journal article·2025-07Open access

Impact of laser shock peening on the microstructure and mechanical performance of 7075 aluminum alloy

Fanghui Wang, Ziheng Ding, Hushan Li, Chaogang Ding, Donghe Zhang, Debin Shan, Bin Guo, Jie Xu

Abstract

7075 aluminum alloy is extensively utilized in high-end manufacturing sectors such as aerospace, owing to its outstanding mechanical properties. However, the 7075 aluminum alloy typically experiences multiple complex working conditions during its service. Enhancing its performance is crucial for improving the service reliability of the entire structure. This study explores the effects of laser shock peening (LSP) on the microstructure and mechanical properties of 7075 aluminum alloy. The results demonstrate that LSP significantly improves microhardness, tensile strength, and strain-hardening behavior, while promoting grain refinement and increasing dislocation density. With an increasing number of LSP cycles, dislocation density rises, leading to the formation of fine-grained surface layer. After LSP for 4 cycles, the surface microhardness increased to 205.8 HV, reflecting a rise of 21.73%. The yield strength and ultimate tensile strength were measured at 510.06 MPa and 572.11 MPa, respectively, indicating increases of 9.62% and 5.40%. Furthermore, LSP-treated specimens exhibited higher strain-hardening rate compared to the untreated alloy, indicating enhanced strengthening. However, elongation decreased with the increase in LSP cycles, likely due to the elevated dislocation density and the consequent reduction in plastic deformation capacity. Overall, LSP emerges as a promising surface treatment technique for enhancing the mechanical properties of 7075 aluminum alloy, with potential applications in industries demanding high-strength materials.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Additive Manufacturing Materials and Processes · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Mechanical behaviour and low cycle fatigue performance of plasma sprayed ZrO2 coated Al-7075-T6 alloy under subzero temperature condition10.1016/j.jallcom.2025.178950 ↗
2. Corrosion damage repair of 7075-T6 aluminum alloy by ultrasonic nanocrystal surface modification10.1016/j.surfcoat.2023.130085 ↗
3. Development and applications of aluminum alloys for aerospace industry10.1016/j.jmrt.2023.09.274 ↗
4. Micro/nanostructure evolution and deformation mechanisms in friction-stir-welded 7075 Al alloy: a comparative analysis of weld zones10.1016/j.jmrt.2025.04.161 ↗
5. Superior mechanical properties and corrosion resistance of laser powder bed fusion 7075 Al/TC4 alloy through microstructure design10.1016/j.jmrt.2024.10.170 ↗
6. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
7. Electrochemical corrosion behavior of 7075 aluminum alloy with different ultrasonic surface rolling microstructures10.1016/j.jmrt.2024.04.166 ↗
8. Orthogonal impact load in 6061-T651 and 7075-T651 aluminum alloy plates10.1016/j.jmrt.2023.08.174 ↗
9. Effect of cooling aging on microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy10.1016/j.matdes.2013.12.024 ↗
10. Effect of coastal atmospheric corrosion on fatigue properties of 2024-T4 aluminum alloy structures10.1016/j.jallcom.2019.06.235 ↗
11. Growth characteristics of stress corrosion cracking in high-strength 7075 aluminum alloy in sodium chloride solutions10.1016/j.engfracmech.2023.109657 ↗
12. Application of shot peening to improve fatigue properties via enhancement of precipitation response in high-strength Al-Cu-Li alloys10.1016/j.jmrt.2024.11.260 ↗
13. Experimental investigation and numerical study on evolution of surface roughness caused by ultrasonic shot peening of 2024 aluminum alloy sheet10.1016/j.jmrt.2024.05.254 ↗
14. Progressive developments, challenges and future trends in laser shock peening of metallic materials and alloys: a comprehensive review10.1016/j.ijmachtools.2023.104061 ↗
15. Influence of shot-peening treatment on wear resistance of medium manganese steel10.1016/j.jmrt.2024.07.101 ↗
16. Nanocrystallization and α martensite formation in the surface layer of medium-manganese austenitic wear-resistant steel caused by shot peening10.1016/j.msea.2006.12.066 ↗
17. Tungsten carbide coating prepared by ultrasonic shot peening to improve the wear properties of magnesium alloys10.1016/j.jmrt.2023.08.079 ↗
18. Ultrasonic horn material dependence of shot dynamics and target property induced by ultrasonic shot peening10.1016/j.jmapro.2024.01.086 ↗
19. Tailoring properties of directed energy deposited Al-Mg alloy by balancing laser shock peening and heat treatment10.1016/j.jmst.2024.03.051 ↗
20. Optimized mechanical properties of the hot forged Ti-6Al-4V alloy by regulating multiscale microstructure via laser shock peening10.1016/j.ijmachtools.2024.104192 ↗
21. Microstructure and high-temperature tribological properties of Ti-6Al-4V alloy treated by laser shock peening10.1016/j.jmrt.2024.02.132 ↗
22. Improvement of gradient microstructure and properties of wire-arc directed energy deposition titanium alloy via laser shock peening10.1016/j.msea.2024.147422 ↗
23. Effect of asynchronized and synchronized laser shock peening on microstructure and mechanical properties of the Ti-6Al-4V laser joint10.1016/j.jmrt.2023.09.219 ↗
24. Homogenization of local microstructure and mechanical properties in friction stir welded Al-Cu alloy joint achieved through laser shock peening10.1016/j.jmatprotec.2024.118579 ↗
25. Microstructure and mechanical properties of wire and arc additive manufactured 2319 aluminum alloy treated by laser shock peening10.1016/j.matchar.2024.114354 ↗
26. Laser shock peening optimized microstructure stabilizes compressive residual stress to improve fatigue performance of high-strength aluminum alloy hole structure
27. Comparison of mechanical and corrosion properties of 7050 aluminum alloy after different laser shock peening10.1016/j.optlastec.2022.108061 ↗
28. Investigation of microstructure and mechanical properties evolution in 7050 aluminum alloy and 316L stainless steel treated by laser shock peening10.1016/j.matchar.2021.111571 ↗
29. Gradient microstructure and vibration fatigue properties of 2024-T351 aluminium alloy treated by laser shock peening10.1016/j.surfcoat.2020.125698 ↗
30. Mechanical properties and microstructural response of 2A14 aluminum alloy subjected to multiple laser shock peening impacts10.1016/j.vacuum.2019.03.058 ↗
31. Experimental and analytical investigation of the effects of laser shock peening processing strategy on fatigue crack growth in thin 2024 aluminium alloy panels10.1016/j.ijfatigue.2020.105969 ↗
32. Combining manufacturing of titanium alloy through direct energy deposition and laser shock peening processes10.1016/j.matdes.2021.109626 ↗
33. Dual skin effect and deep heterostructure of titanium alloy subjected to high-frequency electropulsing-assisted laser shock peening10.1016/j.ijmachtools.2024.104196 ↗
34. Gradient microstructure and fatigue properties of TC21 titanium alloy processed by laser shock peening10.1016/j.jallcom.2022.168139 ↗
35. Effect of laser shock peening without coating (LPwC) on a surface and sub-surface characteristics of aged Ti 15V-3Al-3Cr-3Sn alloy10.1016/j.matpr.2020.11.289 ↗
36. Effect of synchronized laser shock peening on decreasing defects and improving microstructures of Ti-6Al-4V laser joint10.3390/ma16134570 ↗
37. Synergistic enhancement of strength and plasticity for laser direct energy deposited Ti60 joint by locally applied laser shock peening10.1016/j.msea.2025.148255 ↗
38. Enhancing strength-ductility balance in AZ31 Mg alloy through single-shot laser shock peening and subsequent annealing10.1016/j.msea.2024.146388 ↗
39. Microstructure, mechanical properties and fretting corrosion wear behavior of biomedical ZK60 Mg alloy treated by laser shock peening10.1016/S1003-6326(23)66216-8 ↗
40. Effect of the initial texture of AZ31 Mg alloys on their microstructure and texture evolution during single pulse laser shock peening10.1016/j.jmrt.2024.01.252 ↗
41. Improvement of strength-ductility synergy of Mg-Al-Mn alloy using laser shock peening-induced gradient nanostructure10.1016/j.msea.2023.144844 ↗
42. Enhanced fatigue resistance and fatigue-induced substructures in an additively manufactured CoCrNi medium-entropy alloy treated by ultrasonic surface rolling process10.1016/j.ijplas.2023.103721 ↗
43. Strengthening CrFeCoNiMn0.75Cu0.25 high entropy alloy via laser shock peening10.1016/j.ijplas.2022.103296 ↗
44. Investigation on mechanical properties and surface strengthening mechanism of the cemented carbide processed by laser shock peening10.1016/j.jmrt.2025.01.188 ↗
45. Tensile behavior of nickel with gradient microstructure produced by laser shock peening10.1016/j.msea.2019.138603 ↗
46. Effect of laser shock peening on microstructure and fatigue behavior of laser welded 7075 aluminum alloy10.1016/j.tafmec.2025.104908 ↗
47. Laser shock peening regulating aluminum alloy surface residual stresses for enhancing the mechanical properties: roles of shock number and energy10.1016/j.surfcoat.2021.127481 ↗
48. The evolution of strain gradient and surface microstructure of aluminum alloy during multiple laser shock peening cycles10.1016/j.apsusc.2025.163067 ↗
49. Grain refinement of LY2 aluminum alloy induced by ultra-high plastic strain during multiple laser shock processing impacts10.1016/j.actamat.2010.03.026 ↗
50. Microstructure and residual stress modulation of 7075 aluminum alloy for improving fatigue performance by laser shock peening10.1016/j.ijmachtools.2022.103979 ↗
51. Improving creep properties of 7075 aluminum alloy by laser shock peening10.1016/j.surfcoat.2018.06.061 ↗
52. Magnetic-assisted laser shock peening of 7075-T6 aluminum alloy10.1016/j.optlastec.2024.111923 ↗
53. Microstructure and fatigue performance of hard Al alloy repaired by supersonic laser deposition with laser shock peening treatment10.1016/j.matchar.2023.112827 ↗
54. The effect of high temperature deformation on the austenite reversion transformation and η-Ni3Ti precipitation behavior in a Ti-Mo maraging steel10.1016/j.jmrt.2024.12.114 ↗
55. An EBSD study on microstructure and texture development in graphene-reinforced Al-Mg-Si nanocomposites via FSP10.1016/j.jmrt.2024.12.190 ↗
56. Design of explosively welded Fe-Al multilayer laminated composite pipes: a critical microscopy analysis of stand-off distance and post-weld heat treatment effects on interface properties10.1016/j.jmrt.2024.10.003 ↗
57. Dislocation evolution in titanium during surface severe plastic deformation10.1016/j.apsusc.2009.01.048 ↗
58. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
59. Microstructure evolution and mechanical properties of aging 6061 Al alloy via laser shock processing10.1016/j.jallcom.2019.06.347 ↗
60. An improvement in fatigue behavior of AISI 4340 steel by shot peening and ultrasonic nanocrystal surface modification10.1016/j.msea.2020.139752 ↗
61. Deposition stability and enhanced microhardness of laser shock peened of Ti6Al4V alloy manufactured by high layer thickness laser additive manufacturing10.1016/j.mfglet.2025.03.004 ↗
62. Effect of overlap pattern on the residual stress, surface morphology and fatigue properties of Ti-6Al-4V alloy by multiple laser shock peening10.1016/j.optlastec.2024.111486 ↗
63. Laser shock peening induced mechanical properties enhancement of 50CrVA alloy10.1016/j.optlastec.2023.110180 ↗
64. Unveiling the origins of work-hardening enhancement and mechanical instability in laser shock peened titanium10.1016/j.actamat.2022.117810 ↗
65. Derivation of lattice resistance for a straight dislocation movement through displacement of the dislocation from its own stress field core
66. Regulating microstructure and mechanical properties of the as-cast Mg-4Zn-0.5Y-0.5Nd alloy by heat treatment
67. Dislocation density based model for plastic deformation and globularization of Ti-6Al-4V10.1016/j.ijplas.2013.04.003 ↗
68. Synergistic integration of laser shock peening and heat treatment for refined microstructure and enhanced mechanical properties in additively manufactured 17-4PH stainless steel10.1016/j.jmatprotec.2024.118395 ↗
69. Microstructural characterisation of metallic shot peened and laser shock peened Ti-6Al-4V10.1016/j.actamat.2016.10.044 ↗