journal article·2022-11Open access

Effect of pre-aging on creep aging properties and microstructure evolution of 2195 Al–Li alloy

Fei Chen, Jue Zhong, Lihua Zhan, Peng Wang, Xiaopeng Ruan, Huiqiang Wu, Yongqian Xu, Bolin Ma, Chunhui Liu, Quanqing Zeng, Zhenggen Hu, Wenli Zhu

Abstract

Creep aging forming (CAF) is a potential process to manufacture large integral components of Al–Li alloys, which exhibits poor formability and susceptibility to damage and cracking via traditional plastic forming processes. Al–Li alloys also have disadvantages, such as low creep and comprehensive properties. To address this problem, this study adopted pre-aging as a treatment process before creep aging (CA). The effects of pre-aging at different temperatures (65 °C, 90 °C, and 115 °C) on the CA of Al–Li alloys were evaluated at 155 °C for 18 h. Creep strain, the evolution of mechanical properties, and the microstructural characteristics were investigated as well. The results showed that pre-aging could effectively influence the subsequent CA behavior. As the pre-aging temperature increased, creep strain accumulation during CA decreased. Meanwhile, pre-aging significantly increased the elongation (EL) of the specimens after CA; Notably, the increase in EL did not compromise strength. Changes in the microstructure of the specimens after pre-aging and CA tests were observed by transmission electron microscopy. The effect of pre-aging on the subsequent CA properties mainly revealed that the strength was not lower than that of the specimen without pre-aging after the same CA test through adjusting the percentage and size of the T 1 and θ′ phases. In addition, pre-aging could promote the transformation of the fracture mechanism from intergranular fracture to mixed fracture in the specimen after CA.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Coincidence Doppler broadening and 3DAP study of the pre-precipitation stage of an Al–Li–Cu–Mg–Ag alloy10.1016/j.actamat.2003.12.043 ↗
2. Development and characterization of Al–Li alloys10.1016/j.msea.2006.01.045 ↗
3. Multiple precipitation reactions and formation of θ’-phase in a pre-deformed Al–Cu alloy10.1016/j.msea.2018.07.039 ↗
4. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
5. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al–Cu–Li alloy10.1016/j.msea.2014.03.024 ↗
6. Atomic structure of T1precipitates in Al–Li–Cu alloys revisited with HAADF-STEM imaging and small-angle X-ray scattering10.1016/j.actamat.2010.09.044 ↗
7. Effects of coarse Al2CuLi phase on the hot deformation behavior of Al-Li alloy10.1016/j.jallcom.2019.152469 ↗
8. The effect of thermo-mechanical treatment on the formation of T1 phase and δ′/θ′/δ′composite precipitate in an Al-Cu-Li-Mg alloy10.1016/j.matchar.2021.111123 ↗
9. Size distribution and coarsening kinetics of δ′ precipitates in Al–Li alloys considering temperature and concentration dependence10.1016/S0921-5093(03)00640-3 ↗
10. Pre-strain-dependent natural ageing and its effect on subsequent artificial ageing of an Al-Cu-Li alloy10.1016/j.jallcom.2019.03.072 ↗
11. Anisotropic yielding stress of 2198 Al–Li alloy sheet and mechanisms
12. Effect of ageing treatments on the precipitation behavior and mechanical properties of Al–Cu–Li alloys10.1016/j.msea.2019.138885 ↗
13. Microstructure evolution of 2195 Al–Li alloy subjected to high-strain-rate deformation10.1016/j.msea.2014.03.118 ↗
14. Evolution of aging precipitates in an Al–Li alloy with 1.5 wt% Li concentration10.1016/j.vacuum.2020.109677 ↗
15. Constitutive behavior and microstructural evolution in hot deformed 2297 Al-Li alloy
16. Constitutive modeling and microstructure characterization of 2196 Al-Li alloy in various hot deformation conditions10.1016/j.jmapro.2020.09.063 ↗
17. An integrated process for modelling of precipitation hardening and springback in creep age-forming10.1016/j.ijmachtools.2006.01.026 ↗
18. A review of the development of creep age forming: experimentation, modelling and applications10.1016/j.ijmachtools.2010.08.007 ↗
19. Effect of age-forming on microstructure, mechanical and corrosion properties of a novel Al–Li alloy10.1016/j.jallcom.2015.03.212 ↗
20. Effects of uniaxial creep ageing on the mechanical properties and micro precipitates of Al-Li-S4 alloy10.1016/j.msea.2017.01.081 ↗
21. Effects of creep aging upon Al-Cu-Li alloy: strength, toughness and microstructure10.1016/j.jallcom.2018.06.103 ↗
22. Regulating effect of pre-stretching degree on the creep aging process of Al-Cu-Li alloy10.1016/j.msea.2019.138157 ↗
23. The effects of pre-deformation on the creep aging behavior and mechanical properties of Al-Li-S4 alloys10.1016/j.msea.2017.07.068 ↗
24. Role of thermal-mechanical loading sequence on creep aging behaviors of 5A90 Al-Li alloy10.1016/j.jmatprotec.2017.12.028 ↗
25. Creep aging properties variation and microstructure evolution for 2195 Al–Li alloys with various loading rates10.1016/j.msea.2021.142055 ↗
26. Creep-aging behaviors of Al-Cu-Li alloy with different grain sizes10.1016/j.jallcom.2022.164992 ↗
27. Pre-strain-dependent creep ageing behavior of an Al-Cu alloy10.1016/j.matchar.2022.112225 ↗
28. Effects of large strain pre-deformation on creep age behavior and microstructural evolution of an Al-Cu-Li alloy10.1016/j.matlet.2022.132699 ↗
29. Investigation of stress effect on creep, precipitation and dislocation evolution of Al–Li alloy during creep age forming10.1016/j.msea.2022.142723 ↗
30. Regulating effect of pre-stretching degree on the creep aging process of Al-Cu-Li alloy10.1016/j.msea.2019.138157 ↗
31. Strong stress-level dependence of creep-ageing behavior in Al–Cu–Li alloy10.1016/j.msea.2020.140381 ↗
32. Improving creep age formability of an Al-Cu-Li alloy by electropulsing10.1016/j.jallcom.2021.159482 ↗
33. Transformation of fracture mode of an Al-Mg-Si-Cu alloy subject to aging treatment10.1016/j.msea.2018.08.028 ↗
34. Rapidly modifying microstructure and mechanical properties of AA7150 Al alloy processed with electropulsing treatment10.1016/j.jmst.2021.03.060 ↗
35. Effect of pre-ageing treatment on second nucleating of GPII zones and precipitation kinetics in an ultrafine grained 7075 aluminum alloy10.1016/j.matdes.2019.108402 ↗
36. Grain boundary fracture in Al–Li alloys10.1179/mst.1986.2.12.1205 ↗
37. Grain boundary precipitate free zones in Al-Li alloys10.1016/0001-6160(87)90253-7 ↗
38. Dislocation creep behavior in Mg–Al–Zn alloys10.1016/j.msea.2005.06.059 ↗
39. Micromechanical behavior of multilayered Ti/Nb composites processed by accumulative roll bonding: an in-situ synchrotron X-ray diffraction investigation10.1016/j.actamat.2020.116546 ↗
40. Dislocations and grain size in ball-milled iron powder10.1016/S0965-9773(96)00048-7 ↗
41. Quantitative description of the T1 formation kinetics in an Al–Cu–Li alloy using differential scanning calorimetry, small-angle X-ray scattering and transmission electron microscopy10.1080/14786435.2013.878047 ↗
42. Distribution and evolution of aging precipitates in Al−Cu−Li alloy with high Li concentration10.1016/S1003-6326(18)64910-6 ↗
43. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al-Li-Cu-X alloy10.1016/S1471-5317(00)00002-X ↗
44. Precipitation behavior of an Al–Cu–Li–X alloy and competing relationships among precipitates at different aging temperatures10.1016/j.msea.2021.141125 ↗
45. Transmission electron microscopy study of the evolution of precipitates in aged Al-Li-Cu alloys: the θ′ and T1 phases10.1016/S1359-6454(03)00253-2 ↗
46. Effect of stretching on the precipitation kinetics of an Al-2.0Li-2.8Cu-0.5Mg (-0.13Zr) alloy10.1007/BF02659485 ↗
47. Improvement of strength and ductility of Al−Cu−Li alloy through cryogenic rolling followed by aging10.1016/S1003-6326(17)60216-4 ↗
48. Quantitative analysis of the influences of pre-treatments on the microstructure evolution and mechanical properties during artificial ageing of an Al–Cu–Li–Mg–Ag alloy10.1016/j.msea.2020.139253 ↗
49. A process model for age hardening of aluminium alloys-II: application of the model10.1016/0956-7151(90)90292-O ↗
50. Enhanced strength and ductility in an Al–Cu–Li alloy via long-term ageing10.1016/j.msea.2021.141092 ↗
51. The influence of a precipitate-free zone on the mechanical properties of an Al-Mg-Zn alloy10.1016/0001-6160(68)90018-7 ↗
52. Quantitative correlation between strength, ductility and precipitate microstructures with PFZ in Al-Zn-Mg (-Ag, Cu) alloys10.4028/www.scientific.net/MSF.519-521.431 ↗
53. Effect of PFZ and grain boundary precipitate on mechanical properties and fracture morphologies in Al-Zn-Mg (Ag) alloys10.4028/www.scientific.net/MSF.638-642.297 ↗
54. Improvement of strength and ductility by controlling PFZ with microalloying elements in Al-Zn-Mg alloys10.4028/www.scientific.net/MSF.561-565.235 ↗
55. Simulation of PFZ on intergranular fracture based on XFEM and CPFEM10.1007/s11771-016-3309-4 ↗
56. Dynamic precipitation, segregation and strengthening of an Al-Zn-Mg-Cu alloy (AA7075) processed by high-pressure torsion10.1016/j.actamat.2018.09.060 ↗