It is well known that lower quench rate leads to the formation of precipitate free zones (PFZs) adjacent to grain boundaries in aging hardening materials such as Al–Mg–Si alloys. However, the combined effect of PFZs and intragranular precipitates on the yield strength of Al–Mg–Si alloys is not systematically understood. To clarify this, an Al–Mg–Si alloy was water/oil/air quenched after solid solution treatment, then aged at 180 °C for 6 h. It was found that a lower quench rate led to coarser precipitates and wider PFZs. The effects of PFZs and precipitates on the yield strength of the Al–Mg–Si alloy were separated by quantitative characterization of multi-scale microstructures and mechanical simulations. Wide PFZs were found to have a notable effect on yield strength, amounting over half the strengthening effect of intragranular precipitates. This effect increases as the width of PFZ increases, due to more serious strain localization caused by PFZs. A corresponding equation has thus been proposed to describe the deleterious effects of PFZs on yield strength of Al–Mg–Si alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Lukacs · 2018 · 12031
2. Sivanur · 2021 · 20032
3. The evolution of orientation relationships during the transformation of a twin-free T-particle to tenfold T-twins in an Al alloy during homogenisation10.1016/j.matchar.2018.03.029 ↗
4. Quantified contribution of β″ and β′ precipitates to the strengthening of an aged Al-Mg-Si alloy10.1016/j.msea.2019.138776 ↗
5. Microstructures and strengthening mechanisms of high Fe containing Al-Mg-Si-Mn-Fe alloys with Mg, Si and Mn modified10.1016/j.msea.2020.140477 ↗
6. Linking mechanical properties to precipitate microstructure in three Al-Mg-Si (-Cu) alloys10.1016/j.msea.2021.140862 ↗
7. Thermodynamic, kinetic and strength calculation of high zinc containing Al-Zn-Mg-Cu alloys10.3390/cryst12020181 ↗
8. Thermodynamic and kinetic calculation of high strength aluminum-lithium alloy10.3390/cryst12040472 ↗
9. Kinetic and strength calculation of age-hardening phases in heat-resistant aluminum alloys with silver10.4028/www.scientific.net/MSF.993.1051 ↗
10. The precipitation sequence in Al-Mg-Si alloys10.1016/S1359-6454(98)00059-7 ↗
11. Atomic pillar-based nanoprecipitates strengthen AlMgSi alloys10.1126/science.1124199 ↗
12. Phase stability and structural relations of nanometer-sized, matrix-embedded precipitate phases in Al-Mg-Si alloys in the late stages of evolution10.1016/j.actamat.2006.02.034 ↗
13. Phase stability and structural features of matrix-embedded hardening precipitates in Al-Mg-Si alloys in the early stages of evolution10.1016/j.actamat.2006.11.019 ↗
14. A yield strength model for the Al-Mg-Si-Cu alloy AA611110.1016/S1359-6454(03)00028-4 ↗
15. Modelling of the microstructure and strength evolution in Al-Mg-Si alloys during multistage thermal processing10.1016/j.actamat.2004.07.002 ↗
16. Simultaneously enhanced strength and ductility of 6xxx Al alloys via manipulating meso-scale and nano-scale structures guided with phase equilibrium10.1016/j.jmst.2019.09.029 ↗
17. Effect of heating rate during solution treatment on the bendability of Al-Mg-Si alloys10.1016/j.msea.2020.139604 ↗
18. The Role of vacancies in the aging of Al-Mg-Si alloys10.4028/www.scientific.net/MSF.794-796.1008 ↗
19. Modeling of excess vacancy annihilation at different types of sinks10.1016/j.actamat.2011.02.020 ↗
20. Influence of quenching temperature on peak aging time and hardness of Al-Mg-Si-Cu alloys strengthened by nano-sized precipitates10.1016/j.msea.2018.11.149 ↗
21. Mechanisms controlling the artificial aging of Al-Mg-Si Alloys10.1016/j.actamat.2011.02.010 ↗
22. The effects of quench rate and pre-deformation on precipitation hardening in Al-Mg-Si alloys with different Cu amounts10.1016/j.msea.2014.04.094 ↗
23. Influence of quenching rate and aging on bendability of AA6016 sheet10.1016/j.msea.2018.05.108 ↗
24. The origin of the grain boundary precipitate free zone10.1016/0001-6160(69)90154-0 ↗
25. Lattice rotations in precipitate free zones in an Al-Mg-Si alloy10.1016/j.matchar.2018.08.002 ↗
26. On the effects of thermomechanical processing on failure mode in precipitation-hardened aluminium alloys10.1023/A:1021095801205 ↗
27. Quantification of grain boundary precipitation and the influence of quench rate in 6XXX aluminum alloys10.1016/j.matchar.2006.03.007 ↗
28. Quench sensitivity of toughness in an Al alloy: direct observation and analysis of failure initiation at the precipitate-free zone10.1016/j.actamat.2008.02.021 ↗
29. Effects of quench rate and natural ageing on the age hardening behaviour of aluminium alloy AA606010.1016/j.matchar.2015.11.009 ↗
30. Analysis of the metastable precipitates in peak-hardness aged Al-Mg-Si(-Cu) alloys with differing Si contents10.1016/j.actamat.2017.04.037 ↗
31. HRTEM study of the effect of deformation on the early precipitation behaviour in an AA6060 Al–Mg–Si alloy10.1080/14786435.2011.593577 ↗
32. The effect of preaging deformation on the precipitation behavior of an Al-Mg-Si alloy10.1007/s11661-012-1235-0 ↗
33. Quantified effect of sample size and gas environment on precipitation of an aged Al-Mg-Si alloy10.1016/j.matchar.2020.110829 ↗
34. The structural and compositional evolution of precipitates in Al-Mg-Si-Cu alloy10.1016/j.actamat.2017.12.036 ↗
35. The influence of alloy composition on precipitates of the Al-Mg-Si system10.1007/s11661-005-0185-1 ↗
36. Quantitative measurement for the microstructural parameters of nano-precipitates in Al-Mg-Si-Cu alloys10.1016/j.matchar.2016.06.007 ↗
37. Williams · 2009
38. Modelling of the age hardening behaviour of Al–Mg–Si alloys10.1016/S1359-6454(00)00301-3 ↗
39. Precipitation hardening10.1007/BF02670416 ↗
40. 124 Modelling of precipitation reactions in industrial processing10.1016/S1359-6454(96)00100-0 ↗
41. Dislocation interaction with semicoherent precipitates (Ω phase) in deformed Al-Cu-Mg-Ag alloy10.1016/S1359-6454(98)00188-8 ↗
42. Straining mechanisms in aluminium alloy 6056. In-situ investigation by transmission electron microscopy10.1016/S0921-5093(02)00184-3 ↗
43. Three-dimensional characterization of interaction between β″ precipitate and dislocation in Al-Mg-Si alloy10.1016/j.jallcom.2014.02.059 ↗
44. Aberration-corrected HAADF-STEM investigations of precipitate structures in Al-Mg-Si alloys with low Cu additions10.1080/14786435.2013.857051 ↗
45. Nano-scale characterisation of sheared β" precipitates in a deformed Al-Mg-Si alloy10.1038/s41598-019-53772-4 ↗
46. Detailed investigation of the shearing mechanism of β" precipitates in Al-Mg-Si alloys10.1051/matecconf/202032601005 ↗
47. Shearing and rotation of β″ and βʹ precipitates in an Al-Mg-Si alloy under tensile deformation: in-situ and ex-situ studies10.1016/j.actamat.2021.117310 ↗
48. Dislocation dynamics simulations with climb: kinetics of dislocation loop coarsening controlled by bulk diffusion10.1080/14786435.2011.573815 ↗
49. A model for the thermodynamics of and strengthening due to co-clusters in Al–Mg–Si-based alloys10.1016/j.actamat.2012.04.032 ↗
50. Hosford · 2010
51. Ultrafine grains and the Hall–Petch relationship in an Al–Mg–Si alloy processed by high-pressure torsion10.1016/j.msea.2011.10.074 ↗
52. Observation of ductile intercrystalline fracture of an Al-Zn-Mg-alloy10.1016/0001-6160(77)90174-2 ↗
53. Interface controlled plastic flow modelled by strain gradient plasticitytheory10.1016/j.crme.2012.02.008 ↗
54. The localization of plastic deformation in the precipitate free zone of an Al-Mg-Si-Mn alloy10.1016/j.actamat.2022.117872 ↗
55. Grain boundary versus transgranular ductile failure10.1016/S0022-5096(02)00102-3 ↗
56. Multiscale modeling of ductile failure in metallic alloys10.1016/j.crhy.2010.07.012 ↗
57. A study of the influence of precipitate-free zones on the strain localization and failure of the aluminium alloy AA7075-T65110.1080/14786435.2015.1040099 ↗
58. A model for predicting fracture mode and toughness in 7000 series aluminium alloys10.1016/j.actamat.2004.01.044 ↗
59. Anisotropic ductile fracture of Al 2024 alloys10.1016/j.engfracmech.2007.04.008 ↗
60. On fracture anisotropy in textured aluminium alloys
61. Strain localization analysis in materials containing randomly distributed voids: competition between extension and shear failure modes10.1016/j.jmps.2022.104933 ↗
62. Effects of manganese and zirconium dispersoids on strain localization in aluminum alloys10.3390/met11020200 ↗