Abstract
In-situ metal matrix composites are desirable for achieving optimum mechanical properties. This study investigated the enhancement of mechanical performance in Hastelloy X (HX) superalloy through in-situ synthesis of TiC and γ′ phases via titanium (Ti) addition using a high-throughput laser additive manufacturing system. The influence of Ti content on phase evolution, microstructure, and mechanical properties was comprehensively analyzed for both the as-deposited and heat-treated HX superalloys. The results revealed that increasing Ti content exacerbated micro-segregation during the deposition, promoting pronounced dendritic growth and a higher σ phase volume fraction. These microstructural changes enhanced tensile strength while concurrently elevated cracking susceptibility, with macroscopic cracking detected upon reaching 5 wt% Ti. Following heat treatment, micro-segregation was significantly reduced. In alloys containing 2–4 wt% Ti, TiC and nano-sized γ′ phases precipitated after heat treatment, leading to a 40 % improvement in yield strength and tensile strength compared to the baseline HX superalloy, while maintaining an elongation of approximately 30 %.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Novel selective laser melting processed in-situ TiC particle-reinforced Ni matrix composite with excellent processability and mechanical properties10.1016/j.msea.2020.140145 ↗
2. Study of the microstructure and cracking mechanisms of Hastelloy X produced by laser powder bed fusion10.3390/ma11010106 ↗
3. Identification of heterogeneous constitutive model of laser additive manufactured materials based on nano-indentation test and orthogonal metal cutting10.1016/j.jmrt.2024.12.041 ↗
4. High‐throughput preparation for alloy composition design in additive manufacturing: a comprehensive review10.1002/mgea.55 ↗
5. High‐throughput experimental techniques for corrosion research: a review10.1002/mgea.20 ↗
6. Laser powder bed fusion of Mg–Zn–Zr alloy: formability, microstructure evolution and biodegradation behavior10.1016/j.jmrt.2024.09.015 ↗
7. Influence of boron on the stress-rupture behavior of an additively manufactured Hastelloy X10.1016/j.msea.2022.144483 ↗
8. On the effect of laser powder-bed fusion process parameters on quasi-static and fatigue behaviour of Hastelloy X: a microstructure/defect interaction study
9. Microstructure-performance relationships in gas tungsten arc welded Hastelloy X nickel-based superalloy10.1016/j.msea.2020.139861 ↗
10. Customizing mechanical properties of additively manufactured Hastelloy X parts by adjusting laser scanning speed10.1016/j.jallcom.2019.152097 ↗
11. Room temperature mechanical properties of additively manufactured Ni-base superalloys: a comparative study10.1016/j.prostr.2022.03.012 ↗
12. Effect of heat treatment on the microstructural evolution and mechanical properties of GH4099 additive-manufactured by directed energy deposition10.1016/j.jallcom.2019.05.348 ↗
13. Evolution of aluminide coating microstructure on nickel-base cast superalloy CM-247 in a single-step high-activity aluminizing process10.1007/s11661-998-0042-0 ↗
14. Effect of solution-treatment on microstructure and mechanical properties of cast fine-grain CM 247 LC superalloy10.2320/matertrans.45.1360 ↗
15. Microstructural evolution of GH4079 superalloy during hot deformation and heat treatment10.1016/j.jmrt.2024.09.030 ↗
16. Cracking during thermal post-processing of laser powder bed fabricated CM247LC Ni-superalloy10.1016/j.matdes.2019.107793 ↗
17. Thermal cycling on microstructure and mechanical properties of laser powder bed fusion manufactured IN738LC alloy10.1007/s12598-024-02851-1 ↗
18. Alloys-by-design: application to new superalloys for additive manufacturing10.1016/j.actamat.2020.09.023 ↗
19. The effect of Al2O3-nanoparticles as the reinforcement additive on the hot deformation behavior of 7075 aluminum alloy10.1016/j.matdes.2015.09.009 ↗
20. Electron beam melted TiC/high Nb–TiAl nanocomposite: microstructure and mechanical property10.1016/j.msea.2021.141059 ↗
21. Selective laser melting of Hastelloy X nanocomposite: effects of TiC reinforcement on crack elimination and strength improvement10.1016/j.compositesb.2020.108442 ↗
22. Laser additive manufacturing of ultrafine TiC particle reinforced Inconel 625 based composite parts: tailored microstructures and enhanced performance10.1016/j.msea.2015.03.043 ↗
23. Additive manufacturing of oxide-dispersion strengthened alloys: materials, synthesis and manufacturing10.1016/j.pmatsci.2022.101049 ↗
24. In situ TiC particle-reinforced FeCoCrNiCu high entropy alloy matrix composites by induction smelting10.1007/s12666-020-02135-z ↗
25. Tuning heterogeneous microstructures to enhance mechanical properties of nano-TiN particle reinforced Haynes 230 composites by laser powder bed fusion10.1007/s12598-024-02677-x ↗
26. Preparation of iron-based composites reinforced with submicron/nano-sized TiC ceramic particles by in-situ reaction in melts and one-step integrated hot pressing densification10.1016/j.ceramint.2024.11.416 ↗
27. Novel method to achieve synergetic strength–ductility improvement of Al–Cu alloy by in situ TiC–TiB2 particles via direct reaction synthesis10.1016/j.msea.2023.144810 ↗
28. Interfacial phenomena in Fe/stainless steel–TiC systems and the effect of Mo10.1515/htmp-2013-0082 ↗
29. Effects of hot isostatic pressing treatment on the microstructure and tensile properties of Ni-based superalloy CM247LC manufactured by selective laser melting10.1016/j.msea.2022.143083 ↗
30. Additive manufacturing of high-strength crack-free Ni-based Hastelloy X superalloy
31. Tailoring the microstructure and mechanical properties for Hastelloy X alloy by laser powder bed fusion via scanning strategy10.1016/j.matdes.2023.112386 ↗
32. Powder recycling effects on porosity development and mechanical properties of Hastelloy X alloy during laser powder bed fusion process
33. Control of crystallographic texture and mechanical properties of hastelloy-X via laser powder bed fusion10.3390/cryst11091064 ↗
34. On the orientation dependent microstructure and mechanical behavior of Hastelloy X superalloy fabricated by laser powder bed fusion10.1016/j.msea.2022.143208 ↗
35. Effects of microstructure on mechanical properties of GH3536 alloy fabricated by selective laser melting
36. Microstructure and hot tensile behavior of Hastelloy X superalloy laser powder-bed fusion-fabricated through different scanning patterns10.1016/j.msea.2023.144717 ↗
37. Effect of Al content on microstructure and microhardness of Inconel 718 superalloy fabricated by laser additive manufacturing10.1016/j.jmrt.2021.12.127 ↗