A novel method enhanced mechanical properties of a selective laser melted Mar-M247 superalloy by progressive remelting
Source abstract
Abstract
A novel method has been proposed to avoid the cracks in the Mar-M247 alloy manufactured via selective laser melting (SLM) related to high cooling rate interacted with carbides and eutectics, i.e., progressive remelting used to design the temperature field reducing the thermal stresses in SLM process. The microstructure evolves from a partly fused state to a completely solid block during progressive remelting, and those cracks inhibit effectively. The temperature gradient is gradually reduced in the process of progressive remelting, and eventually 29% lower than that in original SLM process. Quantitative temperature-field analysis signifies a substantial decrease in the cooling rate during manufacturing via progressive remelting, which explains crack inhibition. Compared to the original SLM-built Mar-M247, progressive remelting leads to a 35.1% increase in ultimate tensile strength (UTS) at RT. The UTS and elongation of progressive remelted Mar-M247 exhibit 747.2 MPa and 6.1% at 900 °C, respectively, superior to that of materials fabricated by casting and heat-treatment. This work helps further comprehend the relationship of volumetric energy density - thermal gradient - cooling rate - microstructure - mechanical properties, especially utilizing accumulative input energy to control temperature field, and offers a new opportunity to non-weldable superalloys fabricated in commercially available SLM systems.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. The effect of homogenization temperature on the microstructure and high temperature mechanical performance of SLM-fabricated IN718 alloy10.1016/j.msea.2020.140427 ↗
3. An effective and efficient model for temperature and molding appearance analyses for selective laser melting process10.1016/j.jmatprotec.2021.117109 ↗
4. Cracking mechanism of Hastelloy X superalloy during directed energy deposition additive manufacturing
5. Reduction of micro-cracking in nickel superalloys processed by Selective Laser Melting: a fundamental alloy design approach10.1016/j.actamat.2015.04.035 ↗
6. Microstructure and mechanical properties of rene 41 alloy manufactured by laser powder bed fusion10.1016/j.msea.2019.138849 ↗
7. Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy10.1016/j.actamat.2017.02.007 ↗
8. Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment10.1016/j.matchar.2016.02.004 ↗
9. Cracking inhibition behavior and the strengthening effect of TiC particles on the CM247LC superalloy prepared by selective laser melting10.1016/j.msea.2022.144119 ↗
10. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy10.1016/j.jallcom.2014.06.172 ↗
11. Scanning strategy induced cracking and anisotropic weakening in grain texture of additively manufactured superalloys
12. Microstructure and mechanical properties of crack-free Inconel 738 fabricated by laser powder bed fusion10.1016/j.msea.2022.143524 ↗
13. Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion
14. Donachie · Superalloys: A Technical Guide · 2002 · 2 · 18
15. Additive manufacturing of nickel-base superalloy rené N5 through scanning laser epitaxy (SLE) − material processing, microstructures, and microhardness properties10.1002/adem.201600690 ↗
16. Microstructure of nickel-base superalloy MAR-M247 additively manufactured through scanning laser epitaxy (SLE)10.1016/j.jallcom.2017.02.013 ↗
17. Allen · 1986
18. Directionally Solidified DS CM 247 LC—Optimized Mechanical Properties Resulting From Extensive γ′ Solutioning
19. The effect of boron and zirconium on the microcracking susceptibility of IN-738LC derivatives in laser powder bed fusion10.1016/j.apsusc.2021.151541 ↗
20. Alloy design via additive manufacturing: advantages, challenges, applications and perspectives10.1016/j.mattod.2021.11.026 ↗
21. On the role of Zr and B addition on solidification cracking of IN738LC produced by laser powder bed fusion10.1016/j.mtla.2022.101609 ↗
22. Reducing cracking sensitivity of CM247LC processed via laser powder bed fusion through composition modification10.1016/j.jmrt.2024.02.082 ↗
23. Alloys-by-design: application to new superalloys for additive manufacturing10.1016/j.actamat.2020.09.023 ↗
24. Inhibition of cracking by grain boundary modification in a non-weldable nickel-based superalloy processed by laser powder bed fusion10.1016/j.msea.2020.139745 ↗
25. Combined effects of heat treatment and TiB2 content on the high-temperature tensile performance of TiB2-modified Ni-based GH3230 alloy processed by laser powder bed fusion10.1016/j.msea.2022.144379 ↗
26. Crack elimination and mechanical properties enhancement in additive manufactured Hastelloy X via in-situ chemical doping of Y2O310.1016/j.msea.2021.141867 ↗
27. Y2O3 nanoparticles decorated IN738LC superalloy manufactured by laser powder bed fusion: cracking inhibition, microstructures and mechanical properties10.1016/j.compositesb.2021.109555 ↗
28. Hagedorn · 2013 · 291
29. Cracking mechanisms and effect of extensive preheating in CM247LC and IN713LC Ni-base superalloy processed by Laser Powder Bed Fusion
30. Evolution of residual stress behavior in selective laser melting (SLM) of 316L stainless steel through preheating and in-situ re-scanning techniques10.1016/j.optlastec.2021.107806 ↗
31. Effect of powder bed preheating on the crack formation and microstructure in ceramic matrix composites fabricated by laser powder-bed fusion process
32. Crack inhibition and mechanical property enhancement of a CM247LC alloy fabricated by laser powder bed fusion through remelting strategy10.1016/j.matchar.2024.114073 ↗
33. Laser powder bed fusion of Hastelloy X: effects of hot isostatic pressing and the hot cracking mechanism10.1016/j.msea.2018.07.008 ↗
34. Healing cracks in selective laser melting by 3D laser shock peening
35. Effects of hot isostatic pressing treatment on the microstructure and tensile properties of Ni-based superalloy CM247LC manufactured by selective laser melting10.1016/j.msea.2022.143083 ↗
36. The limit of hot isostatic pressing for healing cracks present in an additively manufactured nickel superalloy10.1016/j.jmatprotec.2021.117398 ↗
37. Ultrahigh-strength titanium gyroid scaffolds manufactured by selective laser melting (SLM) for bone implant applications10.1016/j.actamat.2018.08.005 ↗
38. Elucidating the effects of solution and double ageing treatment on the mechanical properties and toughness of MAR-M247 superalloy at high temperature10.1016/j.matchemphys.2007.11.041 ↗
39. Effect of heat treatment on the microstructural evolution and mechanical property of nickel-based superalloy K447A manufactured by Powder Bed Fusion Laser Beam (PBF-LB)10.1016/j.msea.2024.146874 ↗
40. Engeli · 2017
41. L.N. Carter, M.M. Attallah, R.C. Reed, Laser powder bed fabrication of nickel-base superalloys: influence of parameters; characterisation, quantification and mitigation of cracking, Superalloys 20122012, pp. 577-586.10.7449/2012/Superalloys_2012_577_586 ↗
42. Melt pool temperature and cooling rates in laser powder bed fusion
43. Reduction of the hot cracking sensitivity of CM-247LC superalloy processed by laser cladding using induction preheating10.1016/j.jmatprotec.2019.116461 ↗
44. Temperature-dependent elastic properties of binary and multicomponent high-entropy refractory carbides10.1016/j.matdes.2021.109634 ↗
45. Assessment of stress characteristic and interfacial delamination in thermal barrier coatings considering the connected crack network10.1016/j.surfcoat.2021.128065 ↗
46. 2021 · 16
47. Influence of microstructure and its evolution on the mechanical behavior of modified MAR-M247 fine-grain superalloys at 871°C10.1016/j.msea.2012.01.059 ↗
48. Correlation between phase stability and tensile properties of the Ni-based superalloy MAR-m24710.1007/s40195-020-01139-4 ↗
49. Densification, microstructure, and mechanical properties of heat-treated MAR-M247 fabricated by Binder Jetting
50. Influence of heat treatment on microstructure and tensile properties of conventionally cast and directionally solidified superalloy CM247LC10.1016/j.matlet.2007.07.058 ↗
51. Anomalous deformation behavior and twin formation of Ni-base superalloys at the intermediate temperatures10.1016/j.msea.2011.05.083 ↗
52. Effect of the cooling rate on microstructure and hardness of MAR-M247 Ni-based superalloy10.1016/j.matlet.2012.01.028 ↗
53. Influence of molten-pool cooling rate on solidification structure and mechanical property of laser additive manufactured Inconel 71810.1016/j.jmrt.2022.06.162 ↗
54. Study of microsegregation and laves phase in INCONEL718 superalloy regarding cooling rate during solidification10.1007/s11661-014-2614-5 ↗
55. Relationship between cooling rate and SDAS in liquid phase separated metastable Cu–Co alloys10.1016/j.jallcom.2021.160823 ↗
56. Localized melt-scan strategy for site specific control of grain size and primary dendrite arm spacing in electron beam additive manufacturing10.1016/j.actamat.2017.08.038 ↗
57. Melt pool evolution and microstructure simulation of SLM 316L based on SPH-PFM coupling model10.1016/j.jmrt.2023.12.206 ↗
58. A comparative study of the γ/γ′ eutectic evolution during the solidification of Ni-base superalloys10.1007/s11661-011-0738-4 ↗
59. Exploring How LPBF process parameters impact the interface characteristics of LPBF Inconel 718 deposited on Inconel 718 wrought substrates10.1016/j.optlastec.2024.110571 ↗
60. Microstructure characteristics of inconel 625 superalloy manufactured by selective laser melting10.1016/j.jmst.2014.09.020 ↗
61. Microstructure evolution of Inconel 738 fabricated by pulsed laser powder bed fusion10.1007/s40964-018-0062-2 ↗
62. Effect of weld cooling rate on Laves phase formation in Inconel 718 fusion zone10.1016/j.jmatprotec.2013.09.006 ↗
63. Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment10.1016/j.msea.2017.02.062 ↗