Effect of additional side shielding on the wire arc additive manufacturing of AZ31 magnesium alloy
Source abstract
Abstract
Magnesium (Mg) alloys have a low density among the structural metals, but it is hard to be plastically deformed due to their crystallographic nature. Wire arc additive manufacturing (WAAM) could be one of the alternative processes to fabricate the Mg products for various industrial applications. Nonetheless, it is used in limited industrial fields due to challenging issues such as low commercial availability of wire, high oxygen affinity, explosive and flammable hazard, and typical defects of WAAM like distortion and side collapse, grain coarsening, etc. In this research, it was tried to find out the better way to fabricate the WAAM of AZ31 alloy. An additional Ar gas side shielding was given during the WAAM process, and compared with the conventional shielding method. It was observed that the global shielding affects the microstructural evolution of the WAAM product, and influences the mechanical property in a positive way.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Thermal process and material flow during dissimilar double-sided friction stir spot welding of AZ31/ZK60 magnesium alloys10.1016/j.jmrt.2022.01.097 ↗
2. Smith · 1993
3. Wire-arc additive manufacturing of AZ31 magnesium alloy fabricated by cold metal transfer heat source: processing, microstructure, and mechanical behavior10.1016/j.jmatprotec.2020.116895 ↗
4. Additive manufacturing of magnesium alloys
5. Applications of magnesium and its alloys: a review
6. Formability, microstructure evolution and mechanical properties of wire arc additively manufactured AZ80M magnesium alloy using gas tungsten arc welding10.1016/j.jma.2020.01.003 ↗
7. Development of a high strength magnesium alloy for wire arc additive manufacturing10.3390/met10060778 ↗
8. Additive manufacturing of biodegradable metals: current research status and future perspectives10.1016/j.actbio.2019.04.046 ↗
9. Mg-alloys for forging applications-A review10.3390/ma13040985 ↗
10. The microstructure and mechanical properties of AZ31 magnesium alloy aircraft brackets produced by a new forging Technology10.1016/j.promfg.2015.07.059 ↗
11. Luo · 2012
12. Moosbrugger · 2017
13. Review on the wire arc additive manufacturing process and trends in non-ferrous alloys10.5781/JWJ.2021.39.6.5 ↗
14. Material-property evaluation of magnesium alloys fabricated using wire-and-arc-based additive manufacturing
15. Dimension precision and uniformability depending on the interpass distance variation of automated-wire arc additive manufacturing using 5 Cr-4 Mo tool steel alloy10.5781/JWJ.2021.39.6.6 ↗
16. Effect of filler metal type on microstructure and mechanical properties of fabricated nial bronze alloy using wire arc additive manufacturing system
17. Additive manufacturing of biodegradable magnesium implants and scaffolds: review of the recent advances and research trends10.1016/j.jma.2020.09.014 ↗
18. Effect of shielding gases on the wire arc additive manufacturability of 5 Cr – 4 Mo tool steel for die casting mold making10.3365/KJMM.2020.58.12.852 ↗
19. Fundamental experiments of pulsed GMA additive manufacturing10.5781/JWJ.2022.40.1.9 ↗
20. Recent progress and perspectives in additive manufacturing of magnesium alloys10.1016/j.jma.2022.03.001 ↗
21. Research on mechanisms and controlling methods of macro defects in TC4 alloy fabricated by wire additive manufacturing10.3390/ma11071104 ↗
22. Wire and arc additive manufacturing of 316L stainless steel/Inconel 625 functionally graded material: development and characterization10.1016/j.jmrt.2022.08.169 ↗
23. Concept and validation of an active cooling technique to mitigate heat accumulation in WAAM10.1007/s00170-020-05201-4 ↗
24. Effect of additional shielding gas on welding seam formation during twin wire DP-MIG high-speed welding10.3390/app8091658 ↗
25. Keränen · 2010
26. Bhattacharyya · 2020
27. High-speed welding of stainless steel with additional compensatory gas jet blow molten pool10.3390/app8112170 ↗
28. Air-cooling influence on wire arc additive manufactured surfaces10.4028/www.scientific.net/KEM.813.241 ↗
29. Increasing the manufacturing efficiency of WAAM by advanced cooling strategies10.1007/s40194-020-00930-2 ↗
30. Wire and arc additive manufacturing of high-strength low-alloy steel: microstructure and mechanical properties10.1002/adem.202001036 ↗
31. Increased shielding of a direct energy deposition process to enable deposition of reactive materials; an investigation into deposition of 15-5 PH stainless steel, inconel 718 and Ti-6Al-4V10.1016/j.cirpj.2020.11.013 ↗
32. Techno-economic evaluation of reducing shielding gas consumption in GMAW whilst maintaining weld quality10.1007/s00170-012-3961-2 ↗
33. The effects of forced interpass cooling on the material properties of wire arc additively manufactured Ti6Al4V alloy10.1016/j.jmatprotec.2018.03.024 ↗
34. Wire Arc additive manufacturing (WAAM) of aluminum alloy AlMg5Mn with energy-reduced gas metal arc welding (GMAW)10.3390/ma13122671 ↗
35. ASTM; B91-12; ASTM International: West Conshohocken, PA, USA, 2012.
36. Microstructure and mechanical properties of as-cast AZ31 with the addition of Sb10.1016/j.msea.2008.07.010 ↗
37. Influence of the composition of the hank's balanced salt solution on the corrosion behavior of AZ31 and AZ61 magnesium alloys10.3390/met7110465 ↗
38. The influence of manganese on the microstructure and mechanical properties of AZ31 gravity die cast alloys10.1016/j.actamat.2006.02.039 ↗
39. Effects of manganese addition on microstructure and press formability of hot-rolled Mg-Al-Zn alloy sheets10.1557/JMR.2008.0368 ↗
40. Effect of β–Mg17Al12 phase on microstructure, texture and mechanical properties of AZ91 alloy processed by asymmetric hot rolling10.1016/j.msea.2018.09.086 ↗
41. Wire-arc directed energy deposition of magnesium alloys: microstructure, properties and quality optimization strategies10.1016/j.jmrt.2022.07.083 ↗
42. Investigation of Co-Cr-Fe-Mn-Ni non-equiatomic high-entropy alloy fabricated by wire arc additive manufacturing10.3390/met12020197 ↗
43. Thermo-mechanical modelling of wire-arc additive manufacturing (WAAM) of semi-finished products10.3390/met8121009 ↗
44. Grain refinement of AZ31 magnesium alloy weldments by AC pulsing technique10.1007/s11661-012-1241-2 ↗
45. Corrosion of Mg-9Al alloy with minor alloying elements (Mn, Nd, Ca, Y and Sn)10.1016/j.matdes.2017.05.048 ↗
46. Effect of welding variables on the quality of weldments