journal article·2024-11Open access

Crack inhibition and crystallographic texture control in an additively manufactured IN738LC Ni-based superalloy

Fangxian Zhang, Liping Zhou, Xinliang Xie, Zhenbo Zhang, Qi Chao, Guohua Fan

Abstract

The additive manufacturing of directionally solidified Ni-based superalloys remains a significant challenge due to the formation of stray equiaxed grains and their high susceptibility to cracking, particularly for high-volume γ´-type Ni-based superalloys. In this study, a novel strategy based on temperature field management was proposed to prevent hot cracking and control crystallographic texture during laser powder bed fusion (LPBF) of IN738LC superalloy. The influence of laser parameters and substrate preheating on crack density, melt pool morphology, and texture of IN738LC superalloy was investigated. The fluid dynamics and thermal behavior of melt pool was simulated using the discrete element model (DEM) and volume of fluid (VOF) method. The processing window for achieving defect-free IN738LC samples was established and was found to be highly affected by substrate preheating. Substrate preheating at 350 °C resulted in expanded processing window, with the volume energy density ranging from 42.9 to 62.5 J/mm³ without substrate preheating to 40–75 J/mm³. The enlarged processing window was achieved by reducing cracking susceptibility due to the reduced temperature gradient and cooling rate. A unique crystallographic lamellar microstructure (CLM), comprising a <110>-oriented major layer and <100>-oriented sub-layer along the building direction, was successfully achieved in the LPBF-processed IN738LC superalloy. The solidification conditions for obtaining such a CLM were discussed on the aspects of temperature gradient and solidification rate within the melt pool. This work provides new insights and methods for preparing crack-free γ´-Ni-based superalloys with specific textures, which is favorable for improving the high-temperature properties.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Micro-cracking, microstructure and mechanical properties of Hastelloy-X alloy printed by laser powder bed fusion: as-built, annealed and hot-isostatic pressed
2. On the strengthening and embrittlement mechanisms of an additively manufactured Nickel-base superalloy10.1016/j.mtla.2020.100657 ↗
3. High temperature material properties of IN738LC processed by selective laser melting (SLM) technology10.1108/13552541311323281 ↗
4. An investigation on the creep and fracture behavior of cast nickel-base superalloy IN738LC10.1007/BF02663308 ↗
5. Inhibition of cracking by grain boundary modification in a non-weldable nickel-based superalloy processed by laser powder bed fusion10.1016/j.msea.2020.139745 ↗
6. Microstructure-property gradients in Ni-based superalloy (Inconel 738) additively manufactured via electron beam powder bed fusion
7. Influence of minor alloying element additions on the crack susceptibility of a nickel based superalloy manufactured by LPBF10.3390/ma14195702 ↗
8. Role of alloy composition on micro-cracking mechanisms in additively manufactured Ni-based superalloys10.1016/j.actamat.2023.119089 ↗
9. Processability of different IN738LC powder batches by selective laser melting10.1016/j.jmatprotec.2015.09.046 ↗
10. Selective laser melting of the hard-to-weld IN738LC superalloy: efforts to mitigate defects and the resultant microstructural and mechanical properties10.1016/j.jallcom.2019.151662 ↗
11. Effect of carbon content on the microstructure, tensile properties and cracking susceptibility of IN738 superalloy processed by laser powder bed fusion
12. Y2O3 nanoparticles decorated IN738LC superalloy manufactured by laser powder bed fusion: cracking inhibition, microstructures and mechanical properties10.1016/j.compositesb.2021.109555 ↗
13. Reducing cracking sensitivity of CM247LC processed via laser powder bed fusion through composition modification10.1016/j.jmrt.2024.02.082 ↗
14. Investigation of cracking mechanism and yield strength associated with scanning strategy for an additively manufactured nickel-based superalloy10.1016/j.jallcom.2022.168532 ↗
15. Crack inhibition and mechanical property enhancement of a CM247LC alloy fabricated by laser powder bed fusion through remelting strategy10.1016/j.matchar.2024.114073 ↗
16. Investigating crack formation in IN738LC Ni-based superalloy fabricated by laser powder-bed fusion process10.1016/j.jmrt.2024.01.264 ↗
17. Cracking mechanism and control of Hastelloy X prepared by laser powder bed fusion10.1016/j.jmrt.2022.10.164 ↗
18. In-situ ultrasonic impact treatment (UIT) to improve the fatigue properties of laser powder bed fusion (LPBF) manufactured inconel 71810.1016/j.matchemphys.2024.129595 ↗
19. Progressive developments, challenges and future trends in laser shock peening of metallic materials and alloys: a comprehensive review10.1016/j.ijmachtools.2023.104061 ↗
20. Ultrasonic surface post-processing of hot isostatic pressed and heat treated superalloy parts manufactured by laser powder bed fusion
21. Influence of heat input on solidification cracking in additively manufactured CM247LC Ni-based superalloy10.1007/s11661-023-07027-7 ↗
22. Grain refinement and crack inhibition of hard-to-weld Inconel 738 alloy by altering the scanning strategy during selective laser melting10.1016/j.matdes.2021.109940 ↗
23. Scanning strategy induced cracking and anisotropic weakening in grain texture of additively manufactured superalloys
24. Mesoscopic evolution of molten pool during selective laser melting of superalloy Inconel 738 at elevating preheating temperature10.1016/j.matdes.2021.110355 ↗
25. Effect of high preheating on the microstructure and mechanical properties of high gamma prime Ni-based superalloy manufactured by laser powder bed fusion10.1016/j.jallcom.2023.170598 ↗
26. Unique crystallographic texture formation in Inconel 718 by laser powder bed fusion and its effect on mechanical anisotropy10.1016/j.actamat.2021.116876 ↗
27. Avoiding cracks in additively manufactured non-weldable directionally solidified Ni-based superalloys
28. Additive manufacturing of nickel-based superalloy single crystals with IN-738 alloy
29. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
30. ImageJ user guide
31. Numerical simulation of melt pool size and flow evolution for laser powder bed fusion of powder grade Ti6Al4V10.1016/j.finel.2023.103971 ↗
32. Denudation of metal powder layers in laser powder bed fusion processes10.1016/j.actamat.2016.05.017 ↗
33. Forming and defect analysis for single track scanning in selective laser melting of Ti6Al4V10.1007/s00339-018-2056-9 ↗
34. Numerical modeling of inconel 738LC deposition welding: prediction of residual stress induced cracking10.1016/j.jmatprotec.2010.07.027 ↗
35. Kerrouault · 2000
36. Chapman · 2008
37. Thermophysical properties of IN738LC, MM247LC and CMSX-4 in the liquid and high temperature solid phase
38. Identifying the keyhole stability and pore formation mechanisms in laser powder bed fusion additive manufacturing10.1016/j.jmatprotec.2023.118153 ↗
39. Columnar to equiaxed transition in solidification processing10.1016/S1468-6996(01)00047-X ↗
40. Epitaxial laser metal forming: analysis of microstructure formation10.1016/S0921-5093(99)00202-6 ↗
41. The role of side-branching in microstructure development in laser powder-bed fusion10.1038/s41467-020-14453-3 ↗
42. Welding metallurgy
43. Understanding the process-microstructure correlations for tailoring the mechanical properties of L-PBF produced austenitic advanced high strength steel
44. Temporal evolution of temperature gradient and solidification rate in laser powder bed fusion additive manufacturing10.1007/s00231-022-03318-8 ↗
45. The printability, microstructure, crystallographic features and microhardness of selective laser melted Inconel 718 thin wall10.1016/j.matdes.2018.07.007 ↗
46. Real-time monitoring of laser powder bed fusion process using high-speed X-ray imaging and diffraction10.1038/s41598-017-03761-2 ↗
47. Excellent mechanical and corrosion properties of austenitic stainless steel with a unique crystallographic lamellar microstructure via selective laser melting10.1016/j.scriptamat.2018.09.017 ↗
48. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
49. Last-stage solidification of alloys: theoretical model of dendrite-arm and grain coalescence10.1007/s11661-003-0083-3 ↗
50. Improved plasticity of Inconel 718 superalloy fabricated by selective laser melting through a novel heat treatment process10.1016/j.matdes.2019.107915 ↗
51. Dislocation models of crystal grain boundaries10.1103/PhysRev.78.275 ↗
52. Role of carbon in modifying solidification and microstructure of a Ni-based superalloy with high Al and Ti contents10.1007/s42243-020-00408-x ↗
53. On the solidification behaviour and cracking origin of a nickel-based superalloy during selective laser melting10.1016/j.matchar.2018.12.032 ↗
54. Controlling the microstructure of hastelloy-X components manufactured by selective laser melting10.1016/j.phpro.2013.03.154 ↗
55. Modelling the coefficient of thermal expansion in Ni-based superalloys and bond coatings10.1007/s10853-015-9554-3 ↗
56. Study of the influence of material properties on residual stress in selective laser melting