journal article·2024-03Open access

Microstructure evolution and fracture behavior of laser welded-brazed titanium/aluminum joints with various gap sizes

Zilin Chen, Chuang Cai, Jie Yu, Jiasen Huang, Hui Chen, Liqun Li

Abstract

In the study, the effects of gap sizes on interfacial reaction and mechanical property were investigated for laser welding-brazing of titanium alloy and aluminum alloy. The wetting width on the joint rear surface was initially increased and then decreased with the increase of gap size. A layer of Ti(Al, Si)3 with uniform thickness was primarily formed in the 0.7 mm-joint and the nanophases Ti5Si3 and Ti7Al5Si12 were dispersed in the IMC layer. The inhomogeneous sandwich structure with a continuous Ti5Si3 strip layer was detected at the Ti/Al interface of the 0.4 mm-joint. The maximum line load of the joint with 0.7 mm gap size was about 395.4 N/mm, which was 261.9 % larger than that with 0 mm gap size. The cracks preferentially initiated at Ti5Si3/Ti(Al, Si)3 interface due to their higher interplanar spacing misfit rate and then propagated inside Ti5Si3 and Ti(Al, Si)3. When the gap size was 0.7 mm, the chemical potential gradient of Si decreased by the higher peak temperature at the bottom of the joint. The continuous Ti5Si3 strip layer was inhibited because Si atoms were more evenly distributed at the Ti/Al interface. Moreover, the IMC layer of Ti(Al, Si)3 was uniform and continuous. Thus, the mechanical property was significantly enhanced.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Lightweight hybrid materials and structures for energy absorption: a state-of-the-art review and outlook10.1016/j.tws.2021.108760 ↗
2. Review on design and structural optimisation in additive manufacturing: towards next-generation lightweight structures10.1016/j.matdes.2019.108164 ↗
3. Effect of hot dip aluminising on interfacial microstructure and mechanical properties of Ti/Al joint by TIG arc welding brazing10.1179/1362171814Y.0000000267 ↗
4. Deformation and fracture of explosion-welded Ti/Al plates: a synchrotron-based study10.1016/j.msea.2016.07.125 ↗
5. Advanced titanium materials processed from titanium hydride powder10.1016/j.powtec.2023.118504 ↗
6. In-situ formed graded microporous structure in titanium alloys and its effect on the mechanical properties10.1016/j.matdes.2015.06.066 ↗
7. Microstructure and mechanical characterization of remelted Ti-6Al-4V and Al-Mg-Si alloys butt weld10.1016/j.vacuum.2018.04.048 ↗
8. Microstructure evolution and fracture behavior of rotating laser welded-brazed 6061 aluminum alloys/304 SS dissimilar joint10.1016/j.matchar.2022.112543 ↗
9. Influence of energy ratio on dual–spot laser welded–brazed Al/steel butt joint10.1016/j.jmatprotec.2020.116624 ↗
10. Effect of the aluminum alloy composition (Al-Cu-Li or Al-Mg-Li) on structure and mechanical properties of dissimilar laser welds with the Ti-Al-V alloy
11. Microstructure and mechanical properties of TC4/6061 and TC4/2024 dissimilar joints by autogenous laser welding-brazing10.1016/j.optlastec.2022.107867 ↗
12. Influence of Si content on interfacial reactions and mechanical properties of dual-spot laser welded-brazed Ti/Al joints10.1016/j.jmapro.2020.06.001 ↗
13. Effects of laser pulse modulation on intermetallic compounds formation for welding of Ti-6Al-4V and AA7075 using AA4047 filler
14. Microstructure and mechanical properties of laser welded-brazed titanium/aluminum joints assisted by titanium mesh interlayer10.1016/j.jmatprotec.2022.117502 ↗
15. Effect of Ag alloying on the microstructure and mechanical properties of laser welded-brazed Ti/Al dissimilar joints
16. Microstructure and tensile properties of Ti/Al dissimilar joint by laser welding-brazing at subatmospheric pressure10.1016/j.jmapro.2020.04.062 ↗
17. Improving intermetallic compounds inhomogeneity of Ti/Al butt joints by dual laser-beam bilateral synchronous welding-brazing
18. Use of welding-brazing technology on microstructural development of titanium/aluminum dissimilar joints10.1080/10426914.2014.921711 ↗
19. Effect of groove shape on laser welding-brazing Al to steel10.1016/j.jmatprotec.2017.10.025 ↗
20. Aluminum to titanium laser welding-brazing in V-shaped groove10.1016/j.jmatprotec.2017.02.009 ↗
21. Effect of oscillating laser beam on the interface and mechanical properties of Ti/Al fusion welding joint10.1016/j.jmrt.2022.05.162 ↗
22. Laser welding of TC4 titanium alloy to 7075 aluminum alloy with infinite-shape oscillating beam
23. Welding characteristics and mechanical property of rotating laser welding-brazing of aluminum alloy to steel10.1016/j.optlastec.2022.107989 ↗
24. Laser welding-brazing under temporal and spatial power modulation for dissimilar materials AA6061 to Ti6Al4V joints10.1016/j.mfglet.2021.07.004 ↗
25. Effect of laser-arc offset and laser-deviation angle on the control of a Ti-Al interlayer10.1016/j.jmatprotec.2019.04.010 ↗
26. Thermodynamic prediction of interface phases at Cu/solder joints10.1007/s11664-998-0065-8 ↗
27. Cohesion in alloys-foundmentals of a semiempirical model10.1016/0378-4363(80)90054-6 ↗
28. Relationship between enthalpy of mixing and excess entropy in liquid binary alloys10.1515/ijmr-1990-810107 ↗
29. Relation between the elastic moduli and the plastic properties of polycrystalline pure metals10.1080/14786440808520496 ↗
30. First-principles calculations to investigate elastic properties, ideal tensile strength and electronic properties of TiSi, Ti5Si3 and Ti5Si410.1016/j.cplett.2022.139992 ↗
31. Plastic deformation of single crystals of Ti5Si3 with the hexagonal D88 structure10.1016/j.actamat.2009.09.062 ↗
32. First-principle calculation on the structural, elastic and thermodynamic properties of Ti-Al intermetallics10.1088/2053-1591/ab3e11 ↗
33. Charting the complete elastic properties of inorganic crystalline compounds
34. First-principles calculations of binary Al compounds: enthalpies of formation and elastic properties10.1016/j.calphad.2011.09.009 ↗
35. Simmons · 1971
36. Enthalpy of formation of Al–Fe–Si alloys II (τ6, τ2, τ3, τ8, τ4)10.1016/S0925-8388(00)00682-4 ↗
37. Grain refinement of commercially pure aluminum with addition of Ti and Zr elements based on crystallography orientation
38. Effect of pulsed laser pretreatment induced pit-structure on the formation of intermetallic compounds in titanium-aluminum dissimilar welded joints10.1016/j.optlastec.2023.109589 ↗