Abstract

Plasma Mo-Si-Ti coating including the (Ti, Mo)5Si3, MoSi2 and TiSi was prepared on γ-TiAl surface to improve the wear resistance. The coating had 12-μm deposition layer and 5-μm diffusion layer, as well as gradual decrease of grain size from substrate to coating, providing gradient structure and high fracture toughness. Hardness (H), elasticity modulus (E), H/E and H3/E2 values of substrate and coating were 8.4 and 19.6 GPa, 167.2 and 251.8 GPa, 0.050 and 0.078, and 0.021 and 0.119 GPa, indicating that coating had high hardness, resistance to plastic deformation and load bearing capacity. During friction, both the substrate and coating showed abrasive and oxidative wear. The substrate flaked off in the form of large wear debris, causing the high wear rate. However, oxide film and compacted layer of fine debris made the wear rates of substrate to decrease as the load increased. The coating released most of external stress in the form of elastic work, showing high load-bearing capacity. High fracture toughness inhibited the generation of cracks and reduced the spallation of coating. Moreover, fine grains promoted the generation of oxide film on coating surface and improved the adhesion between oxide film and coating. Meanwhile, the presence of oxide film resulted in a reduction of wear rate as the load increased. The excellent nanomechanical properties and fracture toughness reduced the fracture of coating and reduced the specific wear rate of γ-TiAl by about 98%, which could effectively improve the wear resistance of γ-TiAl at room temperature.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. TiAl alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
2. Aluminum diffusion inhibiting properties of Ti5Si3 at 900 °C and its beneficial properties on Al-rich oxidation protective coatings on γ-TiAl10.1016/j.corsci.2022.110265 ↗
3. Light-weight intermetallic titanium aluminides-status of research and development10.4028/www.scientific.net/AMR.278.551 ↗
4. Review of the effect of alloy composition on the growth rates of scales formed during oxidation of gamma titanium aluminide alloys10.1016/S0921-5093(02)00064-3 ↗
5. Development of TiAl-Si alloys-A review10.3390/ma14041030 ↗
6. Atomic-scale investigation on fretting wear mechanism of γ phase in a cast Ti-45Al alloy10.1016/j.apsusc.2021.150555 ↗
7. High-temperature sliding wear behavior of an intermetallic γ-based TiAl alloy10.1016/j.wear.2018.11.025 ↗
8. Fretting wear evolution of γ -TiAl alloy10.1016/j.triboint.2020.106721 ↗
9. Characterisation of the oxidation and creep behaviour of novel Mo-Si-Ti alloys10.1016/j.actamat.2019.11.045 ↗
10. On the chemical and microstructural requirements for the pesting-resistance of Mo-Si -Ti alloys10.1016/j.jmrt.2020.06.002 ↗
11. Microstructural and chemical constitution of the oxide scale formed on a pesting-resistant Mo-Si-Ti alloy10.1016/j.corsci.2020.109081 ↗
12. Oxidation mechanisms in Mo-reinforced Mo5SiB2(T2)-Mo3Si alloys10.1016/S1359-6454(02)00039-3 ↗
13. Microstructure and oxidation mechanism of multiphase Mo-Ti-Si-B alloys at 800 °C10.1016/j.corsci.2021.109518 ↗
14. Constitution, oxidation and creep of eutectic and eutectoid Mo-Si-Ti alloys10.1016/j.intermet.2018.10.028 ↗
15. Interface reactions of magnetron sputtered Si-based dual layer coating systems as oxidation protection for Mo-Si-Ti alloys10.1016/j.surfcoat.2022.128620 ↗
16. Effect of Si content on microstructure, mechanical and oxidation properties of hot pressed Mo-Ti-Si alloys10.1016/j.intermet.2018.06.013 ↗
17. High temperature isothermal oxidation behavior of electron beam melted multi-phase γ-TiAl alloy10.1016/j.intermet.2021.107424 ↗
18. Structure and oxidation behavior of γ-TiAl coating produced by laser cladding on titanium alloy10.1016/j.surfcoat.2017.04.008 ↗
19. A combined surface treatment of surface texturing-double glow plasma surface titanizing on AISI 316 stainless steel to combat surface damage : comparative appraisals of corrosion resistance and wear resistance10.1016/j.apsusc.2019.06.028 ↗
20. Role of the nitrogen ratio on mechanical properties and wear resistance of CrN/Fe functionally graded coating produced by double glow plasma alloying10.1016/j.apsusc.2022.152735 ↗
21. Research progress in strengthening surface performance of Iron and steel materials by double glow plasma surface alloying technology: a brief review
22. Recent developments in research of double glow plasma surface alloying technology : a brief review10.1016/j.jmrt.2020.03.123 ↗
23. Investigation of low temperature oxidation behavior of MoNbTaW thin films10.1016/j.jallcom.2021.163373 ↗
24. Fracture behaviour of ceramic-metallic glass gradient transition coating10.1016/j.ceramint.2018.12.015 ↗
25. Microstructure and mechanical properties of TiC-Fe surface gradient coating on a pure titanium substrate prepared in situ10.1016/j.jallcom.2018.08.316 ↗
26. Role of integrated lateral stress in surface deformation of He-implanted surfaces10.1063/1.323332 ↗
27. Measurement of hardness and elastic modulus by instrumented indentation : advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
28. XPS investigations of tribofilms formed on CrN coatings10.1016/j.apsusc.2016.10.194 ↗
29. A study for pre-processing of Nb diffusion in Nb-N layer by double-glow plasma alloying10.1016/j.jallcom.2019.153121 ↗
30. Nanoindentation study of mechanical properties of Ti based alloys with Fe and Ta additions10.1016/j.jallcom.2016.09.123 ↗
31. Toward hard yet tough ceramic coatings10.1016/j.surfcoat.2014.07.007 ↗
32. Modifying Cr/CrN composite structure by Fe addition: toward manufacturing cost-effective and tough hard coatings10.1016/j.apsusc.2021.149025 ↗
33. Correlation between residual stresses and the tribological behaviour of Inconel 625 coatings10.1016/j.surfcoat.2021.127288 ↗
34. A simple model for the formation of compressive stress in thin films by ion bombardment10.1016/0040-6090(93)90201-Y ↗
35. High temperature oxidation behavior of Ti0.5Al0.5N coating and Ti0.5Al0.4Si0.1N coating10.1016/j.vacuum.2012.04.013 ↗
36. The influence of the alloy microstructure on the oxidation behavior of Ti–46Al–1Cr–0.2Si Alloy10.1023/A:1004534830767 ↗
37. Surface characterization of wear particles10.1016/S0043-1648(98)00397-4 ↗
38. Characterization and classification of wear particles and surfaces10.1016/S0043-1648(01)00562-2 ↗
39. Investigation on wear characteristics of a titanium alloy/steel tribo-pair10.1016/j.matdes.2014.09.016 ↗
40. Recent developments in wear-mechanism maps10.1016/S0301-679X(98)00011-5 ↗
41. Dynamic modelling of wear evolution in rolling bearings10.1016/j.triboint.2014.11.021 ↗
42. Nanoindentation study of the mechanical and damage behaviour of suspension plasma sprayed TiO2 coatings10.1016/j.surfcoat.2011.11.010 ↗
43. Nanoindentation hardness, texture and microstructure of α-Al2O3 and κ-Al2O3 coatings10.1016/j.tsf.2007.10.078 ↗
44. Study on sliding friction and wear behavior of M50 bearing steel with rare earth addition10.1016/j.triboint.2022.107725 ↗
45. Effect of load and sliding speed on friction and wear behavior of silver/h-BN containing Ni-base P/M composites10.1016/j.wear.2010.08.013 ↗
46. Loading and unloading of a spherical contact : from elastic to elastic-perfectly plastic materials10.1016/j.ijmecsci.2012.01.006 ↗
47. Numerical simulation for three dimensional elastic-plastic contact with hardening behavior10.1115/1.1924573 ↗