journal article·2025-07Open access

Residual stress, microstructure and micro-hardness evolution of laser powder bed fusion Ti6Al4V: Effect of stress relief annealing

Zhongxu Xiao, Xu Luo, Pan Liu, Guanjun Fu, Jun Wang, Guangxuan Zhou, Xiaojia Nie, Yang Qi, Haihong Zhu

Abstract

Stress relief annealing serves as a critical post-processing in laser powder bed fusion (LPBF) of Ti6Al4V alloy to release the inherited residual stress. However, most researches on the heat treatment of Ti6Al4V alloy in LPBF mainly focused on the high-temperature stress-relief annealing to regulate the microstructure and mechanical properties. The research on the low-temperature stress-relief annealing which has a low impact on the microstructure is relatively few. In this study, the effect of the low-temperature stress-relief annealing at 350°C on the residual stress behavior, microstructure and micro-hardness evolution were investigated systematically, with comparisons to conventional annealing treatments at 500 to 650°C. The results indicated that the residual stress can be almost released at the low-temperature annealing of 350°C with duration of 600 min, and the composition phases don’t decompose with the duration extending. When treated with the high-temperature annealing of 500°C and 650°C, the white β phase began to precipitate and its fraction increases with the duration extending. Due to the partial decomposition of the acicular α' phase in the as-built specimens to form smaller substructures, the micro-hardness of the annealed specimens is consistently higher than that of the as-built specimens. The micro-hardness reaches the highest at the annealing temperature of 500°C with the duration of 10 min.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Additive manufacturing of nano-W composite high Nb-TiAl alloys fabricated via selective laser melting10.1016/j.matlet.2023.134569 ↗
2. A high strength Al–Li alloy produced by laser powder bed fusion: densification, microstructure, and mechanical properties
3. Interior defect-induced crack initiation mechanism and initial growth behavior for Ti6Al4V alloy fabricated using laser powder bed fusion10.1016/j.jmrt.2022.10.043 ↗
4. Columnar grain width control for SS316L via hatch spacing manipulation in laser powder bed fusion10.1080/21663831.2022.2140018 ↗
5. Micro laser powder bed fusion of stainless steel 316L: cellular structure, grain characteristics, and mechanical properties10.1016/j.msea.2022.143345 ↗
6. The effect of support structure on residual stress in laser powder bed fusion of Ti6Al4V alloy10.1016/j.jmrt.2023.11.139 ↗
7. Compositional regulation in additive manufacturing of precipitation-hardening (CoCrNi)94Ti3Al3 medium-entropy superalloy: cellular structure stabilization and strength enhancement10.1016/j.compositesb.2024.111570 ↗
8. Influence of heat treatment parameters on microstructure and mechanical performance of titanium alloy in LPBF: a brief review10.1016/j.jmrt.2023.04.090 ↗
9. Underwater wire-feed laser deposition of the Ti–6Al–4V titanium alloy10.1016/j.matdes.2019.108284 ↗
10. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
11. Review on residual stress in selective laser melting additive manufacturing of alloy parts10.1016/j.optlastec.2020.106283 ↗
12. In-situ control of residual stress and its distribution in a titanium alloy additively manufactured by laser powder bed fusion10.1016/j.matchar.2023.112953 ↗
13. From crack-prone to crack-free: eliminating cracks in additively manufacturing of high-strength Mg2Si-modified Al-Mg-Si alloys10.1016/j.jmst.2024.04.009 ↗
14. Effect of stress-relief annealing on the fatigue properties of X80 welded pipes10.1016/j.msea.2021.140854 ↗
15. Mechanism of stress relaxation and phase transformation in additively manufactured Ti-6Al-4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
16. Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
17. Hybrid additive manufacturing of Ti6Al4V with powder-bed fusion and direct-energy deposition10.1016/j.msea.2023.145229 ↗
18. Review of laser powder bed fusion (LPBF) fabricated Ti-6Al-4V: process, post-process treatment, microstructure, and property
19. Impact of post-process heat treatments performed on Ti6Al4V titanium alloy specimens obtained using LPBF technology10.3390/technologies11040100 ↗
20. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: a comparative study10.1016/j.msea.2020.140415 ↗
21. Low temperature stress relief and martensitic decomposition in selective laser melting produced Ti6Al4V10.1002/mdp2.138 ↗
22. An experimental investigation on the influence of elevated-temperature constrained groove pressing on the microstructure, mechanical properties and hardening behaviour of Ti6Al4V alloy10.1016/j.msea.2020.140651 ↗
23. Effect of nano-yttria stabilized zirconia addition on the microstructure and mechanical properties of Ti6Al4V parts manufactured by selective laser melting10.1016/j.matdes.2019.107909 ↗
24. In-situ XRD study on the effects of stress relaxation and phase transformation heat treatments on mechanical and microstructural behaviour of additively manufactured Ti-6Al-4V10.1016/j.msea.2021.141534 ↗
25. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
26. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
27. Influence of rescanning parameters on selective laser melting of Ti6Al4V10.1016/j.jmapro.2022.08.034 ↗
28. Unique opportunities for microstructure engineering via trace B4C addition to Ti-6Al-4V through laser powder bed fusion process: as-built and heat-treated scenarios
29. Microstructure and mechanical property of selective laser melted Ti6Al4V dependence on laser energy density10.1108/RPJ-12-2015-0193 ↗
30. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
31. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of selective laser melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
32. Effect of subtransus heat treatment on the microstructure and mechanical properties of additively manufactured Ti-6Al-4V alloy10.1016/j.jallcom.2017.11.263 ↗
33. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
34. Review of mechanical properties of Ti-6Al-4V made by laser-based additive manufacturing using powder feedstock10.1007/s11837-015-1759-z ↗