Additive friction stir deposition of WE43: The influence of rotation speed on microstructure, mechanical and corrosion properties
Source abstract
Abstract
The additive friction stir deposition (AFSD) process was successfully conducted on WE43 Mg alloy. WE43 buildings under a wide range of heat input condition (rotation speed of print head from 300 rpm to 600 rpm) with four layers were successfully prepared using AFSD. The comprehensive relationship between the heat input and microstructure-mechanical-corrosion properties was revealed through scanning electron microscopy, electron back-scattered diffraction, X-ray diffraction, tensile testing, electrochemical testing and immersion testing. After AFSD, the average grain size reduced from ∼87 μm to <5 μm. Results of tensile test indicated that samples at 350 rpm exhibited the best comprehensive mechanical properties with the yield strength, ultimate tensile strength and elongation were 216.1 ± 1.9 MPa, 242.6 ± 2.3 MPa and 10.6 ± 1.9 %, respectively. Regardless of heat input, a relatively dense corrosion product was formed on the surface of AFSD samples during immersion. The findings of this work attempted to provided theoretical and practical foundations to guide the parameter-microstructure-performance connection of high-performance Mg-based alloys fabricated by AFSD.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Achieving synergistic strength-ductility-corrosion optimization in Mg-Li-Al-Zn alloy via cross-pass friction stir processing10.1016/j.jallcom.2023.170581 ↗
2. Regulating microstructure of Mg–Li–Al–Zn alloy for enhancing comprehensive performance through friction stir additive manufacturing10.1016/j.msea.2024.146239 ↗
3. Microstructural evolution and its influence on mechanical and corrosion behaviors in a high-Al/Zn containing duplex Mg-Li alloy after friction stir processing10.1016/j.jmst.2023.10.019 ↗
4. Effect of the processing route on the microstructure and mechanical behavior of superlight Mg-9Li-1Zn alloy via friction stir processing10.1016/j.jma.2021.12.002 ↗
5. Recent developments and applications on high-performance cast magnesium rare-earth alloys10.1016/j.jma.2020.06.021 ↗
6. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
7. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
8. On the role of melt flow into the surface structure and porosity development during selective laser melting10.1016/j.actamat.2015.06.004 ↗
9. Directed energy deposition (DED) process: state of the art10.1007/s40684-020-00302-7 ↗
10. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
11. A review on additive/subtractive hybrid manufacturing of directed energy deposition (DED) process
12. State-of-the-art of selective laser melting process: a comprehensive review10.1016/j.jmsy.2022.04.002 ↗
13. Research progress of friction stir additive manufacturing technology
14. Recent advances in additive friction stir deposition: a critical review10.3390/ma17215205 ↗
15. Effect of rotation speed on microstructure and mechanical anisotropy of Al-5083 alloy builds fabricated by friction extrusion additive manufacturing10.1016/j.msea.2022.144237 ↗
16. Effect of rotational speed and feed rate on microstructure and mechanical properties of 6061 aluminum alloy manufactured by additive friction stir deposition10.1007/s00170-023-11527-6 ↗
17. Additive friction stir deposition of AA7075-T6 alloy: impact of process parameters on the microstructures and properties of the continuously deposited multilayered parts10.3390/app131810255 ↗
18. 3D printing of fine-grained aluminum alloys through extrusion-based additive manufacturing: microstructure and property characterization10.1016/j.jmst.2022.08.017 ↗
19. Influence of rotation speed on interfacial bonding mechanism and mechanical performance of aluminum 6061 fabricated by multilayer friction-based additive manufacturing10.1007/s00170-023-11378-1 ↗
20. In-situ monitoring of additive friction stir deposition of AA6061: effect of rotation speed on the microstructure and mechanical properties10.1016/j.msea.2024.146620 ↗
21. In-situ monitoring of additive friction stir deposition of AA6061: effect of layer thickness on the microstructure and mechanical properties
22. Process-structure-property relations for as-deposited solid-state additively manufactured high-strength aluminum alloy
23. Towards understanding the relationships between processing conditions and mechanical performance of the additive friction stir deposition process10.3390/met13101663 ↗
24. Microstructural and mechanical properties of a solid-state additive manufactured magnesium alloy10.1115/1.4052968 ↗
25. Elucidating the effect of additive friction stir deposition on the resulting microstructure and mechanical properties of magnesium alloy WE4310.3390/met11111739 ↗
26. A multi modal approach to microstructure evolution and mechanical response of additive friction stir deposited AZ31B Mg alloy10.1038/s41598-022-17566-5 ↗
27. Microstructure heterogeneity and mechanical properties of Mg-Gd-Y-Zr alloy fabricated by force-controlled additive friction stir deposition10.1016/j.matlet.2023.134164 ↗
28. Morphological and microstructural investigation of the non-planar interface formed in solid-state metal additive manufacturing by additive friction stir deposition
29. Evolution of microstructure and mechanical properties of an as-cast Mg-8.2Gd-3.8Y-1.0Zn-0.4Zr alloy processed by high pressure torsion10.1016/j.msea.2017.05.115 ↗
30. Insight the long-term biodegradable Mg-RE-Sr alloy for orthopaedics implant via friction stir processing
31. Characterisation of strengthening precipitate phases in a Mg–Y–Nd alloy10.1016/S1359-6454(00)00013-6 ↗
32. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
33. Evolution of a honeycomb network of precipitates in a hot-rolled commercial Mg–Y–Nd–Zr alloy10.1080/09500839.2013.791751 ↗
34. Macro- and microstructural studies of laser-processed WE43 (Mg-Y-Nd) magnesium alloy10.1007/s11663-013-9896-7 ↗
35. Effect of microstructure on the uniaxial tensile deformation behavior of Mg–4Y–3RE alloy10.1016/j.msea.2013.10.009 ↗
36. Wire-based friction stir additive manufacturing towards isotropic high-strength-ductility Al-Mg alloys10.1080/17452759.2024.2417369 ↗
37. Wire-feeding friction stir welding for large-gap width tolerances10.1177/13621718241264781 ↗
38. Effect of linear friction welding process on microstructure evolution, mechanical properties and corrosion behavior of GH4169 superalloy10.1016/j.cja.2024.03.039 ↗
39. Effect of initial microstructure on performance and corrosion behavior of GH4169 superalloy joint produced by linear friction welding10.1016/j.cja.2024.09.002 ↗
40. Humphreys · 2004 · 48
41. Particle pinning during grain growth—a new analytical model for predicting the mean limiting grain size but also grain size heterogeneity in a 2D polycrystalline context10.1016/j.actamat.2024.120174 ↗
42. Microstructure evolution and superelastic behavior in Ti-35Nb-2Ta-3Zr alloy processed by friction stir processing10.1016/j.actamat.2017.03.079 ↗
43. Mechanism of continuous dynamic recrystallization of Ti−6Al−4V alloy during superplastic forming with sub-grain rotation10.1016/S1003-6326(23)66145-X ↗
44. Enhancing microstructural control and performance of 5A06 alloy through liquid CO2-assisted friction stir processing10.1016/j.jallcom.2024.175289 ↗
45. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
46. Influence of texture and grain refinement on the mechanical behavior of AA2219 fabricated by high shear solid state material deposition10.1016/j.msea.2018.03.088 ↗
47. Improved corrosion resistance achieved in a friction stir processed Mg-5Zn-0.3Ca alloy with fragmented precipitates10.1016/j.corsci.2022.110675 ↗
48. The microstructure, texture, and room temperature mechanical properties of friction stir processed Mg-Y-Nd alloy10.1016/j.msea.2017.02.096 ↗
49. Mechanical properties optimization of AZX612-Mg alloy joint by double-sided friction stir welding10.1016/j.jmatprotec.2017.11.014 ↗
50. Effect of Ca addition on the microstructure and the mechanical properties of asymmetric double-sided friction stir welded AZ61 magnesium alloy10.1016/j.jma.2020.02.001 ↗
51. Texture variation and its influence on the tensile behavior of a friction-stir processed magnesium alloy10.1016/j.scriptamat.2006.02.019 ↗
52. Grain structure evolution during friction-stir welding of AZ31 magnesium alloy10.1016/j.actamat.2009.07.041 ↗
53. Effect of microstructure on tensile and compressive behavior of WE43 alloy in as cast and heat treated conditions10.1016/j.msea.2017.10.084 ↗
54. Hall-Petch relationship and deformation mechanism of pure Mg at room temperature10.1016/j.jallcom.2022.165924 ↗
55. Microstructure and mechanical properties of WE43 magnesium alloy fabricated by wire-arc additive manufacturing10.1016/j.tws.2024.112699 ↗
56. Measurement of the corrosion rate of magnesium alloys using Tafel extrapolation10.1016/j.corsci.2009.10.016 ↗
57. Enhancing corrosion resistance of Mg-Al-Mn-Ca-Y dilute alloy via novel core-shell structured Al8Mn4Y-Al2Ca and controllable solute segregation10.1016/j.jma.2023.10.009 ↗
58. Influence of grain boundary character distribution on sensitization and intergranular corrosion of alloy 60010.1016/0956-716X(95)00420-Z ↗
59. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
60. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
61. Effect of grain size and crystal orientation on the corrosion behavior of as-extruded Mg-6Gd-2Y-0.2Zr alloy10.1016/j.corsci.2019.108338 ↗
62. Influence of texture on corrosion rate of AZ31 Mg alloy in 3.5wt.% NaCl10.1016/j.matdes.2011.04.031 ↗
63. Crystal orientation and electrochemical corrosion of polycrystalline Mg10.1016/j.corsci.2012.05.019 ↗
64. Effect of the crystallographic orientation and twinning on the corrosion resistance of an as-extruded Mg–3Al–1Zn (wt.%) bar10.1016/j.scriptamat.2014.06.015 ↗
65. Crystallographic effects on the corrosion of twin roll cast AZ31 Mg alloy sheet10.1016/j.actamat.2017.05.027 ↗
66. Effect of crystal orientation on corrosion behavior of directionally solidified Mg-4 wt% Zn alloy10.1016/j.jmst.2017.06.009 ↗