Abstract

The effect of γ/γ′ phase lattice misfit on hydrogen embrittlement (HE) behavior was fundamentally investigated by utilizing a Ni-based single crystal CMSX-4 superalloy with a simple microstructure that can exclude the H-trapping effects of grain boundary, c-vacancy, and misfit dislocation. Increasing isothermal aging time increased γ′ precipitate size while maintaining its volume fraction and a fully coherent interface. The magnitude of negative lattice misfit between the γ and γ′ phases increased from −0.08 to −0.22% according to γ′ precipitate coarsening, resulting in a well-developed tensile-strain field within the γ′ precipitate. The increased tensile-strain field enhanced activation energy for H-desorption in the γ′ precipitate from 31.9 to 35.1 kJ/mol. Therefore, H is preferentially distributed along the γ/γ′ interface within the γ′ precipitate even before deformation. H basically promotes the slip planarity through the H-enhanced localized plasticity (HELP) mechanism in Ni-based single crystal alloys, in which slip is the dominant deformation behavior. As the superalloy possesses a larger negative lattice misfit, H becomes trapped as diffusible-state at the tensile-strain field of the γ/γ′ interface, resulting in cuboidal brittle fracture along the {001} planes. In this process, the HELP mechanism facilitated H localization at the γ/γ′ interface. Thus, the HE behavior distinctly transitioned from HELP to an interaction between HELP and H-enhanced decohesion mechanisms (HEDE) with an increase in the magnitude of the lattice misfit. The HE behavior was investigated by correlating microstructural characterization, H-trapping behavior, and crystallographic fracture mechanism analysis.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Hydrogen embrittlement understood10.1007/s11663-015-0325-y ↗
2. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
3. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗
4. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
5. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
6. Trap theory of hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
7. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
8. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
9. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
10. Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel10.1016/j.actamat.2021.116635 ↗
11. The effect of nanosized (Ti,Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel10.1016/j.actamat.2014.04.051 ↗
12. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
13. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
14. Effect of dislocation cell walls on hydrogen adsorption, hydrogen trapping and hydrogen embrittlement resistance10.1016/j.corsci.2020.108428 ↗
15. The predominant role of strain-induced vacancies in hydrogen embrittlement of steels: overview10.1016/j.actamat.2018.12.013 ↗
16. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
17. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
18. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
19. The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
20. Optimizing the hydrogen embrittlement resistance by tuning the structures of Cu-rich nanoprecipitates in high strength martensite stainless steels10.1016/j.actamat.2023.118722 ↗
21. Environmental embrittlement of boron-doped Ni3(Al, Ti) single crystals at room temperature10.1557/JMR.1993.2534 ↗
22. Hydrogen trapping behavior in vanadium-added steel10.2355/isijinternational.43.527 ↗
23. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
24. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel10.1016/j.actamat.2018.05.003 ↗
25. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
26. First-principles investigation of hydrogen interaction with TiC precipitates in α-Fe
27. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
28. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe-Mn-Al-C light weight austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
29. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography10.1016/j.scriptamat.2010.03.012 ↗
30. Density functional theory calculations of iron–vanadium carbide interfaces and the effect of hydrogen10.1016/j.ijhydene.2019.11.102 ↗
31. Numerical analysis of hydrogen trap state by TiC and V4C3 in bcc-Fe10.2355/isijinternational.52.1693 ↗
32. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
33. The effect of hydrogen on the deformation of pearlite in steels
34. Reed · 2006
35. Effect of lattice misfit on the evolution of the dislocation structure in Ni-based single crystal superalloys during thermal exposure10.1016/j.actamat.2016.08.035 ↗
36. Effect of γ′ precipitate size on hardness and creep properties of Ni-base single crystal superalloys: experiment and simulation10.1016/j.mtla.2020.100692 ↗
37. Numerical modelling of creep deformation in a CMSX-4 single crystal superalloy turbine blade
38. The importance of sign and magnitude of γ/γ′ lattice misfit in superalloys—with special reference to the new γ′-hardened cobalt-base superalloys10.1016/j.actamat.2014.08.005 ↗
39. First-principles study of the influence of lattice misfit on the segregation behaviors of hydrogen and boron in the Ni–Ni3Al system10.1016/j.actamat.2007.05.006 ↗
40. First-principles understanding of environmental embrittlement of the Ni/Ni3Al interface10.1016/j.scriptamat.2010.04.033 ↗
41. Hydrogen-enhanced decohesion mechanism of the Ni-Ni3X interfaces in precipitation-hardened Ni-based alloys10.1016/j.jallcom.2023.171186 ↗
42. Hydrogen-enhanced interfacial damage in Ni-based single crystal superalloy10.1016/j.scriptamat.2017.07.023 ↗
43. Hydrogen effects in [001] oriented nickel-base superalloy single crystals10.1007/BF02669816 ↗
44. Solution heat treatment of the single crystal nickel-base superalloy CMSX-4 fabricated by selective electron beam melting10.1002/adem.201500037 ↗
45. Effect of heat treatment on chemical segregation in CMSX-4 nickel-base superalloy10.1007/s11665-013-0843-1 ↗
46. [100] Directional alignment of Ni-based single- crystal superalloys to measure orientation and accurate misfit between γ and γ’ phases via high-resolution X-ray diffraction10.1016/j.jallcom.2019.153521 ↗
47. The effect of Si on hydrogen embrittlement of Fe-18Mn-0.6C-xSi twinning-induced plasticity steels10.1016/j.actamat.2015.10.015 ↗
48. Effects of Cu addition on resistance to hydrogen embrittlement in 1 GPa-grade duplex lightweight steels10.1016/j.actamat.2020.06.051 ↗
49. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
50. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
51. Coarsening kinetics of cuboidal γ' precipitates in single crystal nickel base superalloy CMSX-4
52. The effect of microstructure on mechanical properties of single crystal CMSX-4 superalloy
53. Lattice misfit measurement in Inconel 706 containing coherent γ′ and γ″ precipitates10.1016/S1359-6462(02)00456-6 ↗
54. Measurement of the unconstrained misfit in the nickel-base superalloy CMSX-4 with CBED10.1016/S1359-6462(97)00559-9 ↗
55. Tensile deformation behavior of a new Ni-base superalloy at room temperature10.1016/j.msea.2015.12.089 ↗
56. Deformation behavior in cold-rolled medium-manganese TRIP steel and effect of pre-strain on the Lüders bands10.1016/j.msea.2016.10.042 ↗
57. Deformation and fracture of the PWA 1472 superalloy single crystal10.1016/S1359-6454(99)00355-9 ↗
58. Rate dependent ductility and damage threshold: application to Nickel-based single crystal CMSX-410.1016/j.ijplas.2018.09.006 ↗
59. Tensile properties, strain rate sensitivity and failure mechanism of single crystal superalloys CMSX-410.1016/j.msea.2020.139105 ↗
60. Processing, microstructures and mechanical properties of a Ni-based single crystal superalloy10.3390/cryst10070572 ↗
61. Hydrogen permeation and diffusion in Inconel 718 and incoloy 90310.1007/BF02646873 ↗
62. Hydrogen transport in solution-treated and pre-strained austenitic stainless steels and its role in hydrogen-enhanced fatigue crack growth10.1016/j.ijhydene.2008.11.018 ↗
63. Atomic scale structure and chemical composition across order-disorder interfaces10.1103/PhysRevLett.102.086101 ↗
64. Effects of lattice misfit on plastic deformation behavior of single-crystalline micropillars of Ni-based superalloys10.1016/j.actamat.2017.07.044 ↗
65. Porter · 2009
66. The diffusion and trapping of hydrogen in steel10.1016/0001-6160(70)90078-7 ↗
67. A new analysis of the diffusion of hydrogen in iron and ferritic steels
68. Marin · 2012
69. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
70. Multi-scale and spatially resolved hydrogen mapping in a Ni–Nb model alloy reveals the role of the δ phase in hydrogen embrittlement of alloy 71810.1016/j.actamat.2016.02.053 ↗
71. Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
72. The trapping and transport phenomena of hydrogen in nickel10.1007/BF02643893 ↗
73. Diffusion of hydrogen in metals
74. The Portevin-Le Chatelier effect in hydrogenated nickel10.1007/BF02819254 ↗
75. Hydrogen diffusion and its relevance to intergranular cracking in nickel10.1007/BF02669608 ↗
76. Hydrogen permeation, diffusion and solution in nickel
77. Hydrogen transport in nickel-base alloys10.1007/BF02663432 ↗
78. First-principle modeling of hydrogen site solubility and diffusion in disordered Ti–V–Cr alloys10.1016/j.ijhydene.2018.07.128 ↗
79. The influence of hydrostatic stress states on the hydrogen solubility in martensitic steels10.1016/j.scriptamat.2014.04.006 ↗
80. Effect of heat-treatment on microstructure and high-temperature deformation behavior of a low rhenium-containing single crystal nickel-based superalloy10.1016/j.msea.2014.03.093 ↗
81. On the creep behavior at 1033 K of new generation single-crystal superalloys10.1016/S0921-5093(04)00925-6 ↗
82. Strengthening of Nimonic alloy PE 16 by ordered particles of Ni3(Al, Ti)10.1016/0001-6160(75)90178-9 ↗
83. Observation of local hydrogen on nickel surfaces10.1007/BF02663321 ↗
84. Embrittlement of interfaces by solute segregation10.1016/0921-5093(89)90372-9 ↗
85. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
86. Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe-Mn-Al-C light weight Austenitic steel10.1016/j.ijhydene.2013.12.171 ↗
87. Microstructure and mechanical properties of nickel-based superalloy fabricated by laser powder-bed fusion using recycled powders10.1007/s12613-020-2147-4 ↗
88. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture
89. Hydrogen induced shear localization of the plastic flow in metals and alloys10.1016/S0997-7538(01)01179-2 ↗
90. Hydrogen-enhanced local plasticity at dilute bulk H concentrations: the role of H–H interactions and the formation of local hydrides10.1016/j.actamat.2011.01.037 ↗
91. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
92. Hydrogen embrittlement and failure mechanisms of multi-principal element alloys: a review10.1016/j.jmst.2022.01.008 ↗
93. Influences of Re on low-cycle fatigue behaviors of single crystal superalloys at intermediate temperature10.1016/j.jmst.2019.05.026 ↗
94. The mechanisms and temperature dependence of superlattice stacking fault formation in the single-crystal superalloy PWA 148010.1007/BF02664997 ↗
95. Microstructural stability and tensile properties of a Ti-containing single-crystal Co–Ni–Al–W-base alloy10.1016/j.msea.2015.08.044 ↗
96. Hydrogen-affected cross-slip process in fcc nickel10.1103/PhysRevB.69.174108 ↗
97. State of 3-D micro-damage in hydrogen redistributed regions of precharged high strength aluminium alloy10.1016/j.corsci.2016.04.050 ↗
98. Investigation of hydrogen embrittlement properties of Ni-based alloy 718 fabricated via laser powder bed fusion10.1016/j.ijhydene.2022.04.045 ↗
99. Effects of laser powder bed fusion process parameters on microstructure and hydrogen embrittlement of high-entropy alloy10.1016/j.jmst.2022.12.074 ↗
100. The effect of lattice misfit on the dislocation motion in superalloys during high-temperature low-stress creep10.1016/j.actamat.2005.06.013 ↗