journal article·2024-11Open access

Effect of heat input on microstructure and mechanical properties of AA6061 alloys fabricated by additive friction stir deposition

Q. Qiao, C.I. Tang, W.I. Lam, J. Pu, H. Shi, H. Qian, Z. Li, D. Guo, D. Zhang, C.T. Kwok, L.M. Tam

Abstract

Heat input (HI) is the major factor that affects the surface quality, microstructure and mechanical properties of the deposition during the additive friction stir deposition (AFSD) process. Effect of HI on the microstructure and mechanical performance of the AFSDed AA6061 has been in-depth explored via adjusting the values of traverse speed ( v ) and layer thickness ( t ). Results indicate that deposition with a higher HI promotes the material flow behavior as well as the plastic deformation, which effectively enhances the grain refinement and structural uniformity, and avoids the formation of defects. Meanwhile, TEM results confirm that the enhanced HI leads to the formation of a higher volume fraction of the finer precipitations (Mg 2 Si and AlFeSi phases), which assists in suppressing abnormal grain growth phenomenon and improves the bonding strength of the deposition. As HI decreases, the transfer efficiency of materials clearly reduces because of the incompletely softened materials, causing less plastic deformation and poor interlayer bonding strength of the deposition. The deposition with the lowest HI displays the worst tensile properties with the lowest micro-hardness (107 HV 0.5 ), YS (273 MPa) and UTS (303 MPa).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Non-beam-based metal additive manufacturing enabled by additive friction stir deposition10.1016/j.scriptamat.2018.03.025 ↗
2. Additive friction stir-enabled solid-state additive manufacturing for the repair of 7075 aluminum alloy10.3390/app9173486 ↗
3. Effect of heat treatment states of feedstock on the microstructure and mechanical properties of AA2219 layers deposited by additive friction stir deposition10.3390/ma16247591 ↗
4. Microstructures and mechanical behavior of Inconel 625 fabricated by solid-state additive manufacturing, Mate10.1016/j.msea.2017.03.105 ↗
5. Microstructure-deformation relationship of additive friction stir-deposition Al-Mg-Si
6. Repairing the 7075 Al alloy plate by additive friction stir deposition with different feedstock rods10.1007/s00170-024-14186-3 ↗
7. Innovative potential of additive friction stir deposition among current laser-based metal additive manufacturing processes: a review10.1016/j.cirpj.2020.12.004 ↗
8. Garcia · 2021
9. Preheating-assisted solid-state friction stir repair of Al-Mg-Si alloy plate at different rotational speeds10.1007/s12613-023-2772-9 ↗
10. Effect of overlapping deposition strategy on microstructure and mechanical properties of Al-clad steel by AFSD10.1016/j.jmapro.2024.08.044 ↗
11. A pseudo thermo-mechanical model linking process parameters to microstructural evolution in multilayer additive friction stir deposition of magnesium alloy10.1016/j.matdes.2022.111412 ↗
12. Characterization of the fatigue behavior of additive friction stir-deposition AA221910.1016/j.ijfatigue.2020.105951 ↗
13. Additive friction stir deposition of AA7075-T6 alloy: impact of process parameters on the microstructures and properties of the continuously deposited multilayered parts10.3390/app131810255 ↗
14. In situ investigation into temperature evolution and heat generation during additive friction stir deposition: a comparative study of Cu and Al-Mg-Si
15. In-Situ monitoring of additive friction stir deposition of AA6061: effect of layer thickness on the microstructure and mechanical properties
16. 2010 · vol. 4 · 1
17. Parametric investigation of parallel deposition passes on the microstructure and mechanical properties of 7075 aluminum alloy processed with additive friction stir deposition10.3390/app14010457 ↗
18. Numerical studies of effect of tool sizes and pin shapes on friction stir welding of AA2024-T3 alloy10.1016/S1003-6326(14)63469-5 ↗
19. Numerical simulation of weld formation in friction stir welding based on non-uniform tool-workpiece interaction: an effect of tool pin size10.1016/j.jmapro.2022.12.052 ↗
20. Modelling and visualisation of material flow in friction stir spot welding10.1016/j.jmatprotec.2015.06.021 ↗
21. Effect of the Zener-Hollomon parameter on the dynamic recrystallization kinetics of Mg-Zn-Zr-Yb magnesium alloy
22. The mechanism of grain coarsening in friction-stir-welded AA5083 after heat treatment10.1007/s11661-010-0426-9 ↗
23. Stability of nugget zone grain structures in high strength Al-alloy friction stir welds during solution treatment10.1016/S1359-6454(02)00598-0 ↗
24. Assessment of different techniques for quantification of α-Al(FeMn)Si and β-AlFeSi intermetallics in AA 6xxx alloys10.1016/S1044-5803(03)00036-6 ↗
25. Microstructure and mechanical properties of a structurally refined Al-Mg-Si alloy for wire-arc additive manufacturing10.1016/j.msea.2021.142318 ↗
26. Distinctive localized corrosion behavior of β-Mg2Si and α-Al(Fe,Mn)Si phases in a 6082 alloy10.1016/j.jmrt.2024.01.217 ↗
27. Characterization of heat affected zone liquation cracking in laser additive manufacturing of Inconel 71810.1016/j.matdes.2015.10.155 ↗
28. Developing ultrafine-grained structure with balanced α/γ fraction via underwater friction stir processing enables enhanced wear and corrosion resistance of duplex stainless steel10.1016/j.surfcoat.2023.129295 ↗
29. Microstructural evolution and mechanical behavior of powder metallurgy based SiC/Al-Mg-Sc-Zr nanocomposite subjected to multi-pass friction stir processing10.1016/j.msea.2021.140831 ↗
30. Insights into the microstructure evolution and mechanical behavior of dissimilar friction stir welded joints of additively manufactured AlSi10Mg and conventional 7075-T651 aluminum alloys10.1016/j.msea.2023.145407 ↗
31. Microstructure, deformation and fracture mechanisms in Al-4043 alloy produced by laser hot-wire additive manufacturing
32. Effect of thermal strain on the microstructure evolution and post-aging mechanical properties of Al-Zn-Mg-Cu alloy in simulating hot stamping process
33. A multi modal approach to microstructure evolution and mechanical response of additive friction stir deposited AZ31B Mg alloy10.1038/s41598-022-17566-5 ↗
34. Effect of welding temperature on microstructure of friction-stir welded aluminum alloy 105010.1007/s11661-014-2651-0 ↗
35. Influence of interrupted quenching on artificial aging of Al-Mg-Si alloys10.1016/j.actamat.2012.04.026 ↗
36. Characteristic and mechanism of nugget performance evolution with rotation speed for high-rotation-speed friction stir welded 6061 aluminum alloy10.1016/j.jmapro.2020.10.081 ↗
37. High-resolution elemental maps for three directions of Mg2Si phase in Al-Mg-Si alloy10.1023/A:1016545124410 ↗
38. Quantitative study on the precipitation behavior of dispersoids in DC-cast AA3003 alloy during heating and homogenization10.1016/S1359-6454(03)00160-5 ↗
39. Influence of heat treatment on the microstructure and mechanical properties of Al-Mg-Si alloy fabricated by double wires+ arc additive manufacturing10.1016/j.jmrt.2024.03.147 ↗
40. Ultrafine grained structure and improved mechanical properties of low temperature friction stir spot welded 6061-T6 Al alloys10.1016/j.matchar.2017.11.033 ↗
41. Precipitation phenomena in ultrafine grained Al-Mg-Si alloy with heterogeneous microstructure10.1016/j.actamat.2015.10.030 ↗
42. Influence of equal-channel angular pressing on precipitation in an Al-Zn-Mg-Cu alloy10.1016/j.actamat.2009.03.017 ↗
43. Laser shock peening effect on the dislocation transitions and grain refinement of Al-Mg-Si alloy10.1016/j.matchar.2014.08.020 ↗
44. Microstructure and mechanical properties of strip cast Al-Mg-Si-X alloys10.2320/matertrans.44.2617 ↗
45. Strength, grain refinement and solute nanostructures of an Al-Mg-Si alloy (AA6060) processed by high-pressure torsion10.1016/j.actamat.2013.10.022 ↗
46. Microstructural variation due to heat gradient of a thick friction stir welded aluminum 7449 alloy10.1016/j.jallcom.2017.04.147 ↗
47. Impact of pore defects on laser additive manufacturing of Inconel 718 alloy based on a novel finite element model: thermal and stress evaluation10.1016/j.optlastec.2023.109782 ↗
48. A comparative study of machine learning in predicting the mechanical properties of the deposited AA6061 alloys via additive friction stir deposition
49. Quantitative study on the correlation between microstructure and mechanical properties of additive friction stir deposited 6061-T6 Al-Mg-Si alloy10.1016/j.jmrt.2023.07.097 ↗
50. Study of microstructure evolution and mechanical properties in friction stir based additive multi-layer manufacturing of Al 6061 alloy: effect of feedstock material form and heat treatment
51. Gradient process parameter optimization in additive friction stir deposition of aluminum alloys
52. Modelling and visualisation of material flow in friction stir spot welding10.1016/j.jmatprotec.2015.06.021 ↗
53. Effects of aging treatment and heat input on the microstructures and mechanical properties of TIG-welded 6061-T6 alloy joints10.1007/s12613-013-0721-8 ↗
54. The impact of heat input on the microstructures, fatigue behaviors, and stress lives of TIG-welded 6061-T6 alloy joints10.1088/2053-1591/abd136 ↗
55. Microstructure and strengthening mechanisms in an ultrafine grained Al-Mg-Sc alloy produced by powder metallurgy10.1007/s11661-014-2569-6 ↗
56. Strengthening mechanisms of an Al-Mg-Sc-Zr alloy10.1016/S1359-6454(02)00258-6 ↗
57. Behavioral simulations and experimental evaluations of stress induced spatial nonuniformity of dynamic bulk modulus in additive friction stir deposited AA 606110.1016/j.jmapro.2023.03.080 ↗
58. Tensile properties of friction stir welds of AA 7020 aluminum alloy10.1007/s12666-014-0508-2 ↗