Abstract

The formation of titanium-iron compounds during the fusion welding of titanium steels continues to pose a significant challenge. In this paper, pure copper filler wire was employed in TIG welding to join TC4 titanium alloy and 304 stainless steel. The solidification behavior of the titanium-steel molten weld interface and the morphological distribution of the brittle phase were controlled by introducing a low-power ultrasonic energy field to assist the welding process. Results indicated that the low-power ultrasonic energy field enhanced the diffusion of joint elements, leading to biased aggregation of brittle phases on the titanium and steel sides, thereby reducing the joint's mechanical properties. The high-frequency vibration produced by the increased ultrasonic power resulted in a slower diffusion of the concentration gradient, creating a more homogeneous distribution of the Ti–Fe brittle phase in the Cu interlayer. This improved the joint properties and results in the middle of the weld consisting mainly of a discontinuous Ti–Fe phases. Additionally, the distribution of the Ti–Cu phase and α-(Fe,Cr) phase became more uniform. The high-frequency vibration effectively reduced the residual stresses in the titanium-steel joints, thereby enhancing the overall performance. The tensile strength of the joints reached up to 346 MPa, an increase of 12.7% compared to before ultrasonic vibration was added.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Advanced Welding Techniques Analysis · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Leyens
2. Titanium alloys and their machinability—a review10.1016/S0924-0136(96)00030-1 ↗
3. New application of stainless steel10.1016/S1006-706X(06)60028-9 ↗
4. Microstructure and mechanical properties of titanium/steel bimetallic joints10.1016/j.matchar.2017.08.025 ↗
5. Interfacial investigation of explosion-welded titanium/steel bimetallic plates10.1007/s11665-019-04535-9 ↗
6. Investigation of the solid-phase joint of VT-14 titanium alloy with 12KH18N10T stainless steel obtained by diffusion welding through intermediate layers10.3390/met11081325 ↗
7. Microstructure and shear property of high-temperature brazing of TiAl alloy and 316L stainless steel with a Ni-based amorphous filler10.3389/fmats.2022.1098397 ↗
8. Brazing TC4 titanium alloy/316L stainless steel joint with Ti50-xZrxCu39Ni11 amorphous filler metals10.1016/j.jallcom.2020.156650 ↗
9. Microstructural and mechanical heterogeneity of electron beam welded thick pure titanium/q235B steel bimetallic plate joint10.1007/s11665-022-07489-7 ↗
10. Butt brazing of titanium alloys/stainless steel plates by MIG-TIG double-sided arc welding process with copper filler metal10.1016/j.jmrt.2018.06.009 ↗
11. Joining of CP-Ti/Q345 sheets by Cu-based filler metal and effect on interface10.1016/j.jmatprotec.2015.05.017 ↗
12. The formation of intermetallics in dissimilar Ti6Al4V/copper/AISI 316 L electron beam and Nd:YAG laser joints10.1016/j.intermet.2011.05.016 ↗
13. Pulsed laser welding of Ti-6Al-4V titanium alloy to AISI 316L stainless steel using Cu/Nb bilayer10.1016/j.matlet.2019.02.075 ↗
14. Weld Formation mechanism and microstructural evolution of TC4/304 stainless steel joint with Cu-based filler wire and preheating10.3390/ma12193071 ↗
15. Three-pass laser welding of Ti alloy-stainless steel using Nb and Ni interlayers10.1016/j.jmrt.2019.12.009 ↗
16. Laser assisted diffusion bonding of TC4 titanium alloy to 301 stainless steel using a Ni interlayer10.1016/j.jmrt.2022.09.065 ↗
17. Dissimilar laser welding of AISI 316L stainless steel to Ti6–Al4–6V alloy via pure vanadium interlayer
18. Two pass laser welding of TC4 Titanium alloy to 301L stainless steel via pure V interlayer10.1016/j.jmrt.2019.11.066 ↗
19. Microstructures and mechanical properties of electron beam-welded titanium-steel joints with vanadium, nickel, copper and silver filler metals10.1007/s11665-014-0897-8 ↗
20. Improving the interfacial microstructure evolution of Ti/stainless steel GTA welding joint by employing Cu filler metal10.1080/10426914.2016.1151042 ↗
21. Dissimilar gas tungsten arc welding of TC4 titanium to 304 stainless steel using CuSi3 filler wire10.1007/s40194-022-01402-5 ↗
22. Nd:YAG pulsed laser welding of TC4 Ti alloy to 301L stainless steel using Ta/V/Fe composite interlayer10.1016/j.matlet.2017.10.057 ↗
23. Two pass laser welding of TC4 titanium alloy and 304 stainless steel using TA2/Q235 composite interlayer10.1016/j.matlet.2019.126521 ↗
24. Evaluation of welded joints of dissimilar titanium alloy Ti-5Al-2.5Sn and stainless-steel 304 at different multi-interlayer modes10.1088/2053-1591/ac9600 ↗
25. Interfacial microstructure evolution and mechanical properties of TC4 alloy-304 stainless steel joints with different joining modes10.1016/j.matlet.2019.126986 ↗
26. Feasibility study of different filler metals on MIG-TIG double-sided arc brazing of titanium alloy-stainless steel10.1016/j.jmapro.2019.09.029 ↗
27. Evolution of microstructure, mechanical properties and corrosion resistance of ultrasonic assisted welded-brazed Mg/Ti joint10.1016/j.jmst.2016.08.029 ↗
28. Joining mechanism evolution of fusion welded TC4 titanium alloy/304 stainless steel dissimilar joint by GTAW10.1080/13621718.2023.2264572 ↗
29. Microcosmic mechanism of high-frequency vibratory stress relief based on dislocation density evolution
30. Interfacial microstructure evolution and mechanical properties of TC4 alloy/304 stainless steel joints with different joining modes10.1016/j.jmapro.2018.09.027 ↗
31. Nd/YAG pulsed laser welding of TC4 titanium alloy to 301L stainless steel via pure copper interlayer10.1007/s00170-016-9453-z ↗
32. Microstructures and mechanical property of laser butt welding of titanium alloy to stainless steel10.1016/j.matdes.2013.07.044 ↗
33. Laser-welded butt joints of Ti2AlNb/42CrMo steel with addition of V interlayer10.1016/j.jmrt.2023.12.272 ↗
34. High strength electron beam welded titanium–stainless steel joint with V/Cu based composite filler metals10.1016/j.vacuum.2013.01.015 ↗
35. Influence of heat input on the intermetallic compound characteristics and fracture mechanisms of titanium-stainless steel MIG-TIG double-sided arc welding joints10.1016/j.intermet.2020.106973 ↗