journal article·2025-07Open access

Hydrogen embrittlement of ferrite-pearlite OCTG steels under electrochemical and gaseous hydrogen environment

Dong-Kyu Oh, Byoungchul Hwang

Abstract

This study investigates the hydrogen embrittlement behavior under electrochemical and gaseous hydrogen charging conditions, providing a multi-scale analysis of the correlation between fracture behavior and microstructural factors in ferrite-pearlite OCTG (oil country tubular goods) steel. The hydrogen embrittlement mechanism at the notch root was predominantly governed by the hydrogen-enhanced decohesion (HEDE) mechanism, which is facilitated by high triaxial stress states and hydrogen accumulation. Although the relative notch tensile strength (RNTS) value remained identical at 0.85 under a gaseous hydrogen pressure of 10 MPa and a current density of 0.5A/m 2 , the fracture behavior exhibited significant differences. Gaseous hydrogen charging facilitated deeper hydrogen penetration into the central regions, leading to quasi-cleavage fracture, whereas electrochemical charging predominantly induced brittle fracture near the surface. Thermal desorption analysis (TDA) revealed low-temperature peaks at 0.19 ppm and 0.07 ppm, corresponding to reversible trap site such as ferrite lattice defects and grain boundaries. A high-temperature peak of 0.40 ppm corresponded to hydrogen trapped in cementite, which was classified as an irreversible trapping site. Fractographic analysis revealed that ferrite underwent cleavage fracture due to hydrogen trapping at lattice sites, whereas pearlite exhibited shear cracking across the cementite lamellae, driven by localized stress concentration. These findings underscore the crucial role of microstructural characteristics and hydrogen trapping behavior in governing hydrogen embrittlement mechanisms, offering insights into the development of hydrogen-resistant OCTG steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Effect of rolling and coiling temperatures on microstructure and mechanical properties of medium-carbon pipeline steel10.1007/s12540-019-00500-2 ↗
2. Effect of precipitation of (Ti, V)N and V(C, N) secondary phases on mechanical properties of V and N microalloyed 1Cr steels
3. Effect of quenching post-intercritical austenitizing on the microstructure and tensile properties of a K55 grade steel for oil and gas industry10.1002/srin.202400478 ↗
4. Review on sulfide stress cracking in sour service for OCTG and recent advances in modeling of hydrogen-assisted fracture10.1016/j.geoen.2023.212174 ↗
5. Super-high strength low alloy steel OCTG with improved sour resistance
6. Causes of structural heterogeneity in high-strength OCTG tubes and minimizing their impact on sulfide stress corrosion cracking resistance10.3390/met11111843 ↗
7. Hydrogen induced cracking (HIC) testing of low alloy steel in sour environment: impact of time of exposure on the extent of damage10.1016/j.corsci.2009.11.044 ↗
8. Effect of quenching and tempering process on sulfide stress cracking susceptibility in API-5CT-C110 casing steel10.1016/j.msea.2017.01.067 ↗
9. The effect of carbon on hydrogen embrittlement in stable Cr-Ni-Mn-N austenitic stainless steels10.1016/j.corsci.2017.05.004 ↗
10. Hydrogen related degradation in pipeline steel: a review10.1016/j.ijhydene.2018.06.064 ↗
11. Tensile and fracture behaviors of austenitic high-manganese steels subject to different hydrogen embrittlement test methods10.1016/j.msea.2019.138367 ↗
12. Comparative study of hydrogen embrittlement of three heat-resistant Cr-Mo steels subjected to electrochemical and gaseous hydrogen charging10.1007/s11661-020-05704-5 ↗
13. Machine learning approach for prediction of hydrogen environment embrittlement in austenitic steels10.1016/j.jmrt.2022.06.046 ↗
14. Hydrogen-assisted fracture features of a high strength ferrite-pearlite steel10.1016/j.jmst.2018.12.019 ↗
15. Hydrogen-enhanced deformation in pearlite10.1016/j.actamat.2024.120327 ↗
16. Role of deformation on the hydrogen trapping in the pearlitic steel10.1016/j.scriptamat.2023.115859 ↗
17. Resistance of pearlite against hydrogen-assisted fatigue crack growth10.1016/j.ijhydene.2022.07.074 ↗
18. Review and assessment of the effect of hydrogen gas pressure on the embrittlement of steels in gaseous hydrogen environment10.3390/met11040637 ↗
19. Effect of hydrogen traps on hydrogen permeation in X80 pipeline steel—a joint experimental and modelling study10.1016/j.ijhydene.2022.10.038 ↗
20. Experimental study on the temperature dependence of gaseous hydrogen permeation and hydrogen embrittlement susceptibility of X52 pipeline steel10.1016/j.engfailanal.2023.107746 ↗
21. Focused review on factors affecting martensitic stainless steels and super martensitic stainless steel passive film in the oil and gas field10.1007/s10008-024-05984-6 ↗
22. Effects of the primary NbC elimination on the SSCC resistance of a HSLA steel for oil country tubular goods10.3390/ma14185301 ↗
23. Microstructure and properties of intercritically reheated coarse-grained heat affected zone in X65 pipeline steel with pre-strain10.1016/j.ijhydene.2023.11.074 ↗
24. Analysis of the physicochemical, mechanical, and electrochemical parameters and their impact on the internal and external SCC of carbon steel pipelines10.3390/ma13245771 ↗
25. Determination of hydrogen diffusion parameters of ferritic steel from electrochemical permeation measurement under tensile loads10.1149/2.1021412jes ↗
26. The effects of NaCl on hydrogen permeation and sulfide stress cracking resistance of C110 high-strength steel10.1149/1945-7111/ac96ad ↗
27. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗
28. Effect of microstructure on hydrogen diffusion and notch tensile strength of large steel forging10.1016/j.msea.2015.01.040 ↗
29. Notched-tensile properties under high-pressure gaseous hydrogen: comparison of pipeline steel X70 and austenitic stainless type 304L, 316L steels10.1016/j.ijhydene.2016.12.069 ↗
30. Notch sensitivity analysis of a 2205 duplex stainless steel in a gaseous hydrogen environment10.1016/j.tafmec.2024.104655 ↗
31. Effect of cementite on the hydrogen diffusion/trap characteristics of 2.25Cr-1Mo-0.25V steel with and without Annealing10.3390/ma11050788 ↗
32. Hydrogen trapping phenomena in carbon steel10.1007/BF00540409 ↗
33. Difference in hydrogen trapping behaviors between epsilon carbide and cementite in steels10.1016/j.matchar.2024.114557 ↗
34. Evaluation of the cementite morphology influence on the hydrogen induced crack nucleation and propagation path in carbon steels10.1016/j.ijhydene.2022.01.222 ↗
35. Investigation of hydrogen-induced embrittlement in pearlitic steels for the use in tensile armor of risers
36. Effects of microstructures on hydrogen induced cracking of electrochemically hydrogenated double notched tensile sample of 4340 steel10.1016/j.msea.2016.02.047 ↗
37. Hydrogen embrittlement processes in microalloyed steel notched tensile samples10.1016/j.tafmec.2020.102878 ↗
38. Effects of defect on the hydrogen embrittlement behavior of X80 pipeline steel in hydrogen-blended natural gas environments10.1016/j.ijhydene.2024.01.107 ↗
39. Notch tip hydrogen assisted microdamage in fully pearlitic steel: the Tearing Topography Surface (TTS)10.1016/j.prostr.2024.04.015 ↗
40. Origin of tearing topography surface in hydrogen-charged pearlitic steel10.1016/j.actamat.2023.119116 ↗
41. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
42. Influence of hydrogen-enhanced plasticity and decohesion mechanisms of hydrogen embrittlement on the fracture resistance of steel
43. Micro-axial cracking in unnotched, cold-drawn pearlitic steel wire: mechanism and beneficial effect on the resistance to hydrogen embrittlement10.1016/j.actamat.2021.117567 ↗
44. Effects of lamellar structure on tensile properties and resistance to hydrogen embrittlement of pearlitic steel10.1016/j.actamat.2019.04.040 ↗
45. Effect of bainite fraction on hydrogen embrittlement of bainite/martensite steel10.1016/j.msea.2021.141226 ↗
46. First-principles study on hydrogen diffusivity in BCC, FCC, and HCP iron10.1007/s11661-018-4815-9 ↗
47. Atomistic study of hydrogen diffusion in presence of defects in bcc and fcc iron10.1016/j.commatsci.2023.112433 ↗
48. Diffusion coefficient of hydrogen interstitial atom in α-Fe, γ-Fe and ε-Fe crystals by first-principle calculations10.1016/j.ijhydene.2017.08.212 ↗