journal article·2024-09Open access

Mechanical characterization and microstructural evolution of Inconel 718 and SS316L TIG weldments at high temperatures

Balram Yelamasetti, B. Tulasi Lakshmi Devi, Kuldeep K. Saxena, Pankaj Sonia, T. Vishnu Vardhan, N. Santhi Sree, Rashi khubnani, Hany Sayed Abdo, Ibrahim Alnaser

Abstract

This study examines the impact of both constant and pulsed current on the tensile characteristics, micro-hardness of weld surface, and metallurgical properties of the Inconel 718 and SS316L weldments. The Tungsten Inert Gas (TIG) welding process utilized two distinct arc modes to combine incompatible metals. The pulse frequency was systematically adjusted within the range of 2 Hz–6 Hz in order to investigate its impact on the welding parameters. A tensile test was performed using a universal testing equipment under various temperature conditions, including room temperature and an elevated temperature of 350 °C. When the samples were welded at a frequency of 4 Hz, both the Ultimate Tensile Strength (UTS) and Yield Strength (YS) were greater compared to when the samples were welded at 2 Hz, 6 Hz, or a continuous arc mode. Furthermore, it was noted that the YS-to-UTS ratio was higher for the weldments produced at 4 Hz pulse frequency. The UTS of current and pulsed (4 Hz) modes at a temperature of 350 °C were determined to be 505 and 524 MPa, respectively. Pulse welding demonstrated a higher hardness number compared to steady welding due to the regulated rate of heat. The TIG weldments of Inconel 718 and SS316L demonstrated superior mechanical and metallurgical qualities when exposed to elevated temperatures. The practical implications of these findings are relevant to the fabrication of turbine discs and shafts.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Influence of filler metals and welding techniques on the structure–property relationships of Inconel 718 and AISI 316L dissimilar weldments10.1016/j.matdes.2014.05.019 ↗
2. Experimental investigation of the effect of induction preheating on the microstructure evolution and corrosion behaviour of dissimilar FSW (IN718 and SS316L) joints10.1016/j.jmapro.2023.04.021 ↗
3. Effect of induction preheating on microstructure and mechanical properties of friction stir welded dissimilar material joints of Inconel 718 and SS316L10.1016/j.cirpj.2022.12.014 ↗
4. Interface characteristics and mechanical behavior of additively manufactured multi-material of stainless steel and Inconel10.1016/j.msea.2022.143318 ↗
5. Ultrasonic-Magnetic field coaxial hybrid controlling the microstructure and mechanical properties of 304 stainless steel GTAW joints10.1016/j.jmrt.2023.07.055 ↗
6. Effect of interlayer time interval on GTAW based wire arc additive manufacturing of 2319 aluminium alloy10.1007/s12046-023-02183-3 ↗
7. Importance of shielding and mechanical characterization of GTAW on Ti-6Al-4V alloy sheet10.1080/09507116.2023.2224929 ↗
8. Comparison of metallurgical and mechanical properties of dissimilar joint of AISI 316 and Monel 400 developed by pulsed and constant current gas tungsten arc welding processes10.1007/s00170-020-05562-w ↗
9. Simultaneously enhanced strength and ductility of TIG welds in Inconel 718 super-alloy via ultrasonic pulse current10.1016/j.msea.2021.140894 ↗
10. The effect of TIG welding parameters and automatization for non-heat-treated Inconel 718 sheets10.1007/s13369-021-06000-z ↗
11. Temperature-based prediction of joint hardness in TIG welding of inconel 600, 625 and 718 nickel superalloys10.3390/ma14020442 ↗
12. Maximizing strength and corrosion resistance of InterPulsed TIG welded Superalloy 718 joints by RSM for aerospace applications10.1016/j.cirpj.2021.07.013 ↗
13. Influence of magnetically constricted arc traverse speed (MCATS) on tensile properties and microstructural characteristics of welded Inconel 718 alloy sheets10.1016/j.dt.2020.07.009 ↗
14. Investigating nanoindentation creep behavior of pulsed-tig welded inconel 718 and commercially pure titanium using a vanadium interlayer10.3390/met11091492 ↗
15. Dissimilar welding of high-entropy alloy to Inconel 718 superalloy for structural applications10.1557/s43578-021-00352-w ↗
16. The effect of TIG welding on the structure and hardness of butt joints made of Inconel 71810.1016/j.heliyon.2023.e13175 ↗
17. Refining microstructures and enhancing mechanical properties of Inconel 718 weldment via fast-frequency double pulsed waveforms adopting in FFP-TIG10.1016/j.jmatprotec.2023.117882 ↗
18. Metallurgical, mechanical and corrosion behaviour of pulsed and constant current TIG dissimilar welds of AISI 430 and Inconel 71810.1016/j.jmrt.2023.04.231 ↗
19. Microstructure and high-temperature mechanical properties of Inconel 718 superalloy weldment affected by fast-frequency pulsed TIG welding10.1016/j.jmapro.2023.01.076 ↗
20. The effects of oxide fluxes on the penetration depth of 316L and A516 steels in A-TIG welding: a comparative study
21. Experimental investigation and parametric optimization of the tungsten inert gas welding process parameters of dissimilar metals10.3390/ma15134426 ↗
22. Influence of surface-active elements on GTA welds with respect to metallographic analysis and temperature distribution
23. Multi-pass butt welding of thick AISI 316L plates by gas tungsten arc welding: microstructural and mechanical characterization10.1016/j.ijpvp.2022.104842 ↗
24. Investigation of mechanical and microstructural properties in joining dissimilar P355GH and stainless 316L steels by TIG welding process10.1016/j.ijpvp.2023.104965 ↗
25. Metallurgical, mechanical and corrosion behaviour of pulsed and constant current TIG dissimilar welds of AISI 430 and Inconel 71810.1016/j.jmrt.2023.04.231 ↗
26. Thermal and metallurgical characteristics of surface modification of AISI 8620 steel produced by TIG arcing process10.1016/j.jmatprotec.2016.10.020 ↗
27. Influence of Ta + Nb addition on microstructure and mechanical properties of ferritic stainless steel TIG weldments
28. Investigation into the viability of K-TIG for joining armour grade quenched and tempered steel10.1016/j.jmapro.2018.03.014 ↗
29. Mechanical and microstructural characterization of TIG welded dissimilar joints between 304L austenitic stainless steel and Incoloy 800HT nickel alloy10.3390/met10050559 ↗
30. Effect of welding speed, pulse frequency, and pulse width on the weld shape and temperature distribution in dissimilar laser welding of stainless steel 308 and brass alloy10.2351/7.0000364 ↗
31. Microstructural characteristics and crack formation in additively manufactured bimetal material of 316L stainless steel and Inconel 625
32. Microstructural variations across a dissimilar 316L austenitic: 9Cr reduced activation ferritic martensitic steel weld joint10.1007/s11661-015-3281-x ↗
33. Comparative study on autogenous diode laser, CO2 laser-MIG hybrid and multi-pass TIG welding of 10-mm thick Inconel 617 superalloy10.1016/j.msea.2022.143967 ↗
34. Tensile and impact behaviour of thermo mechanically treated and micro-alloyed medium carbon steel bar10.1016/j.conbuildmat.2018.10.098 ↗
35. Mechanical and microstructure properties evaluation of tig welded dissimilar metal Ss304-Ss316
36. Studies on the structural property, mechanical relationships and corrosion behaviour of Inconel 718 and SS 316L dissimilar joints by TIG welding without using activated flux10.1016/j.jmapro.2017.09.028 ↗
37. Improvement in strength and ductility of rotary friction welded Inconel 600 and stainless steel 316L with Cu interlayer10.1016/j.cirpj.2022.12.006 ↗
38. Study of metallurgical and mechanical behavior of laser butt-welded dissimilar joint of Inconel and stainless steel