Coupled effect of Ag and In addition on the microstructure and mechanical properties of Sn–Bi lead-free solder alloy

Tianhan Hu, Shun Li, Zhen Li, Guanzhi Wu, Ping Zhu, Wufeng Dong, Yu Sun, Jiayi Zhou, Bingjia Wu, Bingge Zhao, Kai Ding, Yulai Gao

Abstract

The microstructure and mechanical properties of Sn-Bi solder alloys with various Ag and In addition are comparatively investigated. The results illustrate that the tensile strength and ductility of the solder alloy could be dramatically enhanced with negligible loss of the plasticity. Especially, the Sn-Bi solder alloy with 0.4 wt. % Ag and 1.5 wt. % In exhibits the maximum tensile strength and elongation of 79.7 MPa and 45.9%, respectively. The microstructure of the Sn-Bi solder alloys is mainly composed of Bi-rich and β-Sn phases. With the addition of elements Ag and In, the microstructure is significantly refined, and the lamellar eutectic structure with thinner interlayer spacing could be detected. Element Ag tends to form Ag3Sn phase while element In solutes in the Sn matrix. The mechanical properties of the as-prepared Sn-Bi solder alloy are improved attributed to the precipitated-phase strengthening of the fined Ag3Sn phase and the refinement effect of In on coarse Bi-rich phase.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Investigation of thermal and mechanical properties of Sn-Zn and Sn-Zn-Bi near-eutectic solder alloys10.1016/j.rinma.2022.100316 ↗
2. Characterization of low-melting-point Sn-Bi-In lead-free solders10.1007/s11664-016-4366-z ↗
3. Structure and properties of Sn-Cu lead-free solders in electronics packaging10.1080/14686996.2019.1591168 ↗
4. Properties of lead-free solder alloys with rare earth element additions10.1016/j.mser.2004.01.001 ↗
5. Alloying regulation mechanism toward microstructure evolution of Sn-bi-based solder joint under current stress10.1016/j.matchar.2022.112094 ↗
6. Creep behavior of eutectic Sn-Ag lead-free solder alloy10.1557/JMR.2002.0420 ↗
7. Influence of graphene content and nickel decoration on the microstructural and mechanical characteristics of the Cu/Sn-Ag-Cu/Cu soldered joint10.1016/j.jmrt.2020.06.026 ↗
8. Effects of Cu and in trace elements on microstructure and thermal and mechanical properties of Sn-Zn eutectic alloy10.1007/s11664-018-06869-x ↗
9. Microstructural and mechanical properties analysis of extruded Sn-0.7Cu solder alloy10.1016/j.jmrt.2014.12.005 ↗
10. Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn-Bi solder alloy10.1016/j.matchar.2015.06.026 ↗
11. Effects of Ag content on the reliability of LED package component with Sn-Bi-Ag solder10.1007/s10854-015-3546-6 ↗
12. Improvement of microstructure and tensile properties of Sn-Bi-Ag alloy by heterogeneous nucleation of β-Sn on Ag3Sn10.1016/j.msea.2020.139372 ↗
13. Microstructural stability of Sn-1Ag-0.5Cu-xAl (x=1, 1.5, and 2wt.%) solder alloys and the effects of high-temperature aging on their mechanical properties10.1016/j.matchar.2013.01.015 ↗
14. Influences of Ag addition to Sn-58Bi solder on SnBi/Cu interfacial reaction10.1016/j.matlet.2017.11.127 ↗
15. Effect of Zn addition on interfacial reactions between Sn-Bi solder and Cu substrate10.2320/matertrans.MD201515 ↗
16. Depressing effect of 0.1wt.% Cr addition into Sn-9Zn solder alloy on the intermetallic growth with Cu substrate during isothermal aging10.1016/j.matchar.2009.12.019 ↗
17. Properties of Sn3.8Ag0.7Cu solder alloy with trace rare earth element Y additions10.1007/s11664-007-0138-0 ↗
18. Three-dimensional (3D) microstructure visualization of LaSn3 intermetallics in a novel Sn-rich rare-earth-containing solder10.1016/j.matchar.2007.10.008 ↗
19. Interfacial microstructure, wettability and material properties of nickel (Ni) nanoparticle doped tin-bismuth-silver (Sn-Bi-Ag) solder on copper (Cu) substrate10.1007/s10854-015-4252-0 ↗
20. Influence of lanthanum additions on the microstructure and microhardness of Sn-3.5Ag solder10.1007/s11664-009-0863-7 ↗
21. Cadmium sulfide cage photocatalysis coupled electroactive biofilm for synergistic promotion of tetracycline degradation and electricity production10.1016/j.jmst.2023.05.018 ↗
22. A zero-dimensional/two-dimensional Ag-Ag2S-CdS plasmonic nanohybrid for rapid photodegradation of organic pollutant by solar light10.1016/j.chemosphere.2022.133973 ↗
23. Synergistic effect of erosion and hydrogen on properties of passive film on 2205 duplex stainless steel10.1016/j.jmst.2020.08.004 ↗
24. The modification and strengthening dual functionality of rare-earth oxide in La2O3-BaO-SiO2 glass for high temperature sealing application10.1016/j.jallcom.2023.169892 ↗
25. Benzo[1, 2-b: 4, 5-b']dithiophene-based copolymers as panchromatic light sensors in organic photodiodes application10.1016/j.jmrt.2020.11.034 ↗
26. Synchronous improvement of mechanical properties and stress corrosion resistance by stress-aging coupled with natural aging pre-treatment in an Al-Zn-Mg alloy with high recrystallization fraction10.1016/j.jmst.2021.11.068 ↗
27. In situ growth of 1D/2D CdS-Bi2MoO6 core shell heterostructures for synergistic enhancement of photocatalytic performance under visible light10.1016/j.chemosphere.2021.130086 ↗
28. Nanoscale analysis of the interface structure and strain of the Bi2Sr2CaCu2O8+δ/LaAlO3 heterogeneous system10.1016/j.jallcom.2023.169734 ↗
29. Coupled effect of SOC and SOH on tensile behaviors of lithium-ion battery electrodes10.1016/j.est.2023.107782 ↗
30. Low melting point solders based on Sn, Bi, and in elements
31. Effect of Ag nanoparticles on microstructure, damping property and hardness of low melting point eutectic tin-bismuth solder10.1007/s10854-017-7465-6 ↗
32. Effect of in on microstructure, thermodynamic characteristic and mechanical properties of Sn-Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
33. The growth and stress vs. strain characterization of the silver solid solution phase with indium10.1016/j.jallcom.2015.11.212 ↗
34. Role of the aging treatment in the microstructure evolution and mechanical properties of Cu/Sn-Bi-Ag-In/Cu joint
35. Cu and Ag additions affecting the solidification microstructure and tensile properties of Sn-Bi lead-free solder alloys10.1016/j.msea.2017.08.059 ↗
36. Effect of the addition of CeO2 nanoparticles on the microstructure and shear properties of Sn–57Bi–1Ag solder alloy10.1016/j.jmrt.2023.07.260 ↗
37. Effects of in and Ni addition on microstructure of Sn-58Bi solder joint10.1007/s11664-014-3359-z ↗
38. Phase equilibria and solidification of ternary Sn-Bi-Ag alloys10.1016/j.jallcom.2010.03.067 ↗
39. Complex eutectic growth and Bi precipitation in ternary Sn-Bi-Cu and Sn-Bi-Ag alloys10.1016/j.jallcom.2016.09.003 ↗
40. Influences of substrate alloying and reflow temperature on Bi segregation behaviors at Sn-Bi/Cu interface10.1007/s11664-011-1742-6 ↗
41. Comparison of Sn2.8Ag20In and Sn10Bi10In solders for intermediate-step soldering10.1007/s11664-006-0302-y ↗
42. Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi-Sn based lead-free solder alloys10.1016/j.msea.2012.09.038 ↗
43. A SnBiAgIn solder alloy with exceptional mechanical properties by rapid quenching10.1007/s10854-021-05539-9 ↗
44. Tensile properties dependency on crystal size and direction of single crystal Ag3Sn intermetallic compound: a molecular dynamics study10.1016/j.jmrt.2022.07.188 ↗
45. Improved reliability and mechanical performance of Ag microalloyed Sn58Bi solder alloys10.3390/met9040462 ↗
46. Improvements in mechanical properties of Sn-Bi alloys with addition of Zn and in10.1016/j.msea.2021.141131 ↗
47. Effects of a third element on microstructure and mechanical properties of eutectic Sn-Bi solder10.5104/jiepeng.2.98 ↗