Microstructure and properties of spinning deformed A356 alloy subject to the solution-DCT-aging multiplex heat treatment
Source abstract
Abstract
The effect of DCT time (1 h,12 h, 24 h, 36 h and 48 h) on the microstructure and mechanical properties of spinning deformed A356 alloy subject to solution-DCT-aging multiplex heat treatment (hereinafter referred to as “DCT multiplex heat treatment”) was studied. The results demonstrate that the best DCT time of multiplex heat treatment is 36 h, which is the critical time for the recrystallization process. Then the recrystallization texture will appear in the 48 h DCT sample. The equal-area-circle diameter of α-Al matrix and Si phase are 24.8 μm and 1.5 μm respectively after 36 h DCT, which are 53.3% and 53.1% smaller than those after sole solution-aging treatment. After 36 h DCT, the tensile strength, yield strength, elongation and microhardness of A356 alloy arrive at the maximum simultaneously as 302.21 MPa, 272.93 MPa, 20.37% and 98.8HV separately, which are increased by 6.8%, 4.1%, 24.0% and 3.9% in comparison to the sole solution-aged sample. Short-term DCT (<36 h) can increase the residual stress and prompt the dislocation density, while long-term DCT (>36 h) is diametrically opposite. The crystal plane of DCT-ed α-Al matrix rotates towards the (200) crystal plane, and accelerates the formation of nanometer Mg2Si precipitates in the matrix, and twin structure can be observed in the Si crystal. The main strengthening and toughening mechanisms of DCT alloy concerns with fine grain strengthening, precipitation strengthening, dislocation strengthening and twin strengthening.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. The effects of mischmetal, cooling rate and heat treatment on the eutectic Si particle characteristics of A319.1, A356.2 and A413.1 Al-Si casting alloys10.1016/j.msea.2007.07.039 ↗
2. Grain refiner effect on the microstructure and mechanical properties of the A356 automotive wheels10.1007/s11665-013-0596-x ↗
3. A new technology to improve the elongation of A356 alloy10.4028/www.scientific.net/SSP.217-218.450 ↗
4. Recent development in aluminium alloys for the automotive industry10.1016/S0921-5093(99)00653-X ↗
5. Effect of mischmetal modification treatment on the microstructure, tensile properties, and fracture behavior of Al-7.0%Si-0.3%Mg foundry aluminum alloys10.1007/s10853-010-5135-7 ↗
6. Effects of in-situ γ-Al2O3 particles and heat treatment on the microstructure and mechanical properties of A356 aluminium alloy10.1016/j.jallcom.2014.11.212 ↗
7. Enhanced grain refinement of cast aluminum alloy by thermal and mechanical treatment of Al-5Ti-B master alloy10.1016/S1003-6326(13)62631-X ↗
8. Microstructure and properties of FeCoNi1.5CrCu/2024Al composites sintered by microwave10.1016/j.msea.2020.140406 ↗
9. A review of spinning, shear forming and flow forming processes10.1016/S0890-6955(03)00172-X ↗
10. Software tool used for simulation of metal spinning process for complex rotational parts10.4028/www.scientific.net/AMM.657.153 ↗
11. Microstructure evolution and strengthening mechanisms of Mg-6Gd-4Y-0.5Zn-0.5Zr alloy during hot spinning and aging treatment10.1016/j.msea.2021.142035 ↗
12. Optimization of conventional spinning process parameters by means of numerical simulation and statistical analysis
13. Enhanced strength-ductility synergy of aging treated (FeCoNi1.5CrCu)p/2024Al composite10.1016/j.jallcom.2022.167372 ↗
14. Effect of deep cryogenic treatment on mechanical properties and residual stress of AlSi10Mg alloy fabricated by laser powder bed fusion10.1016/j.jmatprotec.2022.117543 ↗
15. Room temperature recovery of cryogenically deformed aluminium alloys10.1016/j.matdes.2020.108819 ↗
16. Effect of deep cryogenic treatment on the artificial ageing behavior of SiCp-AA2009 composite10.3390/met12101767 ↗
17. Nanocrystalline structure fabricated by cryogenic temperature rolling of AA 2099 aluminum alloy10.1016/j.jallcom.2020.158293 ↗
18. Residual stress in engineering materials: a review10.1002/adem.202100786 ↗
19. Recent progress of residual stress measurement methods: a review10.1016/j.cja.2019.10.010 ↗
20. Microstructure and mechanical behavior of Al 7075-T6 subjected to shallow cryogenic treatment10.1007/s11665-016-2052-1 ↗
21. Effect of heat treatment on mechanical properties of Ti-6Al-4V ELI alloy10.1016/j.msea.2008.11.018 ↗
22. The use of β titanium alloys in the aerospace industry10.1007/s11665-013-0728-3 ↗
23. Microstructure and improved plasticity of (FeCoNi1.5CrCu)p/Al composites subject to adjusted deep cryogenic treatment (DCT)10.1016/j.jallcom.2021.162690 ↗
24. Effect of electromagnetic stirring with low current frequency on re distribution in semisolid aluminum alloy
25. Performance and microstructure of TC4 titanium alloy subjected to deep cryogenic treatment and magnetic field10.1016/j.jallcom.2019.06.007 ↗
26. Enhanced strength-ductility synergy in a boron carbide reinforced aluminum matrix composite at 77 K, J. Alloy10.1016/j.jallcom.2019.153310 ↗
27. Microstructure evolution in metastable β titanium alloy subjected to deep cryogenic treatment10.1016/j.msea.2018.03.003 ↗
28. Microstructure study of hot rolling nanosized in-situ Al2O3 particle reinforced A356 matrix composites10.1016/j.jallcom.2020.157107 ↗
29. Microstructure strengthening mechanisms in different equal channel angular pressed aluminum alloys10.1016/j.msea.2012.09.086 ↗
30. Analysis of dislocation nucleation from a crystal surface based on the Peierls–Nabarro dislocation model10.1016/S0022-5096(03)00067-X ↗
31. Evolution of microstructure in semi-solid slurries of rheocast aluminum alloy10.1016/S1003-6326(09)60353-8 ↗
32. Secondary precipitation in Al-Zn-Mg-(Ag) alloys10.1016/S1359-6454(03)00364-1 ↗
33. Self-organized Sr leads to solid state twinning in nano-scaled eutectic Si phase
34. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
35. Effect of TiB2 content on microstructure and mechanical properties of (TiB2p+B4Cp)/Al composites fabricated by microwave sintering10.1016/j.jmrt.2021.05.084 ↗
36. Mechanical properties and dislocation substructure of 6061-T6 aluminum alloy impacted at cryogenic temperatures10.2320/matertrans.M2015170 ↗
37. Evolution of dislocation and stacking-fault densities for a Cu-0.7Cr-0.07Zr alloy during cryogenic tensile test: an in-situ synchrotron X-ray diffraction analysis10.1016/j.msea.2021.141154 ↗
38. Mechanical properties and dislocation substructure of inconel 690 alloy impacted at cryogenic temperatures10.2320/matertrans.M2014165 ↗