Abstract

The Ti–6Al–4V alloy is the most widely used titanium-based alloy in aerospace and biomedical applications. Due to the complex shapes required for components in these application areas, additive manufacturing has become a promising option with its advantageous speed and precision. This study examined the impact of direct energy deposition (DED) and powder bed fusion (PBF) technologies on the resulting properties of the Ti–6Al–4V alloy. DED-produced samples showed almost fully dense structure, while PBF-produced ones were characterized by 0.3 % residual porosity. In all states, the α or α′ phase predominated in the material microstructure. The Ti–6Al–4V alloy produced by different additive manufacturing methods showed comparable hardness values in both, as-printed (380 HV) and as-printed + heat-treated (370 HV) states. However, the samples printed by the PBF method exhibited higher tensile strength and yield strength than those printed by the DED method. These values before and after stress-relief heat treatment differed by approximately 100 MPa. Conversely, the DED-printed material is more stable at elevated temperatures (up to 800 °C) compared to the one printed by PBF.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Machinability of titanium alloys (Ti6Al4V and Ti555.3)10.1016/j.jmatprotec.2008.06.020 ↗
2. Mechanical properties of titanium-based Ti–6Al–4V alloys manufactured by powder bed additive manufacture
3. Additive manufacturing of Ti–6Al–4V parts through laser metal deposition (LMD): process, microstructure, and mechanical properties10.1016/j.jallcom.2019.04.255 ↗
4. Tribology of Ti6Al4V: a review10.1007/s40544-019-0338-7 ↗
5. Comparison of the microstructural, mechanical and corrosion resistance properties of Ti6Al4V samples manufactured by LENS and subjected to various heat treatments10.3390/ma17051166 ↗
6. Formation of α-Widmanstätten structure: effects of grain size and cooling rate on the Widmanstätten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
7. Advances in additively manufactured titanium alloys by powder bed fusion and directed energy deposition: microstructure, defects, and mechanical behavior10.1016/j.jmst.2023.11.003 ↗
8. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
9. Corrosion and passivation behavior of Ti-6Al-4V surfaces treated with high-energy pulsed laser: a comparative study of cast and 3D-printed specimens in a NaCl solution10.1016/j.surfcoat.2023.129849 ↗
10. Research progress in metal additive manufacturing: challenges and Opportunities10.1007/s12008-023-01661-6 ↗
11. Multimetal research in powder bed fusion: a review10.3390/ma16124287 ↗
12. Microstructure and mechanical behavior of rhombic dodecahedron-structured porous β-Ti composites fabricated via laser powder bed fusion10.1016/j.jmrt.2024.06.077 ↗
13. Multi-material additive manufacturing with lightweight closed-cell foam-filled lattice structures for enhanced mechanical and functional properties
14. Additive manufacturing technologies: current status and future perspectives10.1111/jopr.13477 ↗
15. C. Cai, K. Zhou, Chapter 7 - metal additive manufacturing, in: C.D. Patel, C.-H. Chen (Eds.), Digital manufacturing, Elsevier2022, pp. 247-298.10.1016/B978-0-323-95062-6.00005-X ↗
16. Understanding melt pool characteristics in laser powder bed fusion: an overview of single- and multi-track melt pools for process optimization
17. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications10.1016/j.mattod.2021.03.020 ↗
18. An overview of Direct Laser Deposition for additive manufacturing; Part I: transport phenomena, modeling and diagnostics
19. The effect of productive and quality deposition strategies on residual stress for Directed Energy Deposition (DED) process10.1016/j.mfglet.2024.09.107 ↗
20. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
21. Influence of island scanning strategy on microstructures and mechanical properties of direct laser-deposited Ti–6Al–4V structures
22. Effect of defects on environment-assisted fracture (EAF) behavior of Ti–6Al–4V alloy fabricated by direct energy deposition (DED)10.1016/j.jmrt.2022.08.158 ↗
23. Effect of processing conditions on the microstructure, porosity, and mechanical properties of Ti-6Al-4V repair fabricated by directed energy deposition10.1016/j.jmatprotec.2018.08.041 ↗
24. Microstructures of laser-deposited Ti–6Al–4V10.1016/j.matdes.2003.09.009 ↗
25. Microstructural evolution and mechanical properties of TiC/Ti6Al4V composites manufactured by selective laser melting after solution and aging treatments10.1016/j.rinp.2024.107781 ↗
26. Microstructure and mechanical behaviour of additive manufactured Ti–6Al–4V parts under tension10.1051/epjconf/201922101037 ↗
27. Tensile behavior of Ti-6Al-4V alloy fabricated by selective laser melting: effects of microstructures and as-built surface quality10.1007/s41230-018-8064-8 ↗
28. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
29. Densification, tailored microstructure, and mechanical properties of selective laser melted Ti–6Al–4V alloy via annealing heat treatment10.3390/mi13020331 ↗
30. Formation of a transition V-rich structure during the α' to α + β phase transformation process in additively manufactured Ti-6Al-4 V10.1016/j.actamat.2022.118104 ↗
31. Compressive fatigue properties of additive-manufactured Ti-6Al-4V cellular material with different porosities10.1016/j.msea.2020.139695 ↗
32. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
33. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
34. Heat treatment of Ti-6Al-4V alloy manufactured by laser-based powder-bed fusion: process, microstructures, and mechanical properties correlations
35. Influence of position and laser power on thermal history and microstructure of direct laser fabricated Ti–6Al–4V samples10.1179/174328405X21003 ↗
36. Hybrid additive manufacturing of Ti6Al4V with powder-bed fusion and direct-energy deposition10.1016/j.msea.2023.145229 ↗
37. Hydrogen embrittlement of Ti-Al6-V4 alloy manufactured by laser powder bed fusion induced by electrochemical charging10.3390/met14020251 ↗
38. Columnar-to-equiaxed grain transition in powder bed fusion via mimicking casting solidification and promoting in situ recrystallization
39. Microstructure evolution and mechanical properties of laser additive manufactured Ti6Al4V alloy under nitrogen-argon reactive atmosphere10.1016/j.msea.2022.143076 ↗
40. Evaluation of heat treatment parameters on microstructure and hardness properties of high-speed selective laser melted Ti6Al4V10.3390/met11020255 ↗
41. Atomization processes of metal powders for 3D printing10.1016/j.matpr.2020.02.364 ↗
42. Laser and electron beam additive manufacturing methods of fabricating titanium bone implants10.3390/app7070657 ↗
43. The influence of electrophoretic deposition parameters and heat treatment on the microstructure and tribological properties of nanocomposite Si3N4/PEEK 708 coatings on titanium alloy10.3390/coatings9090530 ↗
44. Monte Carlo simulations of solidification and solid-state phase transformation during directed energy deposition additive manufacturing10.1007/s40964-021-00253-8 ↗
45. Site-specific microstructure, porosity and mechanical properties of LENS™ processed Ti–6Al–4V alloy10.1016/j.msea.2021.141494 ↗
46. A review of the fatigue properties of additively manufactured Ti-6Al-4V
47. Roudnická · 2020
48. Vojtěch · 2006
49. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗
50. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
51. Differences in the response of additively manufactured titanium alloy to heat treatment - comparison between SLM and EBM10.21062/ujep/353.2019/a/1213-2489/MT/19/4/668 ↗
52. Microstructure evolution and microhardness of TiAl based alloy blade by vacuum suction casting10.1016/j.vacuum.2019.02.028 ↗
53. Effect of solutionizing and quenching treatment on Ti6Al4V alloy: a study on wear, cavitation erosion and corrosion resistance10.1007/s10853-023-08688-w ↗