Experimental study of high-temperature resistance of alkali-activated slag crushed aggregate mortar
Source abstract
Abstract
Rational utilization of blast furnace slag improves resource utilization rate and is a measure to ameliorate environmental degradation and climate crisis. Alkali-activated slag cementitious material (AASCM) has high temperature resistance and can provide material choice for high temperature environment construction and building fire resistance. In order to solve the thermal incompatibility problem between aggregate and paste of AASCM mortar with natural aggregate, a special type of mortar with alkali-activated slag as cementitious material was examined, which aggregates consisted of crushed and sieved particles of alkali-activated slag paste. The compressive strengths of 126 cubic and 126 prismatic specimens during and after high-temperature treatment were investigated. The test results showed that both the compressive and flexural strengths of the mortar during and after high-temperature treatment decreased with increasing temperature. Moreover, the compressive strength of the mortar after high-temperature treatment was higher than that during the treatment in which strength grade and temperature were constant. The formulated equations for calculating the compressive and flexural strengths during and after high-temperature treatment provided a basis for evaluating the fire resistance of this new type of masonry material. The microstructure and composition of the mortar were analyzed using scanning electron microscopy with energy-dispersive spectrometry and X-ray diffraction. At 600 °C, the mortar gradually produced new products akermanite, merwinite and gehlenite.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Fire effects on concrete materials · Concrete Properties and Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Report: damage analysis for a fire exposed industrial building10.2749/101686603777964469 ↗
2. Environmental contamination following the Grenfell Tower fire10.1016/j.chemosphere.2019.03.153 ↗
3. Lissade · 2022
4. The effect of temperature on the compressive strength of concrete10.1680/macr.1956.8.23.85 ↗
5. Evolution of mechanical properties of concrete with temperature and humidity at high temperatures
6. Residual compressive strength of high-strength concrete exposed to elevated temperatures
7. Effect of transient high temperature on high-strength concrete
8. Effects of elevated temperatures on properties of concrete10.1016/j.firesaf.2007.01.003 ↗
9. There is no Plan B for dealing with the climate crisis10.1080/00963402.2019.1654255 ↗
10. 2020
11. A review of waste heat recovery technologies towards molten slag in steel industry
12. Effectiveness of alkali-activated slag cementitious material as adhesive for structural reinforcement
13. Wardhono A, Law DW, Strano A. The strength of alkali-activated slag/fly ash mortar blends at ambient temperature. The 5th International Conference of Euro Asia Civil Engineering Forum (EACEF-5) https://doi.org/10.1016/j.proeng.2015.11.095.10.1016/j.proeng.2015.11.095 ↗
14. Strength and drying shrinkage of alkali-activated slag paste and mortar
15. Jiao · 2019
16. Resistance of alkali-activated slag mortar to abrasion and fire10.1680/adcr.2011.23.6.289 ↗
17. Influence of activator Na₂O concentration on residual strengths of alkali-activated slag mortar upon exposure to elevated temperatures10.3390/ma11081296 ↗
18. The influence of curing conditions and alkaline activator concentration on elevated temperature behavior of alkali activated slag (AAS) mortars10.1016/j.conbuildmat.2018.09.099 ↗
19. Zhu · 2014
20. Strength and drying shrinkage of reactive MgO modified alkali-activated slag paste10.1016/j.conbuildmat.2013.10.081 ↗
21. Shrinkage characteristics of alkali-activated slag cements10.1061/(ASCE)MT.1943-5533.0001058 ↗
22. Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar10.1016/j.conbuildmat.2007.10.011 ↗
23. Chemical shrinkage of cement pastes and mortars at very early age: effect of limestone filler and granular inclusions10.1016/j.cemconcomp.2007.06.004 ↗
24. Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages10.1016/j.cemconcomp.2014.07.007 ↗
25. Understanding the drying shrinkage performance of alkali-activated slag mortars10.1016/j.cemconcomp.2016.11.010 ↗
26. Concrete strength for fire safety design10.1680/macr.2005.57.8.445 ↗
27. Effects of elevated temperatures on properties of concrete10.1016/j.firesaf.2007.01.003 ↗
28. Effect of coarse aggregate type and loading level on the high temperature properties of concrete10.1016/j.conbuildmat.2014.12.096 ↗
29. Fly-ash based geopolymer mortar for high-temperature application–Effect of slag addition10.1016/j.jclepro.2021.128168 ↗
30. The effect of elevated temperature on the residual tensile strength and physical properties of the alkali-activated slag concrete10.1016/j.jobe.2018.08.015 ↗
31. Residual compressive behavior of alkali-activated concrete exposed to elevated temperatures10.1002/fam.983 ↗
32. Effect of elevated temperatures on geopolymer paste, mortar and concrete10.1016/j.cemconres.2009.10.017 ↗
33. Thermal and mechanical properties of alkali-activated slag paste, mortar and concrete utilising seawater and sea sand10.1016/j.conbuildmat.2017.10.104 ↗
34. An investigation on blast-furnace stag as fine aggregate in alkali-activated slag mortars subjected to elevated temperatures10.1016/j.jclepro.2015.07.127 ↗
35. Examination of mechanical properties and microstructure of alkali activated slag and slag-metakaolin blends exposed to high temperatures10.1002/suco.202000080 ↗
36. Li · 2017
37. 2008
38. Use of industrial waste slag in alkali-activated slag ceramsite concrete hollow blocks10.3390/app8122358 ↗
39. Pottery sand as fine aggregate for preparing alkali-activated slag mortar
40. Effect of the activator on the performance of alkali-activated slag mortars with pottery sand as fine aggregate10.1016/j.conbuildmat.2018.11.178 ↗
41. JGJ/T70 · 2009
42. GB/T17671 · 2020
43. Strength and drying shrinkage of reactive MgO modified alkali-activated slag paste10.1016/j.conbuildmat.2013.10.081 ↗
44. Strength and hydration properties of reactive MgO-activated ground granulated blastfurnace slag paste10.1016/j.cemconcomp.2014.10.007 ↗
45. High temperature and residual properties of reactive powder concrete – a review
46. Mechanical properties of steel fiber-reinforced reactive powder concrete at high temperature and after cooling10.1016/j.proeng.2017.11.119 ↗
47. Properties and microstructure of alkali-activated slag cement cured at below- and about-normal temperature10.1016/j.conbuildmat.2014.12.068 ↗
48. Development of greener alkali-activated cement: utilisation of sodium carbonate for activating slag and fly ash mixtures10.1016/j.jclepro.2015.12.010 ↗
49. Chemical acceleration of a neutral granulated blast-furnace slag activated by sodium carbonate10.1016/j.cemconres.2015.02.014 ↗
50. Use of glass waste as an activator in the preparation of alkali-activated slag. Mechanical strength and paste characterisation[J]10.1016/j.cemconres.2013.12.005 ↗
51. Chemical and mechanical stability of sodium sulfate activated slag after exposure to elevated temperature10.1016/j.cemconres.2011.10.007 ↗
52. Similarities and differences of microstructure and macro properties between Portland and blended cement10.1016/S0008-8846(97)00169-5 ↗
53. Properties of alkali activated aluminosilicate material after thermal load10.1007/s10765-006-0077-7 ↗
54. Fu · 2014