Processing defect, microstructure evolution and mechanical properties of laser powder bed fusion Al-12Si alloys
Source abstract
Abstract
The laser power and scan speed are significant processing parameters influencing the defects and microstructures due to affecting the thermal state within the melt pool during laser powder bed fusion (LPBF). To this end, these process parameter combinations under a constant laser energy density are correlated with defects (balling phenomenon and pores) and microstructures (melt pool arrangement and cell morphology). Setting the parameter combination (laser power and scan speed are 200 W and 910 mm/s, respectively) yields large balling droplets (average size of 150 μm) due to the relatively high melt viscosity resulting from the low melt pool temperature. In this case, a limited surface tension difference acting on a liquid surface cannot provide sufficient driving forces against viscous drags to promote the efficient spreading of the molten alloy. Cavity regions are formed between the large balling droplets and the previous layer, forming lack-of -fusion pores. By increasing the laser power and scan speed gradually, samples with relative densities greater than 99.5% are produced. This phenomenon can be attributed to the increases in laser power and scan speed, which improves the spreading ability of the molten alloy. With increasing laser power and scan speed, the cell size decreases (from 0.51 μm to 0.42 μm) because of the increase in the cooling rate. The sample (laser power and scan speed are 350 W and 1590 mm/s, respectively) has the highest performance (310 MPa yield strength, 470 MPa ultimate tensile strength, and 6.6% fracture strain) due to its highest relative density (greater than 99.5%) and fine microstructure (average cell size of 0.45 μm). All four samples exhibit anisotropic mechanical properties resulting from the combination of the melt pool boundary and lack-of-fusion pores.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
2. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
3. A lightweight and support-free design method for selective laser melting
4. Development of gradient microstructure in the lattice structure of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.jmst.2019.06.015 ↗
5. Porosity formation mechanisms and fatigue response in Al-Si-Mg alloys made by selective laser melting10.1016/j.msea.2017.11.078 ↗
6. Microstructures and mechanical properties of A356 (AlSi7Mg0.3) aluminum alloy fabricated by selective laser melting10.1016/j.matdes.2015.10.065 ↗
7. Reducing porosity in AlSi10Mg parts processed by selective laser melting
8. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
9. Investigation into spatter behavior during selective laser melting of AISI 316L stainless steel powder10.1016/j.matdes.2015.08.086 ↗
10. A study on the effect of energy input on spatter particles creation during selective laser melting process
11. The effect of texture on the anisotropy of thermophysical properties of additively manufactured AlSi10Mg
12. Heterogeneous microstructure and voids dependence of tensile deformation in a selective laser melted AlSi10Mg alloy10.1016/j.msea.2020.140109 ↗
13. 3D printing of Aluminium alloys: additive Manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
14. Selective laser melting of AlSi10Mg alloy: process optimisation and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
15. Microstructure prediction of selective laser melting AlSi10Mg using finite element analysis10.1016/j.matdes.2018.01.022 ↗
16. Fracture resistance of AlSi10Mg fabricated by laser powder bed fusion10.1016/j.actamat.2021.116869 ↗
17. Stress partitioning behavior of an AlSi10Mg alloy produced by selective laser melting during tensile deformation using in situ neutron diffraction10.1016/j.jallcom.2016.06.011 ↗
18. Anisotropy in local microstructure – does it affect the tensile properties of the SLM samples?10.1016/j.mfglet.2018.02.012 ↗
19. Anisotropic mechanical behavior of AlSi10Mg parts produced by selective laser melting10.1007/s11837-016-2230-5 ↗
20. Role of melt pool boundary condition in determining the mechanical properties of selective laser melting AlSi10Mg alloy10.1016/j.msea.2018.10.083 ↗
21. Electrical resistivity of additively manufactured AlSi10Mg for use in electric motors
22. Microstructural origin of the anisotropic flow stress of laser powder bed fused AlSi10Mg10.1016/j.actamat.2021.117346 ↗
23. A simple scaling model for balling defect formation during laser powder bed fusion
24. Microstructure and mechanical properties of AlSi10Mg alloy built by laser powder bed fusion/direct energy deposition hybrid laser additive manufacturing
25. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al–Si-based alloys
26. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
27. Effect of solution and aging treatments on the microstructure and mechanical properties of dual-phase high-entropy alloy prepared by laser-powder bed fusion using AlSi10Mg and FeCoCrNi powders10.1007/978-3-031-04721-3 ↗
28. The effect of atmosphere on the structure and properties of a selective laser melted Al–12Si alloy10.1016/j.msea.2014.01.012 ↗
29. Influence of scan strategy and molten pool configuration on microstructures and tensile properties of selective laser melting additive manufactured aluminum based parts10.1016/j.optlastec.2017.08.015 ↗
30. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
31. Observation of spatter-induced stochastic lack-of-fusion in laser powder bed fusion using in situ process monitoring
32. Factors that affect the properties of additively-manufactured AlSi10Mg: porosity versus microstructure
33. Effect of processing parameters on pore structures, grain features, and mechanical properties in Ti-6Al-4V by laser powder bed fusion
34. Quantification and characterisation of porosity in selectively laser melted Al–Si10–Mg using X-ray computed tomography10.1016/j.matchar.2015.12.001 ↗
35. On the role of melt flow into the surface structure and porosity development during selective laser melting10.1016/j.actamat.2015.06.004 ↗
36. Damage mechanisms in selective laser melted AlSi10Mg under as built and different post-treatment conditions10.1016/j.msea.2019.138210 ↗
37. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
38. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
39. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗
40. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes
41. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
42. Superheat-dependent microstructure of molten Al–Si alloys of different compositions studied by small angle neutron scattering10.1016/j.jallcom.2012.09.086 ↗
43. Rapid solidification: selective laser melting of AlSi10Mg10.1007/s11837-015-1763-3 ↗
44. Pulsed SLM-manufactured AlSi10Mg alloy: mechanical properties and microstructural effects of designed laser energy densities10.1016/j.jmapro.2018.09.007 ↗
45. Gradient in microstructure and mechanical property of selective laser melted AlSi10Mg10.1016/j.jallcom.2017.11.020 ↗
46. Influence of working environment and built orientation on the tensile properties of selective laser melted AlSi10Mg alloy10.1016/j.msea.2019.01.103 ↗
47. Effect of construction angles on microstructure and mechanical properties of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.jallcom.2021.160459 ↗
48. Modeling strength and failure variability due to porosity in additively manufactured metals10.1016/j.cma.2020.113471 ↗
49. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting10.1016/j.actamat.2016.06.009 ↗
50. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: effect of heat treatment10.1016/j.msea.2013.10.023 ↗
51. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
52. Microstructure and strength analysis of eutectic Al-Si alloy in-situ manufactured using selective laser melting from elemental powder mixture10.1016/j.jallcom.2016.08.249 ↗
53. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder b e d fusion10.1016/j.actamat.2021.116698 ↗
54. Effect of energy per layer on the anisotropy of selective laser melted AlSi12 aluminium alloy
55. Fatigue assessment of laser additive manufactured AlSi12 eutectic alloy in the very high cycle fatigue (VHCF) range up to 1E9 cycles10.1016/j.matpr.2016.07.004 ↗
56. Influence of process-induced microstructure and imperfections on mechanical properties of AlSi12 processed by selective laser melting10.1016/j.jmatprotec.2015.02.023 ↗
57. Influence of Si precipitates on fracture mechanisms of AlSi10Mg parts processed by Selective Laser Melting10.1016/j.actamat.2019.06.013 ↗
58. Effect of molten pool boundaries on the mechanical properties of selective laser melting parts10.1016/j.jmatprotec.2014.06.002 ↗