journal article·2024-03Open access

Microstructure and mechanical properties of high-temperature free-oxygen rolled Cu/1060Al bimetallic composite materials

Zhida Jiang, Haowen Zhu, Jiawei Sun, Yuchuan Huang, Guohua Wu, Zhengping Shang, Wencai Liu

Abstract

In this work, Cu/1060Al bimetallic composite materials manufactured by high-temperature free-oxygen rolling process are reported. The results show that with the increase of rolling passes, the microstructure of Cu and 1060Al gradually extends and elongates in the rolling direction, and the interface that has few compounds is dominated by mechanical bonding. It is worth noting that layered fracture occurs during the tensile process. After annealing, the interface changes from mechanical bonding to metallurgical bonding, and the layered fracture is alleviated under the traction of the interface layer. With the increase of annealing time and temperature, the thickness of the interface compounds gradually increase, and the interface compounds from the copper layer to the aluminum layer are Cu9Al4, CuAl and CuAl2, respectively. Annealing at 350 °C for 2 h exhibits the best comprehensive performance, a tensile strength of 138 MPa and an elongation of 64 %. Tensile behavior in the rolled state and annealed state has been discussed based on failure theory, and compound growth after annealing has been analyzed on account of the theories of dynamics and thermodynamics.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Deformation behavior of multilayered Al-Cu clad composite during cold-swaging10.1016/j.matdes.2015.10.145 ↗
2. Regulation of precipitation behavior among T1, S', and θ' phases in Al-Cu-Li-(Mg-Ag) alloys by optimizing Ag/Mg ratios10.1016/j.msea.2023.145158 ↗
3. Selection of explosive welding parameters of cooper-aluminum bimetal
4. Research and development of explosive welding of dissimilar metals
5. Study on microstructure and properties of ultra-thin Cu/Al composite sheets using the cold-rolled composite method at the microscale10.3390/met13040780 ↗
6. Gradient alternating deformation mechanism of two metals and interface bonding mechanism of cu/Al cold rolling composite process10.1016/j.matchar.2023.112989 ↗
7. Deformation behavior and bonding properties of Cu/Al laminated composite plate by corrugated cold roll bonding10.1016/j.jmrt.2022.12.135 ↗
8. Study on microstructure evolution and fracture behavior of Al/Al/Cu multilayer composites10.1016/j.jmrt.2023.07.014 ↗
9. Formation mechanism of dynamic multi-neutral points and cross shear zones in corrugated rolling of Cu/Al laminated composite10.1016/j.jmatprotec.2021.117157 ↗
10. Study on the phase structure of the interface zone of Cu-Al composite plate in cast-rolling state and different heat treatment temperatures based on EBSD10.1016/j.jmrt.2023.03.063 ↗
11. Microstructure and properties of Al/Cu bimetal in liquid–solid compound casting process10.1016/S1003-6326(16)64261-9 ↗
12. Interfacial microstructure and bonding strength of copper cladding aluminum rods fabricated by horizontal core-filling continuous casting10.1007/s11661-011-0785-x ↗
13. Microstructure and mechanical behaviors of Al/Cu laminated composites fabricated by accumulative roll bonding and intermediate annealing10.1016/j.msea.2021.142510 ↗
14. Effects of annealing temperature on interface microstructure and element diffusion of ultra-thin Cu/Al composite sheets10.1016/j.matlet.2022.132491 ↗
15. Interface strengthening of a roll-bonded two-ply Al/Cu sheet by short annealing10.1016/j.matchar.2021.111021 ↗
16. Rolling deformation behaviour and interface evaluation of Cu-Al bimetallic composite plates fabricated by horizontal continuous composite casting10.1016/j.jmatprotec.2021.117296 ↗
17. Characterization of intermetallic compounds in Cu-Al ball bonds: mechanical properties, interface delamination and thermal conductivity10.1016/j.microrel.2013.02.020 ↗
18. Effect of annealing on the interfacial structure of aluminum-copper joints10.2320/matertrans.MER2006371 ↗
19. Evaluation of interface structure and high-temperature tensile behavior in Cu/Al8011/Al5052 trilayered composite10.1016/j.msea.2020.140129 ↗
20. Characteristic investigation of trilayered Cu/Al8011/Al1060 composite: interface morphology, microstructure, and in-situ tensile deformation10.1016/j.pnsc.2021.08.005 ↗
21. Intermetallic compound growth and stress development in Al-Cu diffusion couple10.1007/s11664-017-5877-y ↗
22. Growth of intermetallic phases in Al/Cu composites at various annealing temperatures during the ARB Process10.1007/s12540-012-0001-6 ↗
23. Formation mechanism of dynamic multi-neutral points and cross shear zones in corrugated rolling of Cu/Al laminated composite
24. Formation and growth of Cu-Al IMCs and their effect on electrical property of electroplated Cu/Al laminar composites10.1016/S1003-6326(16)64462-X ↗
25. Tailoring of interface structure and mechanical properties in ARBed 1100/7075 laminated composites by cold rolling10.1016/j.msea.2019.03.075 ↗
26. A novel approach for preparing Cu/Al laminated composite based on corrugated roll10.1016/j.matlet.2018.09.060 ↗
27. The diffusion behaviors at the Cu-Al solid-liquid interface: a molecular dynamics study10.1016/j.rinp.2020.102998 ↗
28. Effect of annealing process on interface microstructure and mechanical property of the Cu/Al corrugated clad sheet10.1016/j.jmrt.2022.12.188 ↗
29. Achievement of high-strength Al/Cu dissimilar joint during submerged friction stir welding and its regulation mechanism of intermetallic compounds layer10.1016/j.msea.2022.144164 ↗
30. Study on diffusion behavior and microstructural evolution of Al/Cu bimetal interface by synchrotron X-ray radiography10.1016/j.jallcom.2014.07.172 ↗
31. Preparation, interfacial regulation and strengthening of Mg/Al bimetal fabricated by compound casting: a review10.1016/j.jma.2023.09.001 ↗
32. Interfacial bonding mechanism and annealing effect on Cu-Al joint produced by solid-liquid compound casting10.1016/j.jmatprotec.2017.10.050 ↗
33. Effect of the annealing process on the formation and growth of intermetallic compounds at the interface of Cu clad Al wire drawn with high area reduction10.1016/j.matlet.2022.133474 ↗
34. Influence of reduction ratio on the interface microstructure and mechanical properties of roll-bonded Al/Cu sheets10.1016/j.msea.2013.06.077 ↗
35. Development of Goss texture in Al–0.3%Cu annealed after heavy rolling10.1016/j.jallcom.2018.03.187 ↗
36. Effect of La on microstructure, mechanical properties and fracture behavior of Al/Mg bimetallic interface manufactured by compound casting10.1016/j.jmst.2021.08.011 ↗
37. Effect of La on microstructure, mechanical properties and fracture behavior of Al/Mg bimetallic interface manufactured by compound casting10.1016/j.jma.2023.09.001 ↗
38. Study on interface behavior and mechanical properties of Al/Cu laminated tubes fabricated by strong staggered spinning at room temperature10.1016/j.jmrt.2023.07.129 ↗
39. Comprehensive study of hot deformation behavior and fracture mechanism of Al/Cu laminated composite10.1016/j.jmapro.2023.04.071 ↗
40. Atomic-scale deformation mechanisms of nano-polycrystalline Cu/Al layered composites: a molecular dynamics simulation10.1016/j.jmrt.2023.03.067 ↗