Insights into process optimization and induction preheating for crack-free laser metal deposition of nickel-based superalloy K417G
Source abstract
Abstract
The additive manufacturing of high-γ′ precipitation-rate superalloys presents both benefits and challenges. For the fabrication of dense and crack-free K417G superalloy, this study utilized laser metal deposition (LMD) in conjunction with induction heating, conducting a comprehensive experimental exploration. The findings demonstrate that a medium energy density promotes densification. The microstructure of deposited K417G includes γ matrix, γ′ precipitation, MC carbides, and γ/γ′ eutectic. The cracking mechanism during the LMD process is intricately related to process parameters. Insufficient energy density leads to the formation of unmelted powder, resulting in localized oxidation and subsequent oxide-induced cracking. In other scenarios, it manifests as liquation cracking. Moreover, an increase in preheating temperature to between 700 °C and 900 °C induces additional ductility-dip cracking. However, by raising the preheating temperature to 1100 °C and maintaining a moderate energy density, crack-free deposits can be achieved. Such conditions not only mitigate thermal stress, but also minimize phase transition stress by preventing repeated γ′ dissolution and precipitation, resulting in a more homogeneous γ′ dimensions distribution. This study confirms the printability of K417G superalloy and enhances the technological understanding of using LMD in conjunction with induction heating to prepare non-weldable superalloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Effect of heat treatment on rotating bending fatigue properties of K417G nickel-base superalloy10.1016/j.jallcom.2022.164209 ↗
2. Microstructure and tensile properties of nickel-based superalloy K417G bonded using transient liquid-phase infiltration10.1016/j.matdes.2013.04.024 ↗
3. Effect of N content on microsegregation, microstructure and mechanical property of cast Ni-base superalloy K417G10.1016/j.msea.2017.06.044 ↗
4. Pores and cracks in the metallic glasses prepared by laser powder bed fusion10.1016/j.jmrt.2023.08.061 ↗
5. Additive manufacturing of metallic components process structure and properties10.1016/j.pmatsci.2017.10.001 ↗
6. Additive manufacturing of Ni-based superalloys: residual stress, mechanisms of crack formation and strategies for crack inhibition10.1016/j.nanoms.2022.08.001 ↗
7. Cracking behavior and control of Rene 104 superalloy produced by direct laser fabrication10.1016/j.jmatprotec.2015.06.002 ↗
8. Cracking mechanism and susceptibility of laser melting deposited Inconel 738 superalloy10.1016/j.matdes.2019.108105 ↗
9. Selective laser melting of the hard-to-weld IN738LC superalloy: efforts to mitigate defects and the resultant microstructural and mechanical properties10.1016/j.jallcom.2019.151662 ↗
10. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
11. Mesoscopic evolution of molten pool during selective laser melting of superalloy Inconel 738 at elevating preheating temperature
12. The initiation and propagation mechanism of the overlapping zone cracking during laser solid forming of IN-738LC superalloy10.1016/j.jallcom.2018.03.366 ↗
13. Reduction of the hot cracking sensitivity of CM-247LC superalloy processed by laser cladding using induction preheating10.1016/j.jmatprotec.2019.116461 ↗
14. Machine-learning assisted laser powder bed fusion process optimization for AlSi10Mg: new microstructure description indices and fracture mechanisms10.1016/j.actamat.2020.10.010 ↗
15. Processing defect, microstructure evolution and mechanical properties of laser powder bed fusion Al-12Si alloys10.1016/j.jmrt.2023.07.231 ↗
16. Fluid and particle dynamics in laser powder bed fusion10.1016/j.actamat.2017.09.051 ↗
17. Balling behavior of stainless steel and nickel powder during selective laser melting process10.1007/s00170-011-3566-1 ↗
18. Constrained groove pressing and subsequent annealing of Al-Mn-Si alloy: microstructure evolutions, crystallographic transformations, mechanical properties, electrical conductivity and corrosion resistance10.1016/j.matdes.2017.03.053 ↗
19. Direct laser metal deposition of Inconel 738
20. HAZ liquation cracking mechanism of IN-738LC superalloy prepared by laser solid forming10.1007/s11661-018-4826-6 ↗
21. Study of solidification features of nickel-base superalloys in relation with composition10.1007/BF02645057 ↗
22. High temperature oxidation of Fe-Cr alloys in atmospheres containing 2.0 % SO2 + 5.0 % O210.1016/j.corsci.2021.109481 ↗
23. Crack and wear behavior of SiC particulate reinforced aluminium based metal matrix composite fabricated by direct metal laser sintering process10.1016/j.matdes.2010.06.020 ↗
24. Boundary liquation and interface cracking characterization in laser deposition of Inconel 738 on directionally solidified Ni-based superalloy10.1016/j.scriptamat.2005.03.047 ↗
25. Heat transfer and material flow during laser assisted multi-layer additive manufacturing10.1063/1.4896751 ↗
26. Plateau–Rayleigh crystal growth of periodic shells on one-dimensional substrates10.1038/nnano.2015.23 ↗
27. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
28. Emerging metallic systems for additive manufacturing: in-situ alloying and multi-metal processing in laser powder bed fusion10.1016/j.pmatsci.2021.100795 ↗
29. The effect of powder oxidation on defect formation in laser additive manufacturing10.1016/j.actamat.2018.12.027 ↗
30. On the solidification behaviour and cracking origin of a nickel-based superalloy during selective laser melting10.1016/j.matchar.2018.12.032 ↗
31. The effect of preheating on microstructure and mechanical properties of laser solid forming IN-738LC alloy10.1016/j.msea.2017.03.046 ↗
32. Process-induced microstructural characteristics of laser consolidated IN-738 superalloy10.1016/j.msea.2010.08.003 ↗
33. The kinetics of precipitation from supersaturated solid solutions10.1016/0022-3697(61)90054-3 ↗
34. An investigation of diffusion-mediated cyclic coarsening and reversal coarsening in an advanced Ni-based superalloy10.1016/j.actamat.2016.02.067 ↗
35. New alloy design approach to inhibiting hot cracking in laser additive manufactured nickel-based superalloys10.1016/j.actamat.2023.118736 ↗
36. Tensile, creep behavior and microstructure evolution of an as-cast Ni-based K417G polycrystalline superalloy10.1016/j.jmst.2018.02.007 ↗