Tianyi Zeng, Qingzhan Zhang, Shuzhang Zhang, Yong Zhou, Yinghui Zhao, Xianbo Shi, Wei Yan

Abstract

To answer a longstanding question towards how the austenitizing temperature affects the sulfide stress cracking (SSC) resistance in high strength low alloyed (HSLA) steels for oil country tubular goods (OCTG), it is necessary to study effects of the austenitizing temperature on martensite microstructure, diffusion and distribution behaviors of hydrogen atoms and SSC resistance. The current work showed that prior austenite grain size (PAGS) greatly increased as the austenitizing temperature was increased from 820 °C to 910 °C, but slightly increased with a further increase to 1000 °C. Similar trend arose in the size and volume fraction of Cr-rich carbides and effective grain size of martensite. The dislocation density was similar after quenching from various austenitizing temperatures, but after tempering it was found to be increased with the increase in austenitizing temperature. Moreover, although dislocations remarkably decreased the effective hydrogen diffusion coefficient ( D 0 ), these trapped hydrogen atoms could readily detrap, increasing the apparent hydrogen solubility ( C app ). High angle grain boundaries (HAGBs) decreased C app , indicating their role as obstacles other than as short-circuit diffusion paths for hydrogen diffusion. Compared with coarse Cr-rich carbides, their small counterparts could stably trap more hydrogen atoms. Without sacrificing the strength, the SSC resistance was greatly increased through decreasing the austenitizing temperature, reasons came down to less dislocations, higher HAGBs density, more recrystallized regions and finer Cr-rich carbides.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (99)

Show source-provided references
1. Corrosion in the oil and gas industry: an increasing challenge for materials10.1007/s11837-013-0675-3 ↗
2. Review on sulfide stress cracking in sour service for OCTG and recent advances in modeling of hydrogen-assisted fracture10.1016/j.geoen.2023.212174 ↗
3. Pipe and tube steels for oil and gas industry and thermal power plant
4. Sulfide stress cracking (SSC) of a commercial Q345 pressure vessel steel in a wet H2S environment10.1177/02670836231219870 ↗
5. Effect of microstructure on the hydrogen embrittlement, diffusion, and uptake of dual-phase low alloy steels with varying ferrite-martensite ratios10.1016/j.ijhydene.2023.07.061 ↗
6. Analysis of electrochemical hydrogen permeation through X-65 pipeline steel and its implications on pipeline stress corrosion cracking10.1016/j.ijhydene.2006.07.018 ↗
7. The role of hydrogen in sulfide stress cracking of low alloy steels10.5006/1.3581948 ↗
8. Roles of H2S in behaviour of engineering alloys10.1179/imr.1985.30.1.291 ↗
9. Hydrogen related degradation in pipeline steel: a review10.1016/j.ijhydene.2018.06.064 ↗
10. Effects of thermal spray aluminium coating on SSC and HIC resistance of high strength steel in a sour environment10.1016/j.surfcoat.2020.126156 ↗
11. Sour service domains of 13Cr martensitic stainless steels: a review of state-of-art knowledge vis-à-vis ANSI/NACE MR0175/ISO 1515610.1007/s12666-023-03253-0 ↗
12. HIC and SSC behavior of high-strength pipeline steels10.1007/s40195-015-0257-1 ↗
13. 2003
14. Role of microstructure on sulfide stress cracking of oil and gas pipeline steels10.1007/s11661-003-0128-7 ↗
15. Effect of applied stress and microstructure on sulfide stress cracking resistance of pipeline steels subject to hydrogen sulfide10.1016/j.msea.2007.05.067 ↗
16. Effect of cooling rate on sulfide stress cracking resistance of a Q345 pressure vessel steel subject toHydrogen sulfide
17. Effects of Ce and La on microstructure and sulfide stress cracking susceptibility of API-5CT-C110 casing steel10.1016/j.ijhydene.2022.10.056 ↗
18. Optimizing the hydrogen embrittlement resistance by tuning the structures of Cu-rich nanoprecipitates in high strength martensite stainless steels10.1016/j.actamat.2023.118722 ↗
19. Simultaneous enhancement of strength and ductility in a medium carbon low-alloy steel induced by secondary martensite and Cu-rich particles
20. Improving mechanical properties and retained-austenite stability of a medium carbon Q&P steel by adjusting phase ratio
21. On the sulfide stress cracking resistance of a 125 ksi grade high-strength low-alloyed steel for oil country tubular goods10.1016/j.corsci.2022.110781 ↗
22. Effect of initial dislocation density on hydrogen accumulation behavior in martensitic steel10.1016/j.scriptamat.2019.11.051 ↗
23. Effect of electrochemical hydrogen charging on an API X70 pipeline steel with focus on characterization of inclusions10.1016/j.ijpvp.2019.05.006 ↗
24. Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures10.1016/j.actamat.2023.119279 ↗
25. Effects of (Ti, Mo)C precipitation on the microstructure, impact toughness, and sulfide stress corrosion cracking resistance of linepipe steels10.1016/j.jmrt.2024.12.071 ↗
26. Design of high-strength martensitic steels by novel mixed-metal nanoprecipitates for high toughness and suppressed hydrogen embrittlement10.1016/j.matdes.2023.112323 ↗
27. The effect of V8C7 size on hydrogen diffusion behavior and hydrogen induced cracking in pipeline steel10.1016/j.ijhydene.2023.08.263 ↗
28. Hydrogen trapping and diffusion in polycrystalline nickel: the spectrum of grain boundary segregation10.1016/j.jmst.2023.07.027 ↗
29. Rapid hydrogen transportation along grain boundary in nickel10.1007/s40195-014-0102-y ↗
30. The diffusion and trapping of hydrogen along the grain boundaries in polycrystalline nickel10.1016/j.scriptamat.2011.09.036 ↗
31. Experimental studies of grain boundary diffusion of hydrogen in metals10.1016/0956-7151(91)90333-V ↗
32. Influence of prior austenite grain structure on hydrogen-induced fracture in as-quenched martensitic steels10.1016/j.engfracmech.2023.109090 ↗
33. Hydrogen embrittlement mechanism of ultrafine-grained iron with different grain sizes10.2355/isijinternational.ISIJINT-2022-562 ↗
34. Hydrogen effect on the intergranular failure in polycrystal ɑ-iron with different crystal sizes10.1016/j.ijhydene.2021.08.126 ↗
35. The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel10.1016/j.ijhydene.2014.11.057 ↗
36. Different aspects of hydrogen diffusion behavior in pipeline steel10.1016/j.jmrt.2023.04.026 ↗
37. Hydrogen trapping and hydrogen embrittlement (HE) susceptibility of X70 grade high-strength, acid-resistant, submarine pipeline steel with Mg treatment10.1016/j.jmrt.2023.03.011 ↗
38. Prior austenite grain growth in heat-affected zone of a 0.5Cr-Mo-V steel10.1179/030716977803292619 ↗
39. The growth behavior of austenite grain in the heating process of 300M steel10.1016/j.msea.2011.02.089 ↗
40. Study on precipitation behavior of Ce and Nb during solidification10.1016/j.jmrt.2024.01.251 ↗
41. Elimination of primary NbC carbides in HSLA steels for oil industry tubular goods10.1007/s11837-022-05202-6 ↗
42. Effects of the primary NbC elimination on the SSCC resistance of a HSLA steel for oil country tubular goods10.3390/ma14185301 ↗
43. Effect of NbC and VC carbides on microstructure and strength of high-strength low-alloyed steels for oil country tubular goods
44. Sörlander · 2022
45. The dissolution of cementite during austenitization of steel10.2355/isijinternational1966.11.149 ↗
46. A quantitative study of the formation of austenite and the solution of cementite at different austenitizing temperatures for a 1.27% carbon steel10.1016/0001-6160(56)90157-2 ↗
47. DICTRA simulation of holding time dependence of NbC size and experimental study of effect of NbC on austenite grain growth10.1007/s11661-015-2922-4 ↗
48. Solubility of niobium carbide and niobium carbonitride in alloyed austenite and ferrite10.1007/BF02644979 ↗
49. In-situ observation and analysis of high temperature behavior of carbides in GCr15 bearing steel by confocal laser scanning microscopy
50. Study of the kinetics of austenite grain growth by dynamic Ti-rich and Nb-rich carbonitride dissolution in HSLA steel: in-situ observation and modeling10.1016/j.matchar.2020.110612 ↗
51. Microstructural characterizations and sulfide stress cracking susceptibility of a high-strength oil country tubular goods-purpose steel under different quenching conditions10.1007/s11661-024-07312-z ↗
52. Carbon redistribution in quenched and tempered lath martensite10.1016/j.actamat.2020.116521 ↗
53. Carbon partitioning into austenite after martensite transformation10.1016/S1359-6454(03)00059-4 ↗
54. Effects of rare-earth micro-alloying on microstructures, carbides, and internal friction of 51CrV4 steels10.1016/j.jallcom.2020.153849 ↗
55. MWP-fit: a program for multiple whole-profile fitting of diffraction peak profiles by ab initio theoretical functions10.1107/S0021889801011451 ↗
56. Effect of block size on the strength of lath martensite in low carbon steels10.1016/j.msea.2005.12.048 ↗
57. Prior austenite grain size and tempering effects on the dislocation density of low-C Nb–Ti microalloyed lath martensite10.1016/j.scriptamat.2015.05.036 ↗
58. Effect of block size on the reduction rate of dislocation density during tempering treatment of lath martensite in low alloy steel10.2355/isijinternational.ISIJINT-2021-469 ↗
59. Effect of grain size and cooling rate on the martensite start temperature of stainless steel10.1002/srin.202200044 ↗
60. Analysis of effect of alloying elements on martensite start temperature of steels10.1179/026708303225001902 ↗
61. Prediction of martensite start temperature in alloy steels with different grain sizes10.1007/s11661-013-1798-4 ↗
62. Effect of austenite grain size on transformation behavior, microstructure and mechanical properties of 0.1C–5Mn martensitic steel10.2355/isijinternational.53.2218 ↗
63. Effect of prior austenite grain size refinement by thermal cycling on the microstructural features of as-quenched lath martensite10.1007/s11661-016-3525-4 ↗
64. Effect of quenching temperature on sulfide stress cracking behavior of martensitic steel10.1016/j.msea.2018.03.063 ↗
65. Secondary recrystallization in copper10.1007/BF03398387 ↗
66. Grain boundary engineering: an overview after 25 years10.1179/026708309X12601952777747 ↗
67. Solute segregation and classification of [100] tilt grain boundaries in α-iron: consequences for grain boundary engineering10.1016/S1359-6454(03)00219-2 ↗
68. On the CSL grain boundary distributions in polycrystals10.1016/0956-716X(94)90554-1 ↗
69. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
70. Grain boundary engineering approach to improve hydrogen embrittlement resistance in FeMnC TWIP steel10.1016/j.ijhydene.2018.04.048 ↗
71. A Taylor-based plasticity model for orthogonal machining of single-crystal FCC materials including frictional effects10.1007/s00170-008-1409-5 ↗
72. Thermomechanical processing model and abnormal microstructure evolution of high-nitrogen stainless steel X30CrMoN15-110.1016/j.jallcom.2022.165498 ↗
73. Elucidating the dual effect of vanadium microalloying on hot deformation behavior of high nitrogen martensitic stainless steel10.1016/j.jmrt.2024.02.216 ↗
74. Effects of Cu addition on resistance to hydrogen embrittlement in 1 GPa-grade duplex lightweight steels10.1016/j.actamat.2020.06.051 ↗
75. Review of hydrogen embrittlement in metals: hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention10.1007/s40195-020-01039-7 ↗
76. Effects of internal hydrogen and surface-absorbed hydrogen on the hydrogen embrittlement of X80 pipeline steel10.1016/j.ijhydene.2019.04.239 ↗
77. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
78. Hydrogen trapping and embrittlement in metals – a review
79. Quantification of hydrogen trapping in multiphase steels: Part I – point traps in martensite10.1016/j.actamat.2020.05.007 ↗
80. Investigation of the effect of carbon on the reversible hydrogen trapping behavior in lab-cast martensitic FeC steels10.1016/j.matchar.2021.111671 ↗
81. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
82. Effects of different cooling rates on the microstructure, crystallographic features, and hydrogen induced cracking of API X80 pipeline steel10.1016/j.jmrt.2021.07.060 ↗
83. Microstructure design strategies to mitigate hydrogen embrittlement in metallic materials10.1111/ffe.14074 ↗
84. Comparative study on the effects of Cr, V, and Mo carbides for hydrogen-embrittlement resistance of tempered martensitic steel10.1038/s41598-019-41436-2 ↗
85. Optimizing the hydrogen embrittlement resistance by Cu addition in a low carbon high strength steel10.1016/j.engfailanal.2024.108004 ↗
86. Evolution of crystal structure of Cu precipitates in a low carbon steel10.1016/j.matdes.2017.08.054 ↗
87. Hydrogen diffusion and hydrogen embrittlement of a 1500 MPa hot-stamped steel 22MnB5 in different austenitizing conditions
88. Temperature dependence of hydrogen-assisted damage evolution and fracture behavior in TRIP-aided bainitic ferrite steel
89. Quantitative investigation on deep hydrogen trapping in tempered martensitic steel10.1016/j.jallcom.2020.157218 ↗
90. On the martensitic structure and hardness in as-quenched Fe-Ni alloys10.1016/j.jallcom.2017.08.285 ↗
91. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
92. Mesoscale quantification of grain boundary character and local plasticity in hydrogen-assisted intergranular and intergranular-like cracking paths in tempered martensitic steel
93. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel10.1016/j.actamat.2005.09.015 ↗
94. Sulfide stress cracking behavior of a martensitic steel controlled by tempering temperature10.3390/ma11030412 ↗
95. Sulphide stress cracking behaviour of the coarse-grained heat-affected zone in X100 pipeline steel under different heat inputs10.1016/j.ijhydene.2020.05.092 ↗
96. Effect of grain boundary character distribution on hydrogen embrittlement in Fe–Ni based alloy
97. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
98. Effect of Nb–Ti multi-microalloying on the hydrogen trapping efficiency and hydrogen embrittlement susceptibility of hot-stamped boron steel
99. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗