Effect of aging treatment on microstructure, mechanical properties and corrosion resistance of 2219 aluminium alloy laser welded joint
Source abstract
Abstract
As a common heat-treatable aluminium alloys, AA2219 welded components are often applied in aerospace and rail transportation fields. However, the service performance like mechanical properties and corrosion resistance of this alloy are difficult to achieve a synergistic improvement after heat treatment. In this paper, different artificial aging processes were treated to establish the relationships between the microstructure, mechanical properties and corrosion resistance of the welded joints. The hardness of the joints increased first and then decreased with the increase of aging time. The tensile strength of aging treated joint increased by 46.4 % compared with the as-welded condition due to the dispersed distribution of fine precipitates. Meanwhile, the decreased potential difference between the Al–Cu precipitates, matrix, and precipitate-free zone enhances the corrosion resistance of the welded joint. Aging at 175 °C for 12 h produced the highest charge-transfer resistance (27564 ± 2776 Ω cm 2 ), a 59.2 % increase over the as-welded condition (17310 ± 609 Ω cm 2 ), indicating superior corrosion resistance of the welded joint. The corresponding research results have laid a foundation for the long-term service of aluminium alloy welded structures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (72)
Show source-provided references
1. Long-term stress relaxation behaviors and mechanisms of 2219 Al–Cu alloy under various temperatures and initial stresses10.1016/j.jmst.2023.06.061 ↗
2. Microstructure and localized corrosion properties of 2219 aluminum alloy manufactured by additive friction stir deposition10.1016/j.corsci.2024.112508 ↗
3. Achievement of high-strength 2219 aluminum alloy joint in a broad process window by ultrasonic enhanced friction stir welding10.1016/j.msea.2020.140587 ↗
4. Heat transfer and melt flow of keyhole, transition and conduction modes in laser beam oscillating welding10.1016/j.ijheatmasstransfer.2022.123821 ↗
5. A methodology to evaluate the reliability impact of the replacement of welded components by additive manufacturing spare parts10.3390/met9090932 ↗
6. Inspection scheduling based on reliability updating of gas turbine welded structures10.1177/1687814018819285 ↗
7. Defect formation, microstructure evolution, and mechanical properties of bobbin tool friction–stir welded 2219-T8 alloy10.1016/j.msea.2021.142414 ↗
8. Effect of ultrasonic impact treatment on microstructure and corrosion behavior of friction stir welding joints of 2219 aluminum alloy10.1016/j.jmrt.2022.03.068 ↗
9. Laser beam oscillating welding of 5A06 aluminum alloys: microstructure, porosity and mechanical properties10.1016/j.optlastec.2018.09.036 ↗
10. Sinusoidal oscillating laser welding of 7075 aluminum alloy: hydrodynamics, porosity formation and optimization10.1016/j.ijheatmasstransfer.2019.05.111 ↗
11. A study on laser beam oscillating welding characteristics for the 5083 aluminum alloy: morphology, microstructure and mechanical properties10.1016/j.jmapro.2020.01.018 ↗
12. Strengthening mechanism in laser-welded 2219 aluminium alloy under the cooperative effects of aging treatment and pulsed electromagnetic loadings10.1016/j.msea.2017.12.081 ↗
13. Segregation in fusion weld of 2219 aluminum alloy and its influence on mechanical properties of weld10.1016/S1003-6326(17)60030-X ↗
14. High-power laser welding of thick steel-aluminum dissimilar joints10.1016/j.phpro.2016.08.041 ↗
15. Effect of post-heat treatment on microstructure and mechanical properties of laser welded al-cu-mg alloy10.1016/j.jmapro.2021.02.008 ↗
16. Welding of 2000 series aluminium alloy materials10.1080/09507116.2011.590669 ↗
17. Atomic-scale mechanism of the θ″ → θ′ phase transformation in Al-Cu alloys10.1016/j.jmst.2016.08.031 ↗
18. Investigation of microstructure evolution after post-weld heat treatment and cryogenic fracture toughness of the weld metal of AA2219 VPTIG joints10.1016/j.matdes.2016.10.010 ↗
19. Effect of post weld heat treatment on properties of variable polarity TIG welded AA2219 aluminium alloy joints10.1016/S1003-6326(14)63193-9 ↗
20. Effect of post weld heat treatment on the microstructure and corrosion behavior of AA2219 aluminum alloy joints welded by variable polarity tungsten inert gas welding10.1016/j.matdes.2014.10.056 ↗
21. Effect of post-processing heat treatment on microstructure and microhardness of water-submerged friction stir processed 2219-T6 aluminum alloy10.1016/j.matdes.2012.11.056 ↗
22. Effect of two-step aging on the mechanical properties of AA2219 DC cast alloy10.1016/j.msea.2014.12.002 ↗
23. Effect of heat treatment on microstructure and corrosion behavior of Al-Cu alloy fabricated by wire arc additive manufacturing10.1016/j.matchar.2024.114516 ↗
24. Inhibiting of softening behavior in AA2219 laser welded joints10.1016/j.msea.2024.147742 ↗
25. Simultaneous refinement in θ’ precipitation and corrosion behavior of a 2xxx series Al–Cu alloys modified via the sole or joint addition of Cr, Mn and Zr
26. Simultaneous improvement in corrosion resistance and hardness of a model 2xxx series Al-Cu alloy with the microstructural variation caused by Sc and Zr additions10.1016/j.corsci.2019.108095 ↗
27. Mechanical properties, corrosion and microstructure distribution of a 2195-T8 Al-Li alloy TIG welded joint10.1016/j.jmapro.2023.02.007 ↗
28. Simulation study on function mechanism of some precipitates in localized corrosion of Al alloys10.1016/j.corsci.2006.12.002 ↗
29. Effect of Mn content on the microstructure and corrosion resistance of al-cu-mg-mn alloys10.1016/j.jallcom.2021.162903 ↗
30. Effects of aging treatment on the intergranular corrosion behavior of al–cu–mg–ag alloy10.1016/j.jallcom.2015.03.174 ↗
31. Effect of aging treatment on the exfoliation corrosion and stress corrosion cracking behaviors of 2195 Al–Li alloy10.1016/j.matdes.2014.11.007 ↗
32. Investigation of grain boundary segregation evolution and corrosion behavior in 7050 aluminum alloy under oscillating laser melting10.1016/j.jallcom.2024.177524 ↗
33. The influence of precipitation on plastic deformation of al–cu–li alloys10.1016/j.actamat.2013.03.015 ↗
34. Investigation of quench sensitivity of high strength 2219 aluminum alloy by TTP and TTT diagrams10.1016/j.jallcom.2016.08.160 ↗
35. Microstructural evolution and mechanical properties of 2219 aluminum alloy from different aging treatments to subsequent electromagnetic forming10.1016/j.matchar.2021.111470 ↗
36. Investigation on laser beam remelted al–cu–li alloy part I: segregation and aging behavior at grain and dendrite boundaries10.1016/j.jallcom.2020.157519 ↗
37. Evaluating the feasibility of using crystalline patterns induced by PBF-LB to predict strength enhancing orientations10.1016/j.matdes.2025.114006 ↗
38. Deformation structures and strengthening mechanisms in an Al-Cu alloy subjected to extensive cold rolling10.1016/j.msea.2017.07.001 ↗
39. Localized corrosion induced surface modifications of al-cu-li alloy studied by ToF-SIMS 3D imaging10.1038/s41529-021-00170-9 ↗
40. Strengthening mechanism of 2219 Al-Cu alloy by room-temperature random vibration
41. Influence of pre-deformation and subsequent aging on the hardening behavior and microstructure of 2219 aluminum alloy forgings10.1016/j.jallcom.2016.06.111 ↗
42. Precipitation behaviors and the related strengthening mechanism in 2219 Al alloy fabricated by wire arc additive manufacturing10.1016/j.jallcom.2024.175243 ↗
43. Evolution of microstructure and properties in 2219 aluminum alloy produced by wire arc additive manufacturing assisted by interlayer friction stir processing10.1016/j.msea.2023.144794 ↗
44. Enhancing the properties of 2219 aluminum alloy deposited by resistance seam additive manufacturing through rolling and heat treatment: microstructure evolution and strengthening mechanism10.1016/j.msea.2025.148253 ↗
45. Effects of Ce content and friction stir processing on the microstructure and mechanical properties of 2219 Al alloy10.1016/j.jmrt.2025.08.103 ↗
46. Mechanism for enhanced strengthening due to pre-stretching of 2219 aluminum alloy10.1016/j.msea.2025.148997 ↗
47. Changes in microstructure and mechanical properties of 2219 Al alloy during hot extrusion and post-extrusion aging10.1016/j.jmrt.2023.04.010 ↗
48. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an al–cu–li alloy10.1016/j.msea.2014.03.024 ↗
49. Effect of grain boundary precipitation on corrosion behaviour of nonisothermally aged al-zn-mg-cu alloys
50. Effects of heat treatment on the microstructure and mechanical properties of extruded 2196 al-cu-li alloy10.1016/j.matdes.2020.108746 ↗
51. Intergranular corrosion of an al-cu-li alloy: the influence from grain structure10.1016/j.corsci.2022.110845 ↗
52. Comparative study on corrosion property of 2219 aluminum alloy sheet and additively manufactured 2319 aluminum alloy10.1016/j.jmrt.2024.04.036 ↗
53. The intergranular corrosion susceptibility of 2024 Al alloy during Re–Aging after solution treating and cold–rolling10.1016/j.corsci.2016.11.013 ↗
54. Laser melting deposition of in-situ (TiB+TiC) hybrid reinforced TC4 composites: preparation, microstructure and room/high-temperature corrosion behaviour10.1016/j.jmst.2024.11.080 ↗
55. Investigation on the passive behavior of Ti-9Mn alloy in 3.5 wt% NaCl solution10.1149/1945-7111/ad4a0a ↗
56. Effect of preferential growth of Shewanella oneidensis MR-1 on microbial corrosion of constituent phases of 2205 duplex stainless steel
57. Effects of aging treatment on the mechanical properties and corrosion resistance of an al-cu-mg-li alloy
58. High strength al-cu-li alloy with enhanced atmospheric corrosion resistance developed by cold rolling tailored precipitation10.1016/j.jmrt.2025.04.187 ↗
59. Second phase particles and mechanical properties of 2219 aluminium alloys processed by an improved ring manufacturing process10.1016/j.msea.2020.139226 ↗
60. Sequence of steps in the pitting of aluminum by chloride ions10.1016/S0010-938X(02)00231-7 ↗
61. Corrosion and fatigue behavior of a stress-aged 2195 al-cu-li alloy10.1016/j.engfailanal.2025.109418 ↗
62. A study on corrosion behavior of friction stir welded and tungsten inert gas welded AA2014 aluminium alloy10.1016/j.corsci.2018.01.012 ↗
63. Effects of pre-deformation on the microstructures and corrosion behavior of 2219 aluminum alloys10.1016/j.msea.2018.03.041 ↗
64. Insight on corrosion behavior of friction stir welded AA2219/AA2195 joints in astronautical engineering10.1016/j.corsci.2021.109800 ↗
65. Microstructure and pitting corrosion of friction stir welded joints in 2219-O aluminum alloy thick plate10.1016/j.corsci.2009.07.004 ↗
66. Investigation of the de-alloying behaviour of θ-phase (Al2Cu) in AA2024-T351 aluminium alloy10.1016/j.corsci.2016.03.003 ↗
67. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
68. Effect of heat treatment on the microstructure and corrosion performance of 2219 Al alloy cold sprayed coatings10.1016/j.corsci.2024.112526 ↗
69. Rapidly modifying microstructure via electro pulsing treatment for AA2219 laser welded joints: synergistic enhancement of strength, ductility, and corrosion resistance10.1016/j.jmapro.2024.10.045 ↗
70. Quasi-continuous-wave laser surface melting of aluminium alloy: precipitate morphology, solute segregation and corrosion resistance10.1016/j.corsci.2019.01.035 ↗
71. Effects of non-isothermal aging on mechanical properties, corrosion behavior and microstructures of al-cu-mg-si alloy10.1016/j.jallcom.2019.152960 ↗
72. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗