Effect of Ag addition on the microstructure and corrosion properties of Sn–9Zn lead-free solder
Source abstract
Abstract
The effects of Ag addition on the microstructure of Sn–9Zn alloy and its corrosion behaviour in neutral and static 3.5 wt% NaCl solutions were investigated using surface characterization techniques and electrochemical techniques. The results show that in Sn–9Zn-xAg alloys, Ag reacts with Zn to form AgZn3 intermetallic compounds (IMCs), which refined the microstructure of the alloys and changed the corrosion mode of the alloy surfaces from pitting corrosion to surface corrosion. The addition of Ag effectively improved the corrosion passivation film structure and electron transfer characteristics of the alloy, increased the self-corrosion potential (Ecorr) and reduced the self-corrosion current (Icorr), thus improving the corrosion resistance of the alloy. The study explained and verified the corrosion mechanism of the alloy from both experimental and theoretical perspectives. It is concluded that Sn–9Zn-0.4Ag alloy shows relatively the best corrosion resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Elevated damping properties of lead-free solders under electric current stressing10.1016/j.scriptamat.2022.115230 ↗
2. Significantly enhanced ductility of Sn–57Bi–1Ag alloy induced by microstructure modulation from in addition10.1007/s10854-023-10946-1 ↗
3. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
4. Lead-free solders: focus on fundamentals, reliability, and applications
5. Effect of Bi on the microstructure and mechanical properties of Sn-Zn alloys processed by rolling10.1016/j.matchar.2018.01.017 ↗
6. Effect of Cu content on performance of Sn-Zn-Cu lead-free solder alloys designed by cluster-plus-glue-atom model10.3390/ma14092335 ↗
7. Study on the effects of Ag addition on the mechanical properties and oxidation resistance of Sn–Zn lead-free solder alloy by high-throughput method10.1007/s10854-022-09756-8 ↗
8. Effects of Ga alloying on microstructure and comprehensive performances of Sn–9Zn–2Bi alloys for the microelectronics industry10.1016/j.microrel.2022.114599 ↗
9. Corrosion failure due to flux residues in an electronic add-on device10.1016/j.engfailanal.2010.02.010 ↗
10. A climate classification for corrosion control in electronic system design
11. Statistical analysis of corrosion failures in hearing aid devices from tropical regions10.1016/j.engfailanal.2021.105758 ↗
12. Electrochemical corrosion behavior of Sn-0.7Cu solder alloy with the addition of bismuth and iron10.1016/j.jallcom.2019.151925 ↗
13. A diffusion model and growth kinetics of interfacial intermetallic compounds in Sn-0.3Ag-0.7Cu and Sn-0.3Ag-0.7Cu-0.5CeO2 solder joints10.1016/j.jallcom.2019.152893 ↗
14. Effect of minor Cu addition on corrosion behavior of Sn-Zn-xCu touch-up solder alloys10.1002/maco.201609313 ↗
15. New solder based on the Sn-Zn eutectic with addition of Ag, Al, and Li10.1007/s11665-023-08103-0 ↗
16. Effect of Al and Bi addition on the corrosion behaviour, hardness, and melting temperature of lead-free solder alloys10.1016/j.microrel.2023.115051 ↗
17. Corrosion behaviour of Sn-9Zn-xS solders in 3.5 wt-% NaCl solution10.1080/02670836.2022.2159635 ↗
18. Ti addition to enhance corrosion resistance of Sn–Zn solder alloy by tailoring microstructure10.1016/j.jallcom.2015.04.168 ↗
19. Effects of small addition of Ag and/or Cu on the microstructure and properties of Sn–9Zn lead-free solders10.1016/j.msea.2010.04.078 ↗
20. Effect of Ag-content on structure, corrosion behaviour and mechanical properties of Sn-9Zn lead-free solder alloy10.1051/epjap/2010150 ↗
21. Corrosion measurement on shear strength of Cu/Sn–9Zn/Cu lap joints10.1016/j.measurement.2015.02.016 ↗
22. Mechanical properties and electrochemical corrosion behavior of Al/Sn-9Zn-xAg/Cu joints10.1007/s11664-010-1459-y ↗
23. Linagliptin drug molecule as corrosion inhibitor for mild steel in 1 M HCl solution: electrochemical, SEM/XPS, DFT and MC/MD simulation approach10.1016/j.colsurfa.2022.130885 ↗
24. Effect of Nd addition on the corrosion behavior of SAC305 solder alloy10.1016/j.corsci.2023.111264 ↗
25. Effect of polyvinyl chloride fire smoke on the long-term corrosion kinetics and surface microstructure of tin–lead and lead-free solders10.1007/s10854-019-02013-5 ↗
26. Corrosion measurement of Sn–Zn lead-free solders in 6 M KOH solution10.1016/j.measurement.2013.10.002 ↗
27. Electrochemical behaviors of the Sn-9Zn-xAg lead-free solders in a 3.5 wt % NaCl solution10.1149/1.1756890 ↗
28. Electrochemical corrosion behaviour of Sn-Zn-xBi alloys used for miniature detonating cords10.1016/j.jmst.2019.03.026 ↗
29. XPS analysis of oxide films on lead-free solders with trace additions of germanium and gallium10.4028/www.scientific.net/MSF.857.63 ↗
30. Effect of Ag3Sn intermetallic compounds on corrosion of Sn-3.0Ag-0.5Cu solder under high-temperature and high-humidity condition10.1016/j.corsci.2012.05.006 ↗
31. XPS study of the surface chemistry of conventional hot-dip galvanised pure Zn, galvanneal and Zn–Al alloy coatings on steel10.1016/S1359-6454(03)00408-7 ↗
32. X-ray photoelectron spectroscopy investigation of argon ion sputtered tin oxides and solder alloy
33. Understanding corrosion mechanism of Sn-Zn alloys in NaCl solution via corrosion products characterization10.1002/maco.201508605 ↗
34. Variations of work function and corrosion behaviors of deformed copper surfaces10.1016/j.apsusc.2004.07.017 ↗
35. Ag layer deposited on Zn by physical vapor deposition with enhanced CO selectivity for electrochemical CO2 reduction10.1016/j.apsusc.2020.146651 ↗
36. High throughput preparation of Ag-Zn alloy thin films for the electrocatalytic reduction of CO(2) to CO10.3390/ma15196892 ↗
37. Work function of metals: relation between theory and experiment10.1016/0079-6816(81)90003-4 ↗
38. Electrochemical behavior of Zn-xSn high-temperature solder alloys in 0.5 M NaCl solution10.1016/j.jallcom.2017.04.281 ↗
39. Electrochemical corrosion behaviour of Sn–Sb solder alloys: the roles of alloy Sb content and type of intermetallic compound10.1080/1478422X.2020.1791446 ↗
40. On the pitting corrosion of tin by sulphate anion10.1016/0010-938X(92)90009-R ↗
41. Study on corrosion behavior of β-Sn and intermetallic compounds phases in SAC305 alloy by in-situ EC-AFM and first-principles calculation10.1016/j.corsci.2021.109244 ↗
42. Effect of Al on the electrochemical corrosion behaviour of Pb free Sn–8.5 Zn–0.5 Ag–XAl–0.5 Ga solder in 3.5% NaCl solution10.1016/j.apsusc.2005.08.020 ↗
43. The role of Zn precipitates and Cl− anions in pitting corrosion of Sn–Zn solder alloys10.1016/j.corsci.2014.12.014 ↗
44. Electrochemical corrosion behaviour of lead-free Sn–8.5 Zn–X Ag–0.1 Al–0.5 Ga solder in 3.5% NaCl solution10.1016/j.msea.2005.05.101 ↗
45. Effect mechanism of Ag and Bi elements on the corrosion process in Sn–9Zn–1Ag and Sn–9Zn–3Bi solders10.1088/2053-1591/ab2663 ↗
46. Kinetics of oxygen evolution on Pb and Pb-Ag anodes during zinc electrowinning10.1016/0013-4686(95)00439-4 ↗
47. Electrochemical corrosion study of Pb-free solders10.1557/jmr.2006.0035 ↗
48. Electrochemical impedance spectroscopy (EIS) as a new tool for investigating methods of corrosion protection10.1016/0013-4686(90)80007-B ↗
49. An electrochemical impedance spectroscopy study of the corrosion behaviour of PVD coated steels in 0.5 N NaCl aqueous solution: Part I. Establishment of equivalent circuits for EIS data modelling10.1016/S0010-938X(02)00213-5 ↗
50. Effect of trace Mn modification on the microstructure and corrosion behavior of Sn−9Zn solder alloy10.1002/maco.201709694 ↗
51. Characterisation of passive films formed on mild steels in bicarbonate solution by EIS10.1016/S0013-4686(02)00077-4 ↗
52. Electronic structure and pitting susceptibility of passive film on carbon steel10.1016/S0013-4686(99)00011-0 ↗
53. Electronic and transport properties of passive films grown on different Ni-Cr binary alloys in relation to the pitting susceptibility10.1016/j.electacta.2014.04.067 ↗
54. Characterization of the passive state on zinc10.1149/1.1838777 ↗
55. Electrochemical and surface characteristics of tin oxide and indium oxide electrodes10.1021/ac60368a035 ↗
56. Electrochemical properties of polycrystalline tin oxide10.1149/1.2407316 ↗
57. Characterization of the passive state on zinc10.1149/1.1838777 ↗
58. Impedance spectroscopy of emiconducting films on tin electrodes10.1016/S0013-4686(99)00298-4 ↗
59. Metastable pitting and its correlation with electronic properties of passive films on Sn–xZn solder alloys10.1016/j.corsci.2015.06.036 ↗
60. Flat-band potential of a semiconductor: using the Mott–Schottky equation10.1021/ed084p685 ↗
61. Metastable pitting and semiconductive properties of passive films10.1149/1.2069520 ↗