journal article·2024-01Open access

Microstructure and mechanical properties of T2 copper /316L stainless steel explosive welding composite with small size wavy interface

Lei Zhu, Qiang Zhou, Congbin Song, Linjie Liu, Linjie Zhang, Keshe Fan, Yudong Zhang, Honghong Lu, Qiwen Hu, Zemin Sheng, Yansong Guo, Kaiyuan Liu

Abstract

Copper/stainless steel composite is often used for preparation of superconducting busbar “double box” lap joints. However, it is a challenge for the large thickness T2 copper/316L stainless steel composite is fabricated by explosive welding, because of the bonding interface is always present many problems such as large ripple size, many microscopic defects, low bonding strength and poor sealing etc. In this paper, the big-thickness T2 copper/316L stainless steel composite with small size wavy interface was successfully fabricated by explosive welding. Microstructure of bonding interface indicated that the welding process could be divided into three stages: detonation growth stage, detonation stabilization stage, detonation descent stage. The morphology of bonding interface presented a regular wavy interface and no defects such as cracks, voids and intermetallic compound were formed in the stable stage, which was consistent with the results of ultrasonic and permeability quality inspection. The hardness of copper side and stainless steel side close to the bonding interface reached 131HV and 432HV, respectively. Dynamic recrystallization and fine grain generated in the bonding interface. The mechanical properties of tensile strength, pull-off strength and shear strength in the stable detonation stage is greater than 110 MPa, which is meeting the requirements of preparation of superconducting busbar “double box” lap joints. The deformation failure mainly occurred in the copper side near the bonding interface, which presented a higher bonding strength than copper. Some dimples and tearing edges with different sizes on the fracture surfaces, indicating that the fracture was a typical ductile fracture.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Evaluation of diffusion welding of 6061 aluminum and AZ31 magnesium alloys without using an interlayer[J]10.1016/j.matdes.2014.09.020 ↗
2. Laser impact welding for joining similar and dissimilar metal combinations with various target configurations[J]
3. Design and R&D results of the joints for the ITER conductor[J
4. Operational limits and disruptions[J]10.1088/0029-5515/47/6/S03 ↗
5. Recent experiments in the east and ht-7 superconducting tokamaks[J]
6. Tsuji · 2008
7. Compromise between magnetic shielding and mechanical strength of thin Al/Steel/Al sandwiches produced by cold roll bonding: experimental and numerical approaches[J]10.1016/j.jallcom.2019.05.243 ↗
8. Diffusion bonding of commercially pure titanium to 304 stainless steel using copper interlayer10.1016/j.msea.2005.07.010 ↗
9. Porosity and microstructure in pulsed Nd:YAG laser welded Ti6Al4V sheet10.1016/j.jmatprotec.2014.01.015 ↗
10. Investigation of interfacial structure and mechanical properties of titanium clad steel sheets prepared by a brazing-rolling process10.1016/j.msea.2017.06.095 ↗
11. Strain rate sensitivity of Al-Fe magnetic pulse welds10.1016/j.jmatprotec.2018.06.021 ↗
12. Effect of microstructure on mechanical properties of titanium-steel explosive welding interface
13. Development of superconducting joint for TOKAMAK feeder busbar[J]10.1016/j.fusengdes.2018.11.005 ↗
14. Design proposal for the ITER feeder busbars10.1109/TASC.2010.2041535 ↗
15. Current sharing temperature of NBTI sultan samples compared to prediction using a single pinning mechanism parametrizationfor NBTI strand10.1088/0953-2048/25/5/054011 ↗
16. Comprehensive microstructural investigation during dissimilar transient liquid phase bonding cobalt-based superalloys by BNi-9 amorphous interlayer foil [J]10.1016/j.jmrt.2021.05.069 ↗
17. The effect of holding time on dissimilar transient liquid-phase-bonded properties of super-ferritic stainless steel 446 to martensitic stainless steel 410 using a nickel-based interlayer[J]10.3390/mi13111801 ↗
18. Comprehensive microstructural and mechanical characterization of transient liquid phase bonded austenitic stainless steel by Ni–Cr–Si–B amorphous interlayer[J]10.1016/j.ijpvp.2023.105078 ↗
19. Experimental and numerical investigation on interface microstructure and phase constitution of radiation resistant Pb/316L stainless steel explosive welded composite plate[J]10.1016/j.jmrt.2023.03.141 ↗
20. Interfacial investigations on the microstructure evolution and thermomechanical behavior of explosive welded CLAM/316L composite[J]10.1016/j.jmrt.2023.06.180 ↗
21. Experimental and numerical investigation of interface and mechanical properties of Al0.3CoCrFeNi/304L explosively weld composite plate[J]10.1016/j.jmrt.2023.07.079 ↗
22. A novel dynamic self-constrained explosive welding method for manufacturing copper-steel bimetallic tube[J]10.1016/j.jmrt.2023.05.019 ↗
23. Effect of the post-weld heat treatment temperature on the mechanical properties and microstructure of magnetic pulse welded Al/Fe tubes[J]10.1016/j.jmrt.2021.10.074 ↗
24. Structure and mechanical properties of aluminum alloy/Ag interlayer/steel non-centered electron beam welded joints[J]10.1016/S1003-6326(11)61096-0 ↗
25. Tensile behavior of the titanium-steel explosive welded interface under quasi-static and high-strain rate loading[J]
26. Microstructure characterization and tensile shear failure mechanism of the bonding interface of explosively welded titanium-steel composite[J]10.1016/j.msea.2021.141559 ↗
27. Production Development and elimination of boundary effect in explosive welding[J]
28. High cooling rates and metastable phases at the interfaces of explosively welded materials10.1016/j.actamat.2017.06.038 ↗
29. Hierarchical microstructure of explosive joints: example of titanium to steel cladding10.1016/j.msea.2010.11.092 ↗
30. Microstructural and microanalysis investigations of bond titanium grade1/low alloy steel st52-3N obtained by explosive welding10.1016/j.jallcom.2016.02.120 ↗
31. Numerical simulation of wave formation in an oblique impact of plates by the method of molecular dynamics10.1134/S0021894412060144 ↗
32. The mechanics of wave formation in ExplosiveWelding [J]
33. Flow configurations in colliding plates: explosive bonding[J]10.1063/1.1729565 ↗
34. Explosive welding of aluminium to stainless steel using carbon steel and niobium interlayers[J]10.1016/j.jmatprotec.2020.116707 ↗
35. Interfaces of the 5083Al/1060Al/TA1/Ni/SUS304 five-layer composite plate fabricated by explosive welding10.1016/j.jmrt.2022.04.157 ↗
36. Chu · 2017
37. Microstructure development during explosive welding of metal foil:morphologies, mechanical behaviors and mechanisms[J]
38. High cooling rates and metastable phases at the interfaces of explosively welded materials10.1016/j.actamat.2017.06.038 ↗
39. Development of dynamic recrystallization theory10.1016/j.msea.2004.01.064 ↗
40. Zhang · 2019
41. Examination of copper/stainless steel joints by explosive welding[J]10.1016/j.matdes.2004.07.021 ↗
42. Investigation of effect of the stand-off distance on interface characteristics of explosively welded copper and stainless10.1016/j.matdes.2007.07.012 ↗
43. Anisotropy in microstructure and shear properties of TA2/Q235 explosive welding interfaces10.1016/j.jmrt.2023.07.080 ↗
44. Investigations on microstructural characteristics and mechanical properties of 316 L stainless steel welded joints using nickel coated filler material by gas tungsten arc welding[J]
45. Intermetallic reaction of the bonding interface of TA2/q235 explosive welding composite