↗
24. Selective laser melting of TiC/Ti bulk nanocomposites: influence of nanoscale reinforcement10.1016/j.scriptamat.2012.04.013 ↗
25. Microstructure evolution and high-temperature oxidation behavior of selective laser melted TiC/TiAl composites10.1016/j.surfcoat.2019.07.059 ↗