journal article·2023-07Open access

Influence of cooling rate on the microstructure and mechanical properties of Al–Cu–Li–Mg–Zn alloy

Qingbo Yang, Wenjing Shi, Miao Wang, Lina Jia, Wenbo Wang, Hu Zhang

Abstract

This work investigated the influence of cooling rate (0.04, 0.87, 15.2 and 156.2 K/s) on the microstructure and compressive properties of Al-4Cu-3Li-0.7Mg-1Zn alloys fabricated by several casting molds. The experiment results revealed that the microstructure cooled at low cooling rates of 0.04, 0.87 and 15.2 K/s is composed of α-Al, α(Al)+T2, θ (Al2Cu), T1 phases and core-shell configuration (Al13Fe4/Al7Cu2Fe phase). This core-shell structure is observed for the first time in an Al-Cu-Li alloy. However, T1 and core-shell configuration vanish at the high cooling rate of 156.2 K/s due to the insufficient diffusion time of Cu, Li and Fe elements. As the cooling rate increases, the average secondary dendrite arm spacing (SDAS) decreases significantly from 110.3 to 7.5 μm and the relationship between SDAS and cooling rate have been established. The average diameter/thickness of the α(Al)+T2, Al2Cu and Al13Fe4/Al7Cu2Fe phases decreases dramatically from 16.9 to 1.0 μm, 8.1 to 0.8 μm and 7.5 to 0.7 μm with the increase of cooling rate, respectively. Fine spherical Al13Fe4/Al7Cu2Fe and Al2Cu phase are beneficial to the improvement of comprehensive compressive properties. Additionally, the solute concentration in the matrix decreases, while the hot-tear resistance and volume fraction of secondary phases increase with increasing cooling rate. The empirical equations are established between (compressive properties, SDAS) and cooling rate. The fracture failure is responsible for the initial hot tearing at low cooling rates, the α(Al)+T2 or Al2Cu or Al13Fe4/Al7Cu2Fe phases at the moderate cooling rate, and the α(Al)+T2 phase at the high cooling rate.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Recent developments in advanced aircraft aluminium alloys [J]10.1016/j.matdes.2013.12.002 ↗
2. Modern Al-Li alloys and prospects of their development [J]10.1007/s11041-013-9603-y ↗
3. Effect of Al3Zr particles on hot compression behavior and processing map for Al-Cu-Li based alloys at elevated temperatures [J]10.1016/S1003-6326(20)65261-X ↗
4. Hot deformation behavior and microstructure of AA2195 alloy under plane strain compression [J]10.1016/j.matchar.2017.06.001 ↗
5. Zhang · 2020 · 160
6. The evolution of Al-Li base products for aerospace and space applications [J]10.1007/s11661-012-1155-z ↗
7. Precipitation behavior of an Al-Cu-Li-X alloy and competing relationships among precipitates at different aging temperatures [J]10.1016/j.msea.2021.141125 ↗
8. Microstructural characteristics and mechanical properties of extruded Al-4Cu-1Li-0.4Mg-0.1Zr-xZn alloy [J]10.1016/j.msea.2018.11.050 ↗
9. Microstructure characteristics of an ultra-high strength extruded Al-4.7Cu-1Li-0.5Mg-0.1Zr-1Zn alloy during heat treatment [J]10.1016/j.jallcom.2019.152216 ↗
10. The effects of cooling rate and heat treatment on mechanical and thermal characteristics of Al-Si-Cu-Mg foundry alloys [J]10.1016/j.jallcom.2014.08.033 ↗
11. Effect of cooling rate on the microstructure and mechanical properties of sand-casting Mg-10Gd-3Y-0.5Zr magnesium alloy [J]10.1016/j.msea.2012.11.016 ↗
12. Effect of cooling rate on microstructure and mechanical properties of an Al-5.0Mg-3.0Zn-1.0Cu cast alloy [J]10.1016/j.jallcom.2019.06.002 ↗
13. Effects of cooling rate on casting ternary Al-Cu-Sc alloy prepared by ultrasound-assisted molten salt electrolysis [J]
14. Effect of cooling rate on microstructure and mechanical properties of sand-casted Al-5.0Mg-0.6Mn-0.25Ce alloy [J]10.1007/s40195-019-00922-2 ↗
15. The role of cooling rate in the microstructure of Al-Fe-Si alloy with high Fe and Si contents [J]10.1016/j.jallcom.2008.06.004 ↗
16. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys [J]10.1016/S0079-6425(03)00037-9 ↗
17. Hot tearing of metals [J]
18. Effect of cooling rate on hot-crack susceptibility of duplex stainless steel [J]10.1016/j.msea.2008.11.036 ↗
19. Investigation on the effect of cooling rate on hot tearing susceptibility of Al2024 alloy using thermal analysis [J]10.1007/s11663-015-0450-7 ↗
20. Determination of three-dimensional grain size distribution by linear intercept measurement [J]10.1016/S1359-6454(97)00442-4 ↗
21. Influence of martensite volume fraction and hardness on the plastic behavior of dual-phase steels: experiments and micromechanical modeling [J]10.1016/j.ijplas.2015.09.006 ↗
22. Microstructural development and mechanical properties of drop tube atomized Al-2.85 wt% Fe [J]10.1016/j.jmst.2021.05.085 ↗
23. The microstructure, fracture mechanism and their correlation with the mechanical properties of as-cast Mg-Nd-Zn-Zr alloy under the effect of cooling rate [J]
24. Underlying causes of poor mechanical properties of aluminum-lithium alloy electron beam welded joints [J]10.1016/j.jmapro.2019.12.052 ↗
25. Effect of Mg level on the microstructure and mechanical properties of die-cast Al-Si-Cu alloys [J]10.1016/j.msea.2015.07.008 ↗
26. Laser cladding of quasicrystal forming Al-Cu-Fe on aluminum [J]10.1016/j.jnoncrysol.2003.12.034 ↗
27. Characterization of pitting corrosion of 7A60 aluminum alloy by EN and EIS techniques [J]10.1016/S1003-6326(14)63550-0 ↗
28. Localized corrosion behavior associated with Al7Cu2Fe intermetallic in Al-Zn-Mg-Cu-Zr alloy [J]10.1016/j.jallcom.2018.12.151 ↗
29. On the phases occurring in alloys of Al with Cu, Mg, Mn, Fe and Si [J]
30. Thermodynamic calculation of the liquidus projections of the Al-Cu-Fe-Si and Al-Cu-Fe-Mg-Si multicomponent systems on Al-rich side [J]10.4028/www.scientific.net/MSF.993.984 ↗
31. On the crystalline and quasi-crystalline phase compounds in an Al-Li-Cu-Mg base alloy [J]10.1016/j.jnoncrysol.2003.11.008 ↗
32. Study of icosahedral quasi-crystalline phase T2-Al6CuLi3 and transformation in 2A97 Al-Li alloy fabricated by laser additive manufacturing [J]10.1016/j.matlet.2022.132014 ↗
33. Effect of variation in the Cu:Mg ratios on the formation of T2 and C phases in AA 8090 alloys [J]10.1016/0956-716X(92)90179-I ↗
34. On the form of the age-hardening response in high strength aluminium alloys [J]10.1016/S0921-5093(01)01054-1 ↗
35. The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys [J]10.1016/j.actamat.2012.12.041 ↗
36. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al-Li-Cu-X alloy [J]10.1016/S1471-5317(00)00002-X ↗
37. Ag and Zn minor solute additions on the precipitation kinetics and strengthening of an Al-Cu-Li alloy [J]10.1016/j.actamat.2017.05.029 ↗
38. Yang · 2022
39. Effect of dendritic arm spacing on mechanical properties and corrosion resistance of Al 9 Wt Pct Si and Zn 27 Wt Pct Al alloys [J]10.1007/BF02586225 ↗
40. Correlation between unsteady-state solidification conditions, dendrite spacings, and mechanical properties of Al-Cu alloys [J]10.1007/s11661-000-0096-0 ↗
41. Modeling dendritic structure and mechanical properties of Zn-Al alloys as a function of solidification conditions [J]10.1016/S0921-5093(01)01455-1 ↗
42. Mechanical properties as a function of microstructure in the new Mg-Al-Ca-La alloy solidified under different conditions [J]10.1016/j.msea.2010.03.041 ↗
43. Improved prediction of the grain size of aluminum alloys that includes the effect of cooling rate [J]10.1016/j.msea.2007.11.009 ↗
44. A simple model for dendrite arm coarsening during solidification [J]10.1016/0025-5416(85)90319-2 ↗
45. Dendrite morphology microsegregation and homogenization of low-alloy steel [J]
46. Solidification processing [J]10.1007/BF02643923 ↗
47. Effect of cooling rate on the thermal and electrical conductivities of an A356 sand cast alloy [J]
48. Experimental study of structure formation in binary Al-Cu alloys at different cooling rates [J]10.1016/j.msea.2005.05.105 ↗
49. The evolution of the growth morphology in Mg–Al alloys depending on the cooling rate during solidification [J]10.1016/j.actamat.2013.04.063 ↗
50. The solidification behavior of 8090 Al-Li alloy [J]10.1007/BF02663146 ↗
51. The sequence of intermetallics formation during the solidification of an Al-Mg-Si alloy containing La [J]10.1007/s11661-010-0453-6 ↗
52. Microstructural aspects of the dissolution and melting of Al2Cu phase in Al-Si alloys during solution heat treatment [J]10.1007/BF02651928 ↗
53. The effect of sc addition on microstructure and mechanical properties of as-cast Zr-containing Al-Cu alloys [J]
54. The effect of volume fraction on particle coarsening: theoretical considerations [J]10.1016/0001-6160(72)90114-9 ↗
55. Two-dimensional modelling and experimental study on microsegregation during solidification of an Al-Cu binary alloy [J]10.1016/j.actamat.2006.10.035 ↗
56. Undercooling effects in microsegregation modelling [J]10.1016/1359-6462(96)00081-4 ↗
57. Discussion of “Effect of dendrite arm coarsening on microsegregation” [J]10.1007/s11661-998-0120-3 ↗
58. The influences of grain size and morphology on the hot tearing susceptibility, contraction, and load behaviors of AA7050 alloy inoculated with Al-5Ti-1B master alloy [J]10.1007/s11661-016-3543-2 ↗
59. Role of grain refinement in the hot tearing of cast Al-Cu alloy [J]10.1007/s11663-013-9801-4 ↗
60. An analysis of the effect of grain refinement on the hot tearing of aluminium alloys [J]
61. Deformation, strength, and fracture above the solidus temperature [J]
62. The aging behavior of Ni-coated carbon fibers and ZrC particles reinforced 2024Al matrix composites [J]10.1016/j.jallcom.2022.165468 ↗
63. Effects of intensive forced melt convection on the mechanical properties of Fe containing Al-Si based alloys [J]10.1016/j.msea.2006.09.038 ↗
64. Microstructures and tensile fracture behavior of 2219 wrought Al-Cu alloys with different impurity of Fe [J]10.3390/met11010174 ↗