Enhanced of friction and wear properties for TiC/TC4 coating based on the precipitation of the lubricating and strengthening phases through laser cladding of Cr–WS2–Ni60 powder
Source abstract
Abstract
To address the shortcomings of TiC/TC4 titanium alloy-based ceramic coatings in wear resistance and high-temperature stability, the TiC/TC4 coating was reinforced by introducing two types of mixed powders, Ni60-WS 2 and Cr-Ni60-WS 2 , onto the surface through laser cladding technology. In the cladding layer of the WS 2 -Ni60 coating, in addition to the original unmelted white blocky TiC phase, new granular W 2 C and strip-like TiNi phases were formed. After Cr was added, fine Cr particles, flake-like TiS 2 phase, granular Cr 3 C 2 phase and uniformly distributed TiC were further generated. The hardness of both coatings showed a gradient distribution across the composite coating zone, heat-affected zone, and near-substrate zone. The highest hardness which was 3 times that of the substrate was observed at 0.25 mm from the surface. When the laser power was 1200 W, the friction coefficients at room temperature and 500°C of the Cr-Ni60-WS 2 coating were 0.32 and 0.30 respectively. The formation of the lubricating phase TiS 2 , the strengthening phase Cr 3 C 2 , and the uniformly distributed TiC phase was the main reason for the excellent wear resistance. Lower power caused incomplete phase decomposition, leading to adhesive wear. Higher power results in delamination wear due to thermal stress and phase coarsening.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · Metal and Thin Film Mechanics · Surface Treatment and Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Naturally high fatigue performance of a 3D printing titanium alloy across all stress ratios
2. Optimal lubricating protection and interfacial behavior for titanium alloy surface from phosphorus-based ionic liquids, J10.1016/j.triboint.2024.109933 ↗
3. Crystal plasticity finite element method investigation of normal tensile deformation anisotropy in rolled pure titanium sheet10.1016/j.tws.2024.111904 ↗
4. Influence of Mo additive on microstructure and corrosion behavior of TC4 metal-cored welding overlay10.1016/j.jmrt.2025.03.159 ↗
5. Competition mechanism of dynamic recrystallization and recovery and microstructure evolution of TC4 alloy during warm deformation10.1016/j.jmrt.2025.04.200 ↗
6. Research status and prospects of novel technology in underwater wet arc welding/laser cladding10.1016/j.jmapro.2025.05.029 ↗
7. A review on ceramic coatings prepared by laser cladding technology10.1016/j.optlastec.2024.110993 ↗
8. Microstructural evolution and fatigue performance of 25CrMo4 steel remanufactured by high-speed laser cladding of Inconel 625 alloy
9. The structure and properties of laser-cladded inconel 625/TiC composite coatings10.3390/ma16031265 ↗
10. Structure and properties of laser-cladded Inconel 625-based in situ composite coatings on S355JR substrate modified with Ti and C powders10.2478/msp-2022-0039 ↗
11. Microstructure evolution mechanisms endowing high compression strength assisted by stacking fault-twin synergy in TiC/TC4 alloy nanocomposites prepared by laser powder bed fusion under hot isostatic pressing10.1016/j.msea.2025.147789 ↗
12. Superior strength-ductility combination in TiC/TC4 composites via in situ construction Ti2Cu nanoparticles10.1016/j.carbon.2024.118805 ↗
13. Mechanisms of superlubricity in WS2/Graphite interfaces: a first-principles study on silicon-based substrates10.1016/j.apsusc.2024.162109 ↗
14. Engineering of multilayered coating on additively manufactured Ti-6Al-4V porous implants to promote tribological and fatigue performances10.1016/j.surfcoat.2024.131400 ↗
15. Friction–wear behaviors and microstructure of AlTiVCrNb lightweight refractory high-entropy alloy coating prepared by laser cladding on Ti–6Al–4V substrate10.1016/j.jmrt.2024.01.107 ↗
16. Effects of TiC particles on tribological and corrosion resistance of PEO coating on TC4 alloy10.1016/j.corcom.2023.10.002 ↗
17. Tribology comparison of laser-cladded CrMnFeCoNi coatings reinforced by three types of ceramic (TiC/NbC/B4C)10.1016/j.surfcoat.2022.129013 ↗
18. Tribological behavior and mechanical properties of thermal sprayed TiO2–ZnO and TiOx ceramic coatings10.1016/j.ceramint.2023.02.243 ↗
19. Effect of Fe content on the microstructure and wear resistance of AlCoCrFeNi high-entropy alloy coating prepared by laser cladding10.1016/j.apsusc.2024.162019 ↗
20. Preparation and cutting performance of (W,Ti,Ta)C/CaF2 nano-self-lubricating cermet tool material via spark plasma sintering
21. Study on the structure and friction properties of NCG/WS2 copper-based self-lubricating composites10.1016/j.jallcom.2024.176828 ↗
22. Effects of annealing on laser clad Ti2SC/CrS self-lubricating anti-wear composite coatings on Ti6Al4V alloy: microstructure and tribology10.1016/j.triboint.2016.05.004 ↗
23. WS2 nanopowders as high-temperature lubricants: an experimental and theoretical study10.1021/acsanm.9b01143 ↗
24. Effect of Cr/Zr metal layer on the microstructure and properties of CrN coating deposited by arc ion plating10.1016/j.surfcoat.2025.132730 ↗
25. One-step construction of CrN coating and Cr-N-Fe metallurgical interface via deposition–nitriding strategy for enhanced fretting wear resistance of 40CrNiMo
26. Ultra-high resistance to electrochemical and high-temperature steam corrosion of MAO/Cr bilayer coatings fabricated on Zr alloys10.1016/j.jmst.2025.04.047 ↗
27. Enhancing high-temperature fretting wear resistance of Ti-64 alloy by laser cladding FeCrAlMo Nb high entropy alloy coatings10.1016/j.jmrt.2024.06.205 ↗
28. Microstructures and mechanical properties of in situ synthesized TiC/TC4 titanium alloy composite coatings prepared by Sol–Gel‐Assisted laser cladding10.1002/adem.202402916 ↗
29. Enhanced high-temperature oxidation resistance of TC11 titanium alloys via laser cladding FeCoNiCrMoBSi high-entropy alloy coatings10.1016/j.matchemphys.2025.130861 ↗
30. TiC in-situ strengthening mechanism and crack initiation mechanism of SiC/TC4 composite coatings by laser cladding10.1016/j.ceramint.2024.10.107 ↗
31. Atomic-scale interfacial strengthening mechanism of nano intermetallic compounds in Ti-Ni bimetallic alloys10.1016/j.mechmat.2025.105329 ↗
32. A threshold of Cr dominated structure transition and stability enhancement of passive films in high entropy alloy CrxMnFeCoNi10.1016/j.corsci.2025.112907 ↗
33. Progress and prospect of transition metal compound cathode materials with stable metal ion storage effect in various battery systems10.1016/j.gee.2025.02.001 ↗
34. Atomistic modeling of long-range ordering in FCC ni-cr-fe alloys10.1016/j.scriptamat.2025.116688 ↗