Effects of Si addition on crystallization process and soft magnetic properties of high-Fe and high-Cu-content Fe–Si–B–P–Cu nanocrystalline alloys
Source abstract
Abstract
In this study, the effects of Si content on the glass-forming ability (GFA), thermal stability, annealing window, nanocrystallization process, and soft magnetic properties (SMPs) of Fe86.3-xSixB10P2Cu1.7 (x = 0, 1, 2, 3, and 4, denoted as Si0, Si1, Si2, Si3, and Si4, respectively) alloys with high Fe and Cu contents were investigated. Moderate addition of Si (x = 1, 2, and 3) enhanced the GFA and suppressed the precipitation of compound phases, thus leading to a large crystallization temperature interval (ΔTx) exceeding 185 °C for the alloys. Appropriate addition of Si also resulted in the formation of high-density and fine pre-existing α-Fe nanocrystals in as-spun ribbons and a high growth active energy of α-Fe crystals during the subsequent nanocrystallization process for the Si1, Si2, and Si3 alloys, enhancing competitive growth between α-Fe crystals and resulting in fine nanostructure and excellent SMPs of the nanocrystalline alloys (NAs). As a result, the Si1, Si2, and Si3 NAs obtained by annealing at 420 °C for 30 min exhibited excellent SMPs with saturation magnetic flux density (Bs) up to 1.84 T and a low coercivity (Hc) of approximately 10 A/m. In addition, statistical analysis of the relationship between the average grain size (D) of α-Fe crystals and Hc values of the NAs indicated that an Hc α D3 dependence is observed when the D is less than approximately 30 nm, while this dependence follows the well-known Hc α D6 relationship when the D is above 30 nm. The dependency relationship between D and Hc of NAs can guide the selection of an appropriate annealing process to optimize their SMPs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High Entropy Alloys Studies · Magnetic Properties of Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Magnetic materials and devices for the 21st century: stronger, lighter, and more energy efficient10.1002/adma.201002180 ↗
2. Applications of nanocrystalline softmagnetic materials for modern electronic devices10.1016/S1359-6462(02)00624-3 ↗
3. Soft magnetic materials for a sustainable and electrified world 2018
4. High B s Fe-based nanocrystalline alloy with high impurity tolerance10.1007/s10853-017-1557-9 ↗
5. Low core losses and magnetic properties of Fe85-86Si1-2B8P4Cu1 nanocrystalline alloys with high B for power applications (invited)10.1063/1.3535169 ↗
6. Nanocrystalline soft magnetic Fe-Si-B-P-Cu alloys with high $B$of 1.8–1.9t contributable to energy saving10.1109/TMAG.2011.2175210 ↗
7. Role of P in Nanocrystallization of ${\rm Fe}85{\rm Si}2{\rm B}8{\rm P}4{\rm Cu}_{110.1109/TMAG.2013.2285247 ↗
8. Soft magnetic Fe-Si-B-Cu nanocrystalline alloys with high Cu concentrations10.1016/j.jallcom.2017.06.128 ↗
9. Unusual alloying effects of Co and Ni on structure and magnetic properties of Fe-Si-B-Cu nanocrystalline alloys with pre-existing α-Fe nanocrystals10.1016/j.jallcom.2022.166030 ↗
10. Effect of heating rate during primary crystallization on soft magnetic properties of melt-spun Fe-B alloys10.1016/j.scriptamat.2017.01.030 ↗
11. Soft magnetic properties of rapidly-annealed nanocrystalline Fe-Nb-B-(Cu) alloys10.1016/j.jallcom.2017.06.208 ↗
12. Effect of Si on the field-induced anisotropy in Fe-rich nanocrystalline soft magnetic alloys10.1016/j.jallcom.2016.11.330 ↗
13. Core loss of ultra-rapidly annealed Fe-rich nanocrystalline soft magnetic alloys10.1016/j.jmmm.2018.12.053 ↗
14. Magnetic field induced anisotropy in nanocrystalline Fe Cu Nb Si B alloys10.1016/0921-5093(94)90760-9 ↗
15. Chapter 3 Nanocrystalline soft magnetic alloys10.1016/S1567-2719(97)10007-5 ↗
16. Soft magnetic nanocrystalline materials10.1016/0956-716X(95)00397-E ↗
17. The effect of coherent uniaxial anisotropies on the grain-size dependence of coercivity in nanocrystalline soft magnetic alloys10.1016/S0304-8853(97)00987-6 ↗
18. Local random magnetocrystalline and macroscopic induced anisotropies in magnetic nanostructures10.1016/j.jnoncrysol.2008.06.118 ↗
19. Magnetic-field-induced anisotropies and exchange softening in Fe-rich nanocrystalline soft magnetic alloys10.1016/j.scriptamat.2012.03.006 ↗
20. Effects of Si on the microstructure, soft magnetic properties and bendability of rapidly-annealed nanocrystalline Fe–Si–B–P–Cu alloy ribbons10.1016/j.jallcom.2023.168799 ↗
21. Effects of the substitution of Si by P on crystallization behavior, soft magnetic properties and bending ductility of FeSiBCuPC alloys10.1016/j.jallcom.2019.152534 ↗
22. Effects of Si content on structure and soft magnetic properties of Fe81.3SixB17-xCu1.7 nanocrystalline alloys with pre-existing α-Fe nanocrystals10.1007/s10853-020-05404-w ↗
23. The scherrer formula for X-ray particle size determination10.1103/PhysRev.56.978 ↗
24. Direct synthesis of Fe-Si-B-C Cu nanocrystalline alloys with superior soft magnetic properties and ductile by melt-spinning10.1016/j.jmst.2021.08.055 ↗
25. Effect of the substitution of Si for B on thermal stability, magnetic properties and corrosion resistance in novel Fe-rich amorphous soft magnetic alloy10.1016/j.intermet.2021.107306 ↗
26. Significant improvement of soft magnetic properties for Fe-based nanocrystalline alloys by inhibiting surface crystallization via a magnetic field assisted melt-spinning process10.1016/j.jmmm.2019.03.110 ↗
27. Formation and crystallization behavior of Fe-based amorphous precursors with pre-existing α-Fe nanoparticles—structure and magnetic properties of high-Cu-content Fe-Si-B-Cu-Nb nanocrystalline alloys10.1016/j.jmst.2020.05.049 ↗
28. Design of FeSiBPCu soft magnetic alloys with good amorphous forming ability and ultra-wide crystallization window10.1016/j.jmst.2022.11.019 ↗
29. Stabilizing Fe-based nanocrystalline alloys via a high-entropy strategy10.1016/j.jallcom.2021.163138 ↗
30. Recent progress in high Bs Fe-based nanocrystalline soft magnetic alloys10.1088/0022-3727/44/6/064004 ↗
31. Enhanced Ms of Fe-rich Fe-B-Cu amorphous/nanocrystalline alloys achieved by annealing treatments10.1016/j.jallcom.2022.168621 ↗
32. High B s Fe 84− x Si 4 B 8 P 4 Cu x (x = 0 – 1.5) nanocrystalline alloys with excellent magnetic softness10.1063/1.3535290 ↗
33. The role of Cu content on structure and magnetic properties of Fe–Si–B–P–Cu nanocrystalline alloys10.1007/s10853-018-3131-5 ↗
34. Optimization of crystallization behavior and soft magnetic properties of the Si-free Fe-B-P-C-Cu nanocrystalline alloys by Cu content tuning10.1016/j.mseb.2020.114740 ↗
35. Effect of heat treatment on the microstructure and soft magnetic properties of nanocrystalline Fe80.5−xCoxCu1.5Si4B14 alloys (x = 0, 2, 4, 10)10.1007/s10854-021-06429-w ↗
36. Optimization of the structure and soft magnetic properties of a Fe87B13 nanocrystalline alloy by additions of Cu and Nb10.1016/j.jmmm.2019.166001 ↗
37. Microstructure and magnetic properties of Fe 81.3 Si 4 B 13 Cu 1.7 nanocrystalline alloys with minor Nb addition10.1007/s42243-018-0087-2 ↗
38. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗