Influence of laser power and scanning speed on microstructure evolutions and mechanical properties of the SLM fabricated Al–Mg–Mn–Sc–Zr alloy
Source abstract
Abstract
The Al–Mg–Mn-Sc-Zr alloy is fabricated by selective laser melting (SLM). The influence of laser power and scanning speed on microstructure evolutions and mechanical properties is studied in this research. Results indicate that increasing laser power can refine grain structures and reduce anisotropy on the printing surface. However, the increase in laser power will enhance the residual stress inside the alloy, leading to a decrease in elongation. The scanning speed affects the molten pool energy input and cooling rate. When the scanning speed is between 750mm/s-1250 mm/s, the alloy achieves a good grain refinement effect and weak texture strength . In addition, there exists a large number of nano-scaled Al 3 (Sc,Zr) particles precipitated during solidification and the subsequent annealing process , which can significantly enhance yield strength of the alloy. Overall, the Al–Mg–Mn-Sc-Zr alloy has a wide SLM forming window. When the laser power ranges from 200 W to 250 W, the scanning speed ranges from 750 mm/s to 1250 mm/s, and the volume energy density ranges from 80 J/mm 3 to 130 J/mm 3 , the Al–Mg–Mn-Sc-Zr alloy can obtain good formability and mechanical property.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
2. Plasticity and fracture of cast and SLM AlSi10Mg: high-throughput testing and modeling
3. Study of in situ formed quasicrystals in Al-Mn based alloys fabricated by SLM10.1016/j.jallcom.2022.164847 ↗
4. Quality control of AlSi10Mg produced by SLM: metallography versus CT scans for critical defect size assessment
5. Selective laser sintering/melting (SLS/SLM) of pure Al, Al–Mg, and Al–Si powders: effect of processing conditions and powder properties10.1016/j.jmatprotec.2013.03.009 ↗
6. Microstructural characterization and wear performance of shot-peened TA15 titanium alloy fabricated by SLM10.1016/j.matchar.2024.113747 ↗
7. Influence of coherent intermetallic nano-precipitates on the nano-level mechanical and tribological properties of the Laser-Powder bed fused Scalmalloy10.1016/j.matchar.2022.112269 ↗
8. Mechanical behavior at elevated temperatures of an Al–Mn–Mg–Sc–Zr alloy manufactured by selective laser melting10.1016/j.msea.2021.142032 ↗
9. Optimization of heat treatment for an Al–Mg–Sc–Mn–Zr alloy with ultrafine grains manufactured by laser power bed fusion10.1016/j.matchar.2022.111977 ↗
10. Pitting and intergranular corrosion of Scalmalloy® aluminum alloy additively manufactured by Selective Laser Melting (SLM)
11. A study on Sc- and Zr-modified Al–Mg alloys processed by selective laser melting10.1016/j.msea.2021.142516 ↗
12. Influence mechanism of process parameters on relative density, microstructure, and mechanical properties of low Sc-content Al-Mg-Sc-Zr alloy fabricated by selective laser melting
13. Effect of heat treatment on microstructure and mechanical anisotropy of selective laser melted Al–Mn-Sc alloy10.1016/j.msea.2023.145743 ↗
14. A new AlSi7Mg-xSc alloy with high strength and high strain Manufactured by Selective Laser Melting10.1016/j.jmrt.2024.04.123 ↗
15. Selective laser melting of rare earth element Sc modified aluminum alloy: thermodynamics of precipitation behavior and its influence on mechanical properties
16. Effects of solute atoms re-dissolution on precipitation behavior and mechanical properties of selective laser melted Al–Mg-Sc-Zr alloys10.1016/j.msea.2022.143870 ↗
17. Deformation effect of melt pool boundaries on the mechanical property anisotropy in the SLM AlSi10Mg
18. Selective laser melting of a novel Sc and Zr modified Al-6.2 Mg alloy: processing, microstructure, and properties10.1016/j.powtec.2017.06.050 ↗
19. Microstructure and mechanical properties of a novel Al-Mg-Er-Sc-Zr alloy fabricated by selective laser melting10.1016/j.jmrt.2023.11.100 ↗
20. Thermal and mechanical properties of an Al-Mg-Sc-Zr high strength alloy fabricated by selective laser melting10.1016/j.jallcom.2023.172387 ↗
21. An SLM-processed Er- and Zr- modified Al–Mg alloy: microstructure and mechanical properties at room and elevated temperatures10.1016/j.msea.2023.145485 ↗
22. Corrosion behavior and oxide layer of selective-laser-melted Al-Mg-Sc-Zr alloy in marine atmospheric environment with different Cl−concentration10.1016/j.apsadv.2023.100572 ↗
23. Fatigue behavior of notched and unnotched AM Scalmalloy specimens subjected to different surface treatments10.1016/j.ijfatigue.2024.108146 ↗
24. Investigation of effects of process parameters on microstructure and fracture toughness of SLM CoCrFeMnNi10.1016/j.jallcom.2024.173998 ↗
25. The structure of nitrogen-supersaturated ferrite produced by ball milling10.1080/14786430802322198 ↗
26. The effect of dislocation contrast on x-ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
27. Influence of scanning strategy and parameter on microstructural feature, residual stress and performance of Sc and Zr modified Al-Mg alloy produced by selective laser melting10.1016/j.msea.2020.139593 ↗
28. Estimating grain-size distributions in nanocrystalline materials from X-ray diffraction profile analysis10.1080/01418619808224072 ↗
29. Effect of double-pulse frequency and post-weld heat treatment on microstructure and mechanical properties of metal-inert welded Al-Mg-Si alloy joints10.1016/j.msea.2024.147029 ↗
30. Predictive process diagram for parameters selection in laser power bed fusion to achieve high-density and low-cracking built parts
31. Microstructure, mechanical property and thermo-stability of traditionally and severely deformed Al–Mg–Sc–Zr alloy10.1016/j.jmrt.2022.04.082 ↗
32. Effect of continuity of annealing time on the recrystallization behavior of Al-Mg-Mn-Sc-Zr alloy10.1016/j.matlet.2020.128208 ↗
33. The effects of SLM process parameters on the relative density and hardness of austenitic stainless steel 316L10.1016/j.jmrt.2024.01.237 ↗
34. Towards the hydrogen pore in additive manufactured AlMgScZr alloy: influence factors, formation kinetics mechanism10.1016/j.jmst.2024.01.092 ↗
35. Precipitation characteristics and morphological transitions of Al3Sc precipitates10.1016/j.jallcom.2019.03.256 ↗
36. Microstructure evolution and mechanical properties of high-performance Al-Mn-Mg-Sc-Zr alloy fabricated by laser powder bed fusion10.1016/S1003-6326(24)66480-0 ↗
37. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
38. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
39. The cleavage strength of polycrystals
40. Significantly improved particle strengthening of Al–Sc alloy by high Sc composition design and rapid solidification10.1016/j.msea.2020.140304 ↗
41. The effect of texture on the anisotropy of thermophysical properties of additively manufactured AlSi10Mg
42. Size effect on fatigue performance of SLM-ed AlSi10Mg alloy: role of defect size distribution10.1016/j.ijfatigue.2024.108163 ↗
43. Enhancing tensile properties of MIG welded AA6061 joints: effect of pulse mode and post-weld heat treatment
44. Study of microstructure and mechanical properties and residual stresses of 24CrNiMo steel prepared by selective laser melting and laser melting deposition10.1016/j.jmrt.2024.01.057 ↗