Influence of natural aging and ramping before artificial aging on the microstructure of two different 6xxx alloys
Source abstract
Abstract
In this study the effect of a ramp up to artificial aging (AA) temperature in combination with natural aging (NA) was analyzed for two different industrial aluminium alloys. The alloys differ in their Mg/Si ratio as well as their copper (Cu) content. Both alloys have, however, a comparable amount of solute and dispersoid forming elements. The peak aged conditions of the alloys were investigated. NA prior to AA reduces the strength as compared with directly aged regardless of ramping. The hardness up to peak is very similar for conditions with and without the ramp if NA is performed, but for the Cu rich alloy a clear increase in peak hardness could be measured when ramped from the supersaturated solid solution (SSSS). The peak strength plateau is shorter for the ramped samples regardless of the NA time. Investigations by (scanning) transmission electron microscopy found longer but fewer precipitates when ramped from the SSSS and an increased precipitate number density when ramped after NA. Fewer hybrid-type precipitates and less overaged precipitates, e.g. B’, and more L/C could be found for all ramped conditions. Atom probe tomography measurements showed that more solute is left in the matrix between the precipitates when ramped directly from the SSSS. This was related to a lower precipitate number density.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Schatzberg · 2015 · 226
2. Precipitation hardening10.4262/denkiseiko.37.65 ↗
3. Roesler · 2007
4. P. Dumitraschkewitz, S. S. Gerstl, L. T. Stephenson, P. J. Uggowitzer, S. Pogatscher, Clustering in age-hardenable aluminum alloys, Adv Eng Mater 20 (10). doi:10.1002/adem.201800255..10.1002/adem.201800255 ↗
5. Saito · 2018
6. R. Holmestad, C. D. Marioara, F. J. H. Ehlers, M. Torsaeter, R. Bjørge, J. Røyset, S. J. Andersen, Precipitation in 6xxx aluminum alloys.
7. The effect of Cu on precipitation in Al-Mg-Si alloys10.1080/14786430701287377 ↗
8. The influence of composition on the clustering and precipitation behavior of Al-Mg-Si-Cu alloys10.1007/s11661-016-3850-7 ↗
9. The effect of low Cu additions on precipitate crystal structures in overaged Al-Mg-Si(-Cu) alloys
10. B. Milkereit, M. J. Starink, P. A. Rometsch, C. Schick, O. Kessler, Review of the quench sensitivity of aluminium alloys: analysis of the kinetics and nature of quench-induced precipitation, Materials 12 (24). doi:10.3390/MA12244083..10.3390/ma12244083 ↗
11. Hardening of Al-Mg-Si alloys: effect of trace elements and prolonged natural aging10.1016/j.matdes.2016.06.014 ↗
12. Natural aging in Al-Mg-Si alloys - a process of unexpected complexity10.1002/adem.201000041 ↗
13. An extended age-hardening model for Al-Mg-Si alloys incorporating the room-temperature storage and cold deformation process stages10.1007/s11661-015-3175-y ↗
14. Quantification of the Mg2Si β” and β’ phases in AlMgSi alloys by transmission electron microscopy10.1007/BF02670664 ↗
15. The determination of foil thickness by scanning transmission electron microscopy10.1002/pssa.2210310251 ↗
16. D. J. Larson, T. Prosa, R. M. Ulfig, B. P. Geiser, T. F. Kelly, Local electrode atom probe tomography, New York, US: Springer Science 2..
17. Experimental artefacts occurring during atom probe tomography analysis of oxide nanoparticles in metallic matrix: quantification and correction10.1016/j.jnucmat.2017.05.008 ↗
18. 3d atom probe study of solute atoms clustering during natural ageing and pre-ageing of an al-mg-si alloy10.1080/09500830600643270 ↗
19. A study on the early-stage decomposition in the al–mg–si–cu alloy aa6111 by electrical resistivity and three-dimensional atom probe10.1080/14786430701408312 ↗
20. Copper enrichment on aluminium surfaces after electropolishing and its effect on electron imaging and diffraction10.1016/j.matchar.2020.110846 ↗
21. Analysis conditions of an industrial al–mg–si alloy by conventional and 3d atom probes10.1016/S0304-3991(01)00098-5 ↗
22. Effect of composition on clustering reactions in AlMgSi(Cu) alloys10.1016/j.scriptamat.2003.08.030 ↗
23. L. Ding, Z. Jia, Z. Zhang, R. E. Sanders, Q. Liu, G. Yang, The natural aging and precipitation hardening behaviour of Al-Mg-Si-Cu alloys with different Mg/Si ratios and Cu additions, Mater Sci Eng 627 (2015) 119–126. doi:10.1016/j.msea.2014.12.086. URL https://doi.org/10.1016/j.msea.2014.12.086.10.1016/j.msea.2014.12.086 ↗
24. M. Torsæter, H. S. Hasting, W. Lefebvre, C. D. Marioara, J. C. Walmsley, S. J. Andersen, R. Holmestad, The influence of composition and natural aging on clustering during preaging in Al-Mg-Si alloys, J Appl Phys 108 (7). doi:10.1063/1.3481090..10.1063/1.3481090 ↗
25. The precipitation sequence in Al-Mg-Si alloys10.1016/S1359-6454(98)00059-7 ↗
26. Solute-vacancy clustering in aluminum10.1016/j.actamat.2020.06.062 ↗
27. Effect of natural ageing or pre-ageing on the evolution of precipitate structure and strength during age hardening of Al–Mg–Si alloy AA 601610.1016/j.msea.2019.05.073 ↗
28. Mechanisms controlling the artificial aging of Al-Mg-Si Alloys10.1016/j.actamat.2011.02.010 ↗
29. The role of vacancies in the aging of Al-Mg-Si alloys10.4028/www.scientific.net/MSF.794-796.1008 ↗
30. The influence of Mg/Si ratio on the negative natural aging effect in Al-Mg-Si-Cu alloys10.1016/j.msea.2015.06.090 ↗
31. The effect of chemical patterning induced by cyclic plasticity on the formation of precipitates during aging of an Al–Mg–Si alloy
32. Study of precipitation in Al-Mg-Si Alloys by atom probe tomography II. Influence of Cu additions10.1016/j.actamat.2015.08.018 ↗
33. Atomic model for GP-zones in a 6082 Al-Mg-Si system10.1016/S1359-6454(00)00302-5 ↗
34. Modeling electrical resistivity of naturally aged al–mg–si alloys10.3390/met9030310 ↗
35. The effect of precipitate shape and orientation on dispersion strengthening in high strength aluminium alloys10.4028/www.scientific.net/MSF.217-222.1257 ↗
36. Cross-Slip on (100) planes in aluminum single crystals compressed along (100) axis10.1016/0001-6160(75)90203-5 ↗
37. Strength contributions from precipitates10.1080/09500839.2015.1125029 ↗
38. An age-hardening model for al-mg-si alloys considering needle-shaped precipitates10.1007/s11661-012-1211-8 ↗
39. Hardening of Al-Mg-Si alloys and effect of particle structure10.4028/www.scientific.net/MSF.706-709.283 ↗
40. Linking mechanical properties to precipitate microstructure in three Al-Mg-Si(-Cu) alloys
41. Microstructural design of high-strength aluminum alloys10.1361/105497198770341734 ↗
42. H. Mao, Y. Kong, D. Cai, M. Yang, Y. Peng, Y. Zeng, G. Zhang, X. Shuai, Q. Huang, K. Li, H. Zapolsky, Y. Du, β” needle-shape precipitate formation in Al-Mg-Si alloy: phase field simulation and experimental verification, Comput Mater Sci 184 (June). doi:10.1016/j.commatsci.2020.109878.10.1016/j.commatsci.2020.109878 ↗
43. Porter · 2009