Abstract
The wettability and reactivity of Al alloys and B4C are of vital importance in the production of B4C-reinforced Al-matrix composites. However, previous research has primarily focused on pure Al/B4C systems, with little focus on alloying elements. In this paper, we investigated the influence of Si, Ti and Cu as alloying elements on the wettability and interfacial reactivity of an Al/B4C system using improved sessile drop methods. The B4C substrate was not wetted by molten Al at 700−1000 °C, with initial contact angles higher than 100°. However, rapid spreading was observed in the initial stages due to the formation of Al3BC and Al4C3. Si had a noticeable effect on the interfacial wettability only at levels of 15 wt% or above, with the interfacial products changing from Al3BC and AlB2 to SiC-dominated phases. The addition of Ti to Al led to the formation of TiB2-dominated interfacial products, which replaced the Al3BC and AlB2 phases, with the spreading kinetics mainly controlled by interfacial reactions in the early stages and the diffusion of Ti from the bulk of the drop to the triple line in the later stages. The addition of Cu had a negligible effect on the wettability but slightly weakened the formation of AlB2 by promoting substrate dissolution.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Influence of length-scales on spatial distribution and interfacial characteristics of B4C in a nanostructured Al matrix10.1016/j.actamat.2015.01.062 ↗
2. Bioinspired nacre-like 2024Al/B4C composites with high damage tolerance10.1016/j.ceramint.2022.05.316 ↗
3. Effect of the B4C content on microstructure, microhardness, corrosion, and neutron shielding properties of Al–B4C composites10.1016/j.ceramint.2022.10.071 ↗
4. Effects of Zr element on the microstructure and mechanical properties of B4C/Al composites fabricated by melt stirring method10.1016/j.compositesb.2021.109156 ↗
5. Processing of boron carbide-aluminum composites10.1111/j.1151-2916.1989.tb06216.x ↗
6. Boron-carbide-aluminum and Boron-carbide-reactive metal cermets
7. Wetting of polycrystalline B4C by molten Al at 1173–1473 K10.1016/j.scriptamat.2009.02.024 ↗
8. The reactive wetting and incorporation of B4C particles into molten aluminium10.1016/S1359-6462(01)00658-3 ↗
9. Interface interaction and wetting behaviour in B4C/(Me-Ti) systems (Me=Cu, Ag, Sn and Au)10.1016/j.msea.2004.12.017 ↗
10. Roles of alloying elements in wetting of SiC by Al10.1016/j.jallcom.2019.01.138 ↗
11. Effect of Ti addition on the wettability of Al–B4C metal matrix composites10.3139/146.110655 ↗
12. Wetting of binary aluminum alloys in contact with Be, B4C, and Graphite10.1111/j.1151-2916.1969.tb11193.x ↗
13. Wettability of low weight borides by commercial aluminum alloys-A basis for metal matrix composite fabrication10.1002/adem.201600297 ↗
14. Reassessment of the binary aluminum-titanium phase diagram10.1361/154770306X109809 ↗
15. Progress in understanding and modeling reactive wetting of metals on ceramics10.1016/j.cossms.2006.04.004 ↗
16. Effects of heat treatment on phase contents and mechanical properties of infiltrated B4C/2024Al composites10.1016/S1003-6326(14)63357-4 ↗
17. Influences of Si and Ti on the wettability and reactivity of Al/graphite system at 900 °C10.1016/j.mtla.2021.101060 ↗
18. Chemical reactivity of aluminium with boron carbide10.1023/A:1018625402103 ↗
19. Wettability of molten aluminum-silicon alloys on graphite and surface tension of those alloys at 1273K (1000°C)10.1007/s11661-016-3460-4 ↗
20. Chemical reaction-limited spreading: the triple line velocity versus contact angle relation10.1016/S1359-6454(02)00309-9 ↗
21. Wetting of polycrystalline SiC by molten Al and Al−Si alloys10.1016/j.apsusc.2014.08.055 ↗
22. B4C/Al composites processed by metal-assisted pressureless infiltration technique and its characterization10.1080/10426914.2016.1140192 ↗
23. Barin · 1955
24. Kinetics of diffusion-limited spreading of sessile drops in reactive wetting10.1016/S1359-6462(96)00431-9 ↗
25. High-temperature wetting and interfacial interaction between liquid Al and TiB2 ceramic10.1007/s10853-015-8814-6 ↗
26. Massalski · 1990
27. Interface reaction in the B4C/(Cu–Si) system10.1016/j.actamat.2004.02.010 ↗
28. Ceramic–metal interaction and wetting phenomena in the B4C/Cu system10.1016/S0955-2219(03)00294-2 ↗
29. Wetting and interface interactions in the B4C/Al–Me (Me=Cu, Sn) systems10.1016/j.msea.2007.04.002 ↗
30. The role of compound formation in reactive wetting: the Cu/SiC system10.1016/S1359-6454(00)00235-4 ↗