journal article·2023-07Open access

Precipitated phase characteristics and fracture behaviour of cast Al–Cu–Mn alloy

Fan Zhang, Dongjin Shi, Ziyu He, Xiao Wang, Lu Li, Zhaolin Zhan, Zhentao Yuan

Abstract

The cast Al4.4Cu0.6Mn alloy samples were subjected to quenching at 530°C for 14 h, followed by aging treatment at 170°C for 6, 8, 10, and 12 h. The effects of aging treatment time on the mechanical properties including the tensile strength (σb), yield strength (σ0.2), elongation (δ5), hardness (HB), and microstructure morphology of the alloy were investigated using metallographic microscopy, scanning electron microscopy, transmission electron microscopy, X-ray diffraction, tensile-property, and hardness tests. The highest tensile strength of the alloy was 481.4 MPa when the aging time was 8 h. The size of precipitates increased gradually with the increase in aging time, and their morphology developed gradually from granular and bundle to reticulation. The main strengthening phases of the alloy were the θ- and T-phases as determined by X-ray diffraction and energy dispersive spectroscopy. Dimples and tear ridges were observed in the fracture morphology of four samples after different aging times, indicating that the fracture mode for the studied alloy is quasi-cleavage fracture. The T-phase has better thermal stability. Therefore, the mechanical properties of the alloy under the heat treatment conditions in this paper were stable and were not significantly affected by the aging time.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Development of hybrid aluminium metal matrix composite and study of property10.1016/j.matpr.2018.02.291 ↗
2. Status and prospect for aluminum industrial development in China
3. Laser welding dissimilar materials of aluminum to steel: an overview10.1007/s00170-016-8725-y ↗
4. Development and application prospects of aluminum-lithium alloys in aircraft and space technology10.1007/s11015-021-01134-9 ↗
5. Characteristic microstructure and microstructure evolution in Al-Cu-Mn alloy under projectile impact10.1016/j.msea.2011.09.109 ↗
6. Dendrite coarsening during directional solidification of Al-Cu-Mn alloys10.1016/S0921-5093(97)00720-X ↗
7. Monotectic Al-Bi-Sn alloys directionally solidified: effects of Bi content, growth rate and cooling rate on the microstructural evolution and hardness10.1016/j.jallcom.2015.09.009 ↗
8. Effects of two-step homogenization on precipitation behavior of Al3Zr dispersoids and recrystallization resistance in 7150 aluminum alloy10.1016/j.matchar.2015.02.016 ↗
9. Influence of electric field on microstructure and mechanical properties of an Al-Cu-Li alloy during ageing10.1016/j.matdes.2016.03.013 ↗
10. Effect of Mn and AlTiB addition and heat treatment on the microstructures and mechanical properties of Al-Si-Fe-Cu-Zr alloy10.1166/jnn.2018.15638 ↗
11. Effect of homogenization treatment on microstructure and mechanical properties of Al-4.5Cu-1.5Mg-0.6Mn-0.2Ti-0.5Zr alloy
12. Effect of Cu and Mn content on solidification microstructure, T-phase formation and mechanical property of Al-Cu-Mn alloys10.1016/j.jallcom.2018.09.362 ↗
13. Microstructure and mechanical properties of as-cast Al-5.0Cu-0.6Mn-0.6Fe alloy produced by ultrasonic vibration and applied pressure10.1016/S1875-5372(18)30088-2 ↗
14. Twinning and orientation relationships of T-phase precipitates in an Al matrix10.1007/s10853-012-7102-y ↗
15. Microstructural characterization of mechanically alloyed Al-Cu-Mn alloy with zirconium10.1016/j.msea.2014.11.048 ↗
16. Morphologies, orientation relationships, and evolution of the T-phase in an Al-Cu-Mg-Mn alloy during homogenisation10.1016/j.jallcom.2017.03.161 ↗
17. Atomic-scale mapping of twins and relevant defective structures in Al20Cu2Mn3 decagonal approximant10.1080/14786435.2016.1205229 ↗
18. Effects of heat treatment on microstructure and mechanical properties of Al-Cu-Mn cast aluminum alloy
19. Quasicrystalline phases in conventionally cast Fe-containing Al-Cu-Mn alloys and its evolution during the annealing at 530 °C
20. Localized corrosion susceptibility of Al-Li-Cu-Mg-Zn alloy AF/C458 due to interrupted quenching from solutionizing temperatures10.1007/s11661-001-0046-5 ↗
21. Deformation behavior of an Al-Cu-Mg-Mn-Zr alloy during hot compression10.1007/s10853-010-5143-7 ↗
22. Microstructure and mechanical behavior of spray-deposited Al-Cu-Mg(-Ag-Mn) alloys10.1007/s11661-000-0145-8 ↗
23. The influence of grain structure on the ductility of the Al- Cu- Li- Mn- Cd alloy 202010.1007/BF02648396 ↗
24. Effects of two-stage creep-aging processing on mechanical properties of an Al-Cu-Mg alloy10.1016/j.matdes.2015.04.047 ↗
25. Effects of creep-aging processing on the corrosion resistance and mechanical properties of an Al-Cu-Mg alloy10.1016/j.msea.2014.03.055 ↗
26. Precipitation hardening of 2024-T3 aluminum alloy during creep aging10.1016/j.msea.2012.12.058 ↗
27. Microstructure evolution and mechanical properties of the electron-beam welded joints of cast Al–Cu–Mg–Ag alloy10.1016/j.msea.2020.140363 ↗
28. Strengthening mechanisms and deformation behavior of cryomilled Al-Cu-Mg-Ag alloy10.1016/j.jallcom.2015.01.160 ↗
29. Precipitation structure and strengthening mechanisms in an Al-Cu-Mg-Ag alloy10.1016/j.msea.2017.06.110 ↗
30. Strengthening of an Al-Cu-Sn alloy by deformation-resistant precipitate plates10.1016/j.actamat.2008.03.028 ↗
31. Enhanced strength-plasticity combination in an Al-Cu-Mg alloy-atomic scale microstructure regulation and strengthening mechanisms[J]