Influence of Ni, Al, W doping on microstructure, corrosion and wear resistance of HVOF spraying Fe-based amorphous alloy coatings
Source abstract
Abstract
A series of novel Fe-based amorphous alloy coatings (AACs) with outstanding corrosion and wear resistance, composed of Fe 57 Cr 15 Mo 4 P 10 C 7 B 3 M 4 (M = Fe, Ni, Al and W, in at. %) with various alloying elements, were fabricated using high-velocity oxygen fuel (HVOF) technique. The effect of Ni, Al, and W on microstructure, thermal behavior, corrosion resistance, and wear resistance of these fabricated Fe-based AACs were investigated systematically compared to 316L stainless steel (316L SS) substrates. Microstructural analysis revealed that the present Fe-based AACs exhibited a dense and uniform microstructure with high thermal stability. Electrochemical test results demonstrated that doping with Ni, Al and W significantly enhanced the corrosion resistance of the base alloy AAC. The W-doped AAC showed the best performance than Ni-doped, Al-doped and base alloy AAC, with a wide passive region (Δ E pass ) of 1.7 V, low self-corrosion current density ( I corr ) of 1.07 ×10 -6 A·cm -2 and the lowest steady-state current densities and highest passivation index. Mott–Schottky analysis and X-ray photoelectron spectroscopy results showed that the W-doped AACs forming the densest and thickest passivation films, ascribed to an increased fraction of protective and stable low-valent metal oxides (Fe 2+ /Cr 3+ /Mo 4+ ), enhanced corrosion resistance by promoting film growth and degradation processes. Dry wear tests revealed that among these Fe-based AACs, the W-doped AAC exhibited the superior wear resistance, with the lowest coefficient of friction (0.42) and wear rate (2.8×10 -5 mm 3 ·N -1 ·m -1 ), because of higher amorphous content and higher hardness. Under wear conditions, the primary wear mechanisms identified for the Fe-based AACs were abrasive, fatigue, and oxidative wear.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (91)
Show source-provided references
1. Manufacturing of metallic glass components: processes, structures and properties10.1016/j.pmatsci.2024.101283 ↗
2. Recent development and application products of bulk glassy alloys10.1016/j.actamat.2010.11.027 ↗
3. Publisher's Note: structural amorphous steels10.1103/PhysRevLett.93.049901 ↗
4. Fe-based bulk metallic glasses: glass formation, fabrication, properties and applications10.1016/j.pmatsci.2019.01.003 ↗
5. Metallic glasses as structural materials10.1016/j.scriptamat.2005.09.051 ↗
6. Structural homology of the strength for metallic glasses
7. Growth characteristics and reinforcing behavior of in-situ NbCp in laser cladded Fe-based composite coating
8. Electrodeposited Ni–Co–B alloy coatings: preparation and properties10.1149/2.1151410jes ↗
9. Effects of tungsten contents on the microstructure, mechanical and anticorrosion properties of Zr–W–Ti thin film metallic glasses10.1016/j.tsf.2015.01.063 ↗
10. Erosion–corrosion of HVOF-sprayed Fe-based amorphous metallic coating under impingement by a sand-containing NaCl solution10.1016/j.corsci.2013.07.006 ↗
11. Fabrication and characterization of Fe-based amorphous coatings prepared by high-velocity arc spraying10.1016/j.matdes.2015.04.027 ↗
12. Corrosion of high-velocity-oxygen-fuel (HVOF) sprayed non-crystalline alloy coating in marine environment10.1016/j.surfcoat.2021.126896 ↗
13. Microstructure and tribological properties of Zr-based amorphous-nanocrystalline coatings deposited on the surface of titanium alloys by Electrospark Deposition10.1016/j.apsusc.2015.08.233 ↗
14. Thermal spray maps: material genomics of processing technologies10.1007/s11666-013-9970-3 ↗
15. Recent advances and strategies for high-performance coatings10.1016/j.pmatsci.2023.101125 ↗
16. A critical review on thermal spray based manufacturing technologies
17. Enhancement of oxidation and wear resistance of Fe-based amorphous coatings by surface modification of feedstock powders10.1016/j.matdes.2015.02.015 ↗
18. Optimization of HVOF spraying parameters for enhanced Fe-based amorphous coatings: a taguchi approach10.1016/j.intermet.2024.108419 ↗
19. Effect of laser remelting on the microstructure and corrosion behavior of high-velocity arc-sprayed FeNiCrBSiNbW amorphous coating10.1016/j.jmrt.2024.02.173 ↗
20. Effects of crystallization on the corrosion resistance of Fe-based amorphous coatings10.1016/j.corsci.2012.02.003 ↗
21. Effect of heat treatment on the structure, cavitation erosion and erosion–corrosion behavior of Fe-based amorphous coatings10.1016/j.triboint.2015.04.039 ↗
22. Fe-based metallic glass coatings by thermal spraying: a focused review on corrosion properties and related degradation mechanisms10.1080/09506608.2022.2084670 ↗
23. Roles of minor additions in formation and properties of bulk metallic glasses10.1016/j.pmatsci.2006.07.003 ↗
24. Selection of a micro-alloying interface active component to stabilize the interface between droplets and liquid matrix in monotectic alloys10.1016/j.actamat.2023.118823 ↗
25. Corrosion behavior of the bulk glassy (Fe44.3Cr5Co5Mo12.8Mn11.2C15.8B5.9)98.5Y1.5 alloy
26. Phase separation and glass forming ability of (Fe0.72Mo0.04B0.24)100-xGdx (x = 4, 8) bulk metallic glasses10.1016/j.jnoncrysol.2016.06.003 ↗
27. Glass forming ability, magnetic and mechanical properties of (Fe72Mo4B24)100−xDyx (x=4–7) bulk metallic glasses10.1016/j.msea.2010.08.092 ↗
28. Magnetocaloric effect of Fe–RE–B–Nb (RE = Tb, Ho or Tm) bulk metallic glasses with high glass-forming ability10.1016/j.jallcom.2015.04.170 ↗
29. Structural amorphous steels10.1103/PhysRevLett.92.245503 ↗
30. Sliding wear behavior of Fe50−xCr15Mo14C15B6Erx (x=0, 1, 2at%) bulk metallic glass10.1016/j.wear.2012.06.007 ↗
31. Corrosion behavior of Fe-based ferromagnetic (Fe, Ni)–B–Si–Nb bulk glassy alloys in aqueous electrolytes10.1016/j.jnoncrysol.2008.06.009 ↗
32. Crystallization and corrosion resistance of (Fe0.78Si0.09B0.13)100-xNix (x=0, 2 and 5) glassy alloys
33. Strategy for preventing excessive wear rate at high loads in bulk metallic glass composites10.1016/j.matdes.2017.09.035 ↗
34. Effect of W on the thermal stability, mechanical properties and corrosion resistance of Fe-based bulk metallic glass10.1016/j.intermet.2022.107485 ↗
35. Effects of W Addition on the electrochemical behaviour and passive film properties of Fe-based amorphous alloys in acetic acid solution10.1007/s40195-018-0791-8 ↗
36. Effect of W addition on the glass forming ability and mechanical properties of Fe-based metallic glass10.1016/j.jallcom.2017.10.104 ↗
37. Unexpected accelerated corrosion of Cr in Ni-xW-6Cr alloy with W content increasing10.1016/j.corsci.2021.109761 ↗
38. Anodic behaviour of Fe73.5Si13.5-xAlxB9Nb3Cu1 (x = 0–2) amorphous, nanostructured and crystalline alloys10.1016/S1359-6462(00)00627-8 ↗
39. Effect of Al content on wear and corrosion resistance of Ni-based alloy coatings by laser cladding10.1016/j.surfcoat.2021.126976 ↗
40. Influence of Al addition on the microstructure and properties of Fe25Co25Ni25(Si0.3B0.7)25 high entropy metallic glass10.1016/j.intermet.2024.108304 ↗
41. Development of novel Fe-based bulk metallic glasses with excellent wear and corrosion resistance by adjusting the Cr and Mo contents10.1016/j.intermet.2022.107801 ↗
42. Temperature-dependent corrosion behaviour of the amorphous steel in simulated wet storage environment of spent nuclear fuels10.1016/j.corsci.2021.109529 ↗
43. Effects of peening duration on surface and wear properties of aircraft graded AA2017 alloy10.1016/j.surfcoat.2023.130361 ↗
44. Standard test method for wear testing with a pin-on-disk apparatus, United States patent US. G 99 – 04. PA19428-12959.
45. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
46. Phase stability in high entropy alloys: formation of solid-solution phase or amorphous phase10.1016/S1002-0071(12)60080-X ↗
47. Effects of alloying elements on glass formation, mechanical and soft-magnetic properties of Fe-based metallic glasses10.1016/j.intermet.2011.05.020 ↗
48. Review of relationship between particle deformation, coating microstructure, and properties in high-pressure cold spray10.1007/s11666-017-0575-0 ↗
49. Influence of the high-velocity oxygen-fuel spray parameters on the porosity and corrosion resistance of iron-based amorphous coatings10.1016/j.surfcoat.2019.03.046 ↗
50. Optimizing process and the properties of the sprayed Fe-based metallic glassy coating by plasma spraying10.1016/j.surfcoat.2017.03.063 ↗
51. Development of a FeCrMnBC-based economical wear and corrosion resistant coating10.1016/j.surfcoat.2019.01.074 ↗
52. Role of passive film in dominating the electrochemical corrosion behavior of FeCrMoCBY amorphous coating10.1016/j.jallcom.2019.151962 ↗
53. Fe-based metallic glass composite coatings by HVOF spraying: influence of Mo on phase evolution, wear and corrosion resistance10.1016/j.matchar.2022.112149 ↗
54. Effects of Cr and Mo additions on formation and mechanical properties of Arc-sprayed FeBSiNb-based glassy coatings10.1016/j.jnoncrysol.2018.07.035 ↗
55. Effect of amorphicity of HVOF sprayed Fe-based coatings on their corrosion performances and contacting osteoblast behavior10.1016/j.surfcoat.2016.12.092 ↗
56. Effect of porosity defects on the long-term corrosion behaviour of Fe-based amorphous alloy coated mild steel10.1016/j.corsci.2016.04.021 ↗
57. Long-term corrosion behavior of HVOF sprayed FeCrSiBMn amorphous/nanocrystalline coating10.1016/S1003-6326(15)63709-8 ↗
58. Preparation and characterization of highly amorphous HVOF stainless steel coatings10.1016/j.jallcom.2010.02.062 ↗
59. A study on the corrosion inhibition of Fe-based amorphous/nanocrystalline coating synthesized by high-velocity oxy-fuel spraying in an extreme environment10.1007/s11666-019-00907-8 ↗
60. Electrochemical behaviour of high nitrogen stainless steel in acidic solutions10.1016/j.corsci.2009.02.026 ↗
61. Thin anodic oxide layers on aluminium and other valve metals: high field regime10.1016/0927-796X(93)90005-N ↗
62. Temperature-dependent corrosion behaviour of the amorphous steel in simulated wet storage environment of spent nuclear fuels10.1016/j.corsci.2021.109529 ↗
63. Effects of electrolyte composition and applied potential on the repassivation kinetics of pure aluminium10.1016/0013-4686(95)94180-3 ↗
64. Effect of halide ion and applied potential on repassivation behaviour of Al-1 wt.%Si-0.5 wt.%Cu alloy10.1016/0013-4686(94)00309-O ↗
65. Passivity breakdown, its relation to pitting and stress-corrosion-cracking processes10.1016/0010-938X(90)90163-Y ↗
66. Investigation on the effect of shot peening coverage on the surface integrity10.1016/j.apsusc.2019.05.281 ↗
67. In situ EC-AFM study of the effect of nanocrystals on the passivation and pit initiation in an Al-based metallic glass10.1016/j.corsci.2014.02.005 ↗
68. Corrosion inhibition of carbon steel using novel N-(2-(2-mercaptoacetoxy)ethyl)-N,N-dimethyl dodecan-1-aminium bromide during acid pickling10.1016/j.corsci.2012.11.031 ↗
69. Long term semiconducting and passive film properties of a novel dense FeCrMoCBY amorphous coating by atmospheric plasma spraying10.1016/j.apsusc.2019.143600 ↗
70. Role of passive film in dominating the electrochemical corrosion behavior of FeCrMoCBY amorphous coating10.1016/j.jallcom.2019.151962 ↗
71. Diffusivity of point defects in the passive film on Fe10.1016/j.jelechem.2005.03.003 ↗
72. Synthesis and corrosion property of pure Ni with a high density of nanoscale twins10.1016/j.electacta.2008.03.070 ↗
73. Enhanced corrosion resistance in Fe-based amorphous coatings through eliminating Cr-depleted zones10.1016/j.corsci.2018.03.005 ↗
74. Influence of yttrium as a minority alloying element on the corrosion behavior in Fe-based bulk metallic glasses10.1016/j.electacta.2008.08.017 ↗
75. A bipolar model of the passivity of stainless steels—III. The mechanism of MoO42− formation and incorporation10.1016/0010-938X(89)90059-0 ↗
76. Electrochemical behaviour of Fe-based metallic glasses in acidic and neutral solutions10.1016/j.corsci.2012.05.025 ↗
77. A tensiostatic study of the anodic behaviour of tungsten in acid solutions10.1016/0022-5088(75)90051-X ↗
78. Formation of amorphous Fe-Cr-Mo-8P-2C coatings by the high velocity oxy-fuel process10.1007/BF02608552 ↗
79. Identifying the role of nanoscale heterogeneities in pitting behaviour of Al-based metallic glass10.1016/j.corsci.2011.05.047 ↗
80. A comparative study of primary and secondary passive films formed on AM355 stainless steel in 0.1 M NaOH10.1016/j.apsusc.2017.08.151 ↗
81. Corrosion behaviors and mechanisms of in-situ Ti-based MGMCs in chloride-containing and chloride-free solutions10.1016/j.intermet.2018.10.010 ↗
82. The history of the Point Defect Model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
83. Passive films on stainless steels—chemistry, structure and growth10.1016/S0013-4686(02)00841-1 ↗
84. Corrosion mechanism of Al, Al–Zn and Al–Zn–Sn alloys in 3 wt.% NaCl solution10.1016/j.corsci.2014.07.018 ↗
85. The effect of tungsten on the corrosion behavior of amorphous Fe‐Cr‐W‐P‐C alloys in 1M HCl10.1149/1.2085581 ↗
86. Strategy for improving the wear-resistance properties of detonation sprayed Fe-based amorphous coatings by cryogenic cycling treatment10.1016/j.surfcoat.2021.126962 ↗
87. Influence of Cold Gas Spray process conditions on the microstructure of Fe-based amorphous coatings10.1016/j.jallcom.2014.11.037 ↗
88. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
89. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
90. Differences in dry sliding wear behavior between HVAF-sprayed amorphous steel and crystalline stainless steel coatings
91. Friction and wear of aluminium–steel contacts lubricated with ordered fluids-neutral and ionic liquid crystals as oil additives10.1016/S0043-1648(03)00442-3 ↗