Enhancing corrosion and wear resistance of a 7075 aluminum alloy via depositing TC4 coating
Source abstract
Abstract
Aluminum alloys have been widely used in engineering due to their high strength and low density. However, their poor corrosion and wear resistance have largely limited their application in marine equipment. This study successfully improved the corrosion and wear resistance of a typical 7075 Al alloy by depositing a high-performance TC4 titanium alloy coating using in-house annular laser cladding equipment. Microstructural investigations revealed that the defect-free TC4 coating is metallurgically bonded to the 7075 Al alloy substrate along with excellent bond strength. Electrochemical test results showed that compared to the hot-forged 7075 Al alloy and hot-forged double-phase TC4 bulk alloy, the TC4 coating exhibits superior corrosion resistance due to its net-basket α-single-phase microstructure. Further, wear testing results showed that the coefficient of friction and wear volume of the TC4 coating are far lower than that of 7075 Al alloy. The enhanced wear resistance is closely related to the high hardness of the TC4 coating and its excellent fatigue-wear resistance. Therefore, this work can serve as a reference to improve Aluminum alloys' corrosion and wear resistance by depositing Titanium alloy coatings using the annular laser cladding process, which shall widen the potential applications of Aluminum alloys in marine equipment.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Mechanical and tribological properties of 5A06 aluminum alloy at low temperature10.1088/2051-672X/acb72c ↗
2. Comparative study on the fretting wear property of 7075 aluminum alloys under lubricated and dry conditions
3. Enhancement of corrosion resistance of a high Zn-yttrium aluminum alloy
4. Mechanical properties and corrosion resistance enhancement of 2024 aluminum alloy for drill pipe after heat treatment and Sr modification
5. Microstructure and properties of Ti/TiBCN coating on 7075 aluminum alloy by laser cladding10.1016/j.surfcoat.2017.11.034 ↗
6. Microstructure and high-temperature properties of laser cladded AlCoCrFeNiTi0.5 high-entropy coating on Ti 6Al-4V alloy
7. Annealed microstructure dependent corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy10.1016/j.jmst.2020.05.058 ↗
8. The corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy: effects of HCl concentration and temperature10.1016/j.jmst.2020.08.066 ↗
9. Effect of laser shock peening on the corrosion properties of Ti-6Al-3Nb-2Zr-1Mo alloy10.1016/j.surfcoat.2022.128425 ↗
10. Tuning microstructure and enhancing corrosion property of Ti-6Al-3Nb-2Zr-1Mo alloy through electron beam surface melting10.1016/j.corsci.2022.110520 ↗
11. Bonding and wear behaviors of supersonic plasma sprayed Fe-based coatings on Al-Si alloy substrate10.1016/j.surfcoat.2019.04.003 ↗
12. Effect of MoS2 content on microstructure and properties of supersonic plasma sprayed Fe-based composite coatings10.1016/j.surfcoat.2020.125699 ↗
13. Tuning the microstructure and mechanical properties of additive manufactured aluminum matrix composites by cold spray
14. Comparative study of coatings with different molybdenum equivalent on titanium alloy forged plate for laser cladding: microstructure and mechanical properties
15. Mechanical behavior of Ti cold spray coatings determined by a multi-scale indentation method10.1016/j.msea.2011.09.083 ↗
16. Corrosion resistant nickel coating with strong adhesion on AZ31B magnesium alloy prepared by an in-situ shot-peening-assisted cold spray10.1016/j.corsci.2018.04.018 ↗
17. Residual stress development in cold sprayed Al, Cu and Ti coatings10.1016/j.actamat.2013.06.033 ↗
18. Effect of thermal energy on the deposition behaviour, wear and corrosion resistance of cold sprayed Ni-WC cermet coatings
19. Effects of Al2O3 on the microstructures and corrosion behavior of low-pressure cold gas sprayed Al 2024-Al2O3 composite coatings on AA 2024-T3 substrate10.1016/j.surfcoat.2019.04.082 ↗
20. Additively manufactured low-gradient interfacial heterostructured medium-entropy alloy multilayers with superior strength and ductility synergy
21. Formation of two distinct cellular structures in 316L stainless steel fabricated by micro-laser beam powder-bed-fusion10.1080/21663831.2023.2292076 ↗
22. Strong yet ductile refractory high entropy alloy fabricated via additive manufacturing
23. Cracking mechanism of brittle FeCoNiCrAl HEA coating using extreme high-speed laser cladding10.1016/j.surfcoat.2021.127617 ↗
24. Effects of laser power on microstructure and properties of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coatings10.1016/j.surfcoat.2018.10.086 ↗
25. High-temperature oxidation performance of laser-cladded amorphous TiNiSiCrCoAl high-entropy alloy coating on Ti-6Al-4V surface10.1016/j.surfcoat.2022.128123 ↗
26. Microstructure and high-temperature wear mechanism of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coating10.1016/j.matlet.2017.09.056 ↗
27. Annular laser cladding of CuPb10Sn10 copper alloy for high-quality anti-friction coating on 42CrMo steel surface10.1016/j.optlastec.2022.108878 ↗
28. Control of grain structure, phases, and defects in additive manufacturing of high-performance metallic components10.1016/j.pmatsci.2023.101153 ↗
29. Additive manufacturing of fine-grained high-strength titanium alloy via multi-eutectoid elements alloying
30. Alloys-by-design: a low-modulus titanium alloy for additively manufactured biomedical implants10.1016/j.actamat.2022.117749 ↗
31. Heat treatment effects on the hydrogen embrittlement of Ti6Al4V fabricated by laser beam powder bed fusion
32. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
33. Long-term corrosion behavior of HVOF sprayed Cr3C2–NiCr coatings in sulfide-containing 3.5 wt.% NaCl solution10.1016/j.jmrt.2021.09.131 ↗
34. Relation between quenching wheel speed and microstructure, thermal stability and corrosion resistance of quinary Al-Ni-Y-Co-Si high entropy metallic glass ribbons prepared by melt spinning10.1016/j.jnoncrysol.2022.122049 ↗
35. Corrosion of Al CoCrFeNi high-entropy alloys: Al-content and potential scan-rate dependent pitting behavior10.1016/j.corsci.2017.02.019 ↗
36. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
37. Influence of microstructure and alloying elements on corrosion behavior of Ti–13Nb–13Zr alloy10.1016/S0010-938X(03)00186-0 ↗
38. Corrosion behavior of Al-containing CoNiV alloys
39. Fe-based metallic glass composite coatings by HVOF spraying: influence of Mo on phase evolution, wear and corrosion resistance10.1016/j.matchar.2022.112149 ↗
40. Microstructures and properties of FeCrAlMoSi high entropy alloy coatings prepared by laser cladding on a titanium alloy substrate10.1016/j.surfcoat.2024.130437 ↗
41. Frictional behaviour of plastics impregnated with molybdenum disulphide
42. Friction, lubrication and wear: a survey of work during the last decade10.1088/0508-3443/17/12/301 ↗