journal article·2025-01Open access

Effect of WC on the microstructure and wear resistance of Invar-WC coatings prepared by laser fusion cladding

Yuheng Li, Qiyu Gao, Xiaohu Guan, Feixiang Tian, Binbin Li, Xiaohong Zhan

Abstract

Invar alloys are frequently utilized in the production of composite molds, owing to their excellent dimensional stability and closely matched coefficient of thermal expansion to that of the composite materials. The inherent wear resistance of Invar alloys is limited, which significantly impacts their overall service life. Therefore, in this study, Invar-WC coating and laser remelting coating were prepared on the surface of Invar alloy by laser cladding technology. The microstructures and phase compositions of the different coatings were analyzed, and the hardness and wear resistance of the two coatings were tested and observed in the wear micro-morphology. The results show that the two coatings are well formed. The main phase composition of Invar-WC coating is Fe 0.64 Ni 0.36 , and the reinforcing phases such as W 2 C、M 7 C 3 , were formed in the substrate under the effect of W and C elements. The wear resistance of the remelted coating was increased by 63.55% over the substrate, and the wear resistance of the Invar-WC coating was further increased by 97.69% over the substrate. The Invar-WC coating was strengthened by fine grain reinforcement and the second phase reinforcement under the action of WC particles, which led to the increase of the hardness of the Invar-WC coating, and the enhancement of the wear-resistant property. Meanwhile, the wear mechanism of the substrate and laser remelting is characterized by adhesive wear, while the wear mechanism of the Invar-WC coating is characterized by abrasive wear due to the presence of WC particles, resulting in a significant increase in wear resistance.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Thermal expansion coefficients in Invar processed by selective laser melting10.1007/s10853-017-1169-4 ↗
2. Origin of zero and negative thermal expansion in severely-deformed superelastic NiTi alloy10.1016/j.actamat.2016.10.054 ↗
3. Strengthening of the Fe-Ni invar alloy through chromium10.3390/ma12081297 ↗
4. Modeling and simulation of the columnar-to-equiaxed transition during laser melting deposition of Invar alloy10.1016/j.jallcom.2018.04.313 ↗
5. A study of thermal expansion coefficients and microstructure during selective laser melting of Invar 36 and stainless steel 316L
6. Additive manufacturing of Invar 36 alloy10.1016/j.jmrt.2024.02.221 ↗
7. Elastic constants of equiatomic Fe–Ni Invar alloy single crystal10.1063/5.0174535 ↗
8. Mechanical properties of Invar 36 alloy additively manufactured by selective laser melting10.1016/j.msea.2019.138799 ↗
9. Microstructure and mechanical properties' modification of friction stir welded Invar 36 alloy joint10.1080/13621718.2018.1490104 ↗
10. Multifunctional nanostructured NiTi alloy with invar, elinvar and rinvar properties10.1016/j.jallcom.2022.164682 ↗
11. Influence of addition of TiAl particles on microstructural and mechanical property development in Invar 36 processed by laser powder bed fusion
12. Microstructures and unique low thermal expansion of Invar 36 alloy fabricated by selective laser melting10.1016/j.matchar.2020.110409 ↗
13. Superior mechanical properties of Invar36 alloy lattices structures manufactured by laser powder bed fusion10.3390/ma16124433 ↗
14. Influence of geometric imperfections on the mechanical behavior for Invar 36 alloy lattice structures fabricated by selective laser melting10.1016/j.ijmecsci.2024.109252 ↗
15. Effects of Ce addition on mechanical properties and thermal expansion behavior of Fe-36Ni Invar alloy10.1016/j.matchar.2023.113584 ↗
16. Mechanical properties of Invar 36 alloy additively manufactured by selective laser melting10.1016/j.msea.2019.138799 ↗
17. Investigation of cryogenic friction and wear properties of Invar 36 alloy against Si3N4 ceramic balls
18. Effect of cold drawing on microstructure and properties of the invar alloy strengthened by carbide-forming elements10.1016/j.jmrt.2021.05.026 ↗
19. Heat treatment and microstructure of an FeNiCo Invar alloy strengthened by intermetallic precipitation10.1016/1044-5803(92)90103-O ↗
20. Phase evolution characteristics, thermal stability, and strengthening processes of Fe–Ni based ODS invar steel produced by mechanical alloying and spark plasma sintering10.1016/j.msea.2022.143972 ↗
21. Enhancing low thermal expansion behavior and strength via induced Zr-rich intermetallic phase in Fe-36Ni Invar alloy10.1016/j.matdes.2023.111644 ↗
22. Alloy modification for additive manufactured Ni alloy components—part I: effect on microstructure and hardness of Invar alloy10.1007/s40194-023-01510-w ↗
23. Deformation induced Elinvar behavior in Fe-Ni Invar alloy10.1016/j.scib.2018.07.006 ↗
24. Microstructure characteristics and mechanical properties of a laser cladded Fe-based martensitic stainless steel coating10.1016/j.surfcoat.2020.126795 ↗
25. Laser nano-technology of light materials: precision and opportunity10.1016/j.optlastec.2021.106988 ↗
26. Microstructure performance enhancement of Si 3 N 4 reinforced laser clad KF110 base composite coatings10.1111/ijac.13904 ↗
27. The immiscible W/Cu composites with heterostructures and excellent bond strength prepared by additively manufactured transient liquid-phase direct bonding: experiments and simulations10.1016/j.compositesb.2024.111981 ↗
28. Microstructure and properties analysis of Ni60-based/WC composite coatings prepared by laser cladding
29. Influence of WC ceramic particles on structures and properties of laser cladding Ni50-WC coatings10.1016/j.jmrt.2023.07.138 ↗
30. Friction and wear behavior of laser cladded WC-Co and Ni/WC-Co deposits at high temperature10.1016/j.ijrmhm.2019.02.025 ↗
31. Effect of WC content on microstructure and properties of high-speed laser cladding Ni-based coating10.1016/j.optlastec.2022.108449 ↗
32. Effect of WC on microstructure, molten pool and properties of Ni based coatings by multi-layer laser cladding10.1016/j.optlastec.2024.110612 ↗
33. Wear behavior of laser cladded WC-reinforced Ni-based coatings under low temperature10.1016/j.triboint.2022.107939 ↗
34. Effect of WC mass fraction on the microstructure and friction properties of WC/Ni60 laser cladding layer of brake discs10.1016/j.ceramint.2021.07.035 ↗
35. Shu · 2017
36. Shuai · 2015
37. Microstructure and element distribution characteristics of Y2O3 modulated WC reinforced coating on Invar alloys by laser cladding10.1016/j.optlastec.2022.108205 ↗
38. Sliding wear behavior of a Laves phase-strengthened CrFeNiNb0.158 alloy at room and elevated temperatures10.1016/j.wear.2024.205469 ↗
39. Process optimization, microstructure characterization, and tribological performance of Y2O3 modified Ti6Al4V-WC gradient coating produced by laser cladding10.1016/j.surfcoat.2024.130496 ↗